← Back to Patent Explorer
US4231906A Expired / Lapsed US ⏱️ 0.0 years remaining

Ink composition for non woven fabrics of synthetic fibers

Assignee: Atex/U Inc SA
•
Filing: 1978-12-11
•
Granted: 1980-11-04
•
Expires: 1998-12-11
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract An ink composition is provided for the lithographic imprinting of non woven fabrics constituted of polyethylene fibers, such a composition comprising a pigment, a desiccant, a binder based on isophthalic and/or urethane varnish, a protective wax and an oleoresinous varnish consisting of phenolic resin, linseed oil, tung oil and high boiling mineral oil.

Inventors

  • 👤 Maurizio Giorgetti

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-03 12:07
CPC Classifications
C; C09; C09D; C09D11/00; C09D11/02; Y; Y10; Y10S; Y10S260/00; Y10S260/38

Claims Analysis

Total Claims: 9
Claim 1
Independent Claim 212 words
An ink composition for the imprinting of polyolefinic non woven fabrics, comprising a pigment, a desiccant, a binder based on isophthalic and/or urethane varnish, a polyethylene protective wax and characterized in that it comprises between 54 and 64 percent by weight of an oleoresinous varnish consisting of a phenolic resin, crude linseed oil, tung oil and high boiling mineral oil, the composition being further characterized in that it imparts significant resistance to washing of the polyolefinic non woven fabrics such that when said fabric is washed as a delicate textile with a bland detergent, no discernible color change occurs after as many as six or seven cycles of washing, the composition being further characterized in that it imparts a feel or "hand" to said imprinted polyolefinic non woven fabric which remains unchanged after repeated washings and prolonged period of storage, the composition being further characterized in that said imprinted polyolefinic non woven fabric demonstrates substantial resistance to abrasion, the composition being further characterized in that said imprinting of polyolefinic non woven fabrics can be carried out lithographically with a desiccation time substantially less than two days, and characterized by a durable chemical linkage between the ink and the non woven fabric such that breakage does not occur under flexing of the fabric.
Claim 2
Dependent Claim 212 words
An ink composition for the imprinting of polyolefinic non woven fabrics, comprising a pigment, a desiccant, a binder based on isophthalic and/or urethane varnish, a polyethylene protective wax and characterized in that it comprises between 54 and 64 percent by weight of an oleoresinous varnish consisting of a phenolic resin, crude linseed oil, tung oil and high boiling mineral oil, the composition being further characterized in that it imparts significant resistance to washing of the polyolefinic non woven fabrics such that when said fabric is washed as a delicate textile with a bland detergent, no discernible color change occurs after as many as six or seven cycles of washing, the composition being further characterized in that it imparts a feel or "hand" to said imprinted polyolefinic non woven fabric which remains unchanged after repeated washings and prolonged period of storage, the composition being further characterized in that said imprinted polyolefinic non woven fabric demonstrates substantial resistance to abrasion, the composition being further characterized in that said imprinting of polyolefinic non woven fabrics can be carried out lithographically with a desiccation time substantially less than two days, and characterized by a durable chemical linkage between the ink and the non woven fabric such that breakage does not occur under flexing of the fabric.
Claim 3
Dependent Claim 49 words
An ink composition according to claim 1 in which said oleoresinous varnish comprises ingredients with the following percentages by weight: ______________________________________ Phenolic resin 39% Bleached neutral crude linseed oil 20% tung (Chinese wood) oil prepared at 230° C. 10% High boiling mineral oil prepared at 190° C. 31% ______________________________________
Claim 4
Dependent Claim 16 words
The composition of claim 1 wherein said polyolefinic non woven fabrics are polyethylene non woven fabrics.
Claim 5
Dependent Claim 14 words
The composition of claim 1 wherein said desiccation time is 1 to 11/2 hours.
Claim 6
Dependent Claim 36 words
An ink composition for the imprinting of polyolefinic non woven fabrics comprising (percentages by weight) ______________________________________ a pigment 10-20% isophthalic varnish 10% urethane varnish 8% oleoresinous varnish 54-64% polyethylene wax 3% cobalt manganese-naphthenate desiccant 3% ______________________________________
Claim 7
Dependent Claim 36 words
An ink composition for the imprinting of polyolefinic non woven fabrics comprising (percentages by weight) ______________________________________ a pigment 10-20% isophthalic varnish 10% urethane varnish 8% oleoresinous varnish 54-64% polyethylene wax 3% cobalt manganese-naphthenate desiccant 3% ______________________________________
Claim 8
Dependent Claim 147 words
A process for making an ink composition for the imprinting of polyolefinic non woven fabrics, comprising the following steps: (a) preparing an oleoresinous varnish by heating at 220° C. in an open cauldron 39 parts of phenolic resin, 20 parts of neutral bleached linseed oil, 10 parts of tung oil prepared at 230° C., and 31 parts of high boiling mineral oil prepared at 190° C.; (b) mixing the components from step (a) for about 50 minutes; (c) unloading and subjecting the mixture from step (b) to refining in a conventional refining device having three cylinders with a minimum of three passages; (d) adding to the product of (c) 23 parts of the same oleoresinous varnish of step (a), together with 3 parts of a desiccant comprising cobalt, manganese-naphthenate; (e) removing the product of step (d) for utilizing in lithographic imprinting of said non woven polyolefinic fabric.
Claim 9
Dependent Claim 147 words
A process for making an ink composition for the imprinting of polyolefinic non woven fabrics, comprising the following steps: (a) preparing an oleoresinous varnish by heating at 220° C. in an open cauldron 39 parts of phenolic resin, 20 parts of neutral bleached linseed oil, 10 parts of tung oil prepared at 230° C., and 31 parts of high boiling mineral oil prepared at 190° C.; (b) mixing the components from step (a) for about 50 minutes; (c) unloading and subjecting the mixture from step (b) to refining in a conventional refining device having three cylinders with a minimum of three passages; (d) adding to the product of (c) 23 parts of the same oleoresinous varnish of step (a), together with 3 parts of a desiccant comprising cobalt, manganese-naphthenate; (e) removing the product of step (d) for utilizing in lithographic imprinting of said non woven polyolefinic fabric.

References Cited (Backward Citations)

US2146598A Cited
US2455541A Cited
US2574971A Cited
US2906590A Cited
US3182105A Cited
US3150917A Cited
US3273498A Cited
FR2009351A1 Cited
CA979555A Cited
US4115329A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1983-11-04 1984-05-05 1984-11-04 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1987-11-04 1988-05-05 1988-11-04 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1991-11-04 1992-05-05 1992-11-04 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag