Patent US4378328A successfully refreshed from Google Patents.
← Back to Patent Explorer
US4378328A Expired / Lapsed US ⏱️ 0.0 years remaining

Method for making chime structure for blow molded hollow member

Assignee: Mauser Werke GmbH
•
Filing: 1980-03-14
•
Granted: 1983-03-29
•
Expires: 2000-03-14
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract The invention sets out a method and apparatus of forming a chime projecting radially outwardly of a blow molded hollow member. The chime is formed immediately after the blow molding of the hollow member by forming a radially outwardly projecting channel-shaped part in the side wall of the hollow member. The surfaces of the channel-shaped part are moved toward each other to form a welded connection at the radially inner end of the channel-shaped part. The movement of the channel-shaped part to form the chime is effected by telescoping slides which move axially at different stroke speeds and at different stroke lengths. The radially inwardly most disposed slide moves farthest and faster so as to produce a rolling movement of the channel-shaped part as the chime is formed. The resulting chime is integrally formed from the material of the hollow member and includes at least an outer wall extending circumferentially around the hollow member and a side wall to which the outer wall is welded at its inner radial end.

Inventors

  • 👤 Dietmar Przytulla
  • 👤 Harald Feuerherm

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-04 14:27
CPC Classifications
B; B29; B29C; B29C49/00; B29C49/42; B29C49/48; B29C49/54; B29C49/02; B29C49/04; B29C49/482; B65; B65D; B65D1/00; B65D1/12; B65D1/14; B65D1/16; B29C2049/542; B29C2049/548

Claims Analysis

Total Claims: 15
Claim 1
Independent Claim 245 words
In the method of producing a chime projecting radially outwardly on a blow-molded hollow member of thermoplastic material by forming the chime directly from the still hot hollow member by actuation of axially movable slide means toward an axially aligned fixed mold surface of a divided blow mold after the two mold halves have been brought together and after a plastic parison gripped between the mold halves has been inflated to a given shape to form the hollow member with a radially outwardly projecting annular channel-shaped part having one side wall thereof lying against the fixed mold surface, its other side wall lying against the slide means and the bottom outer wall lying against a radially outwardly disposed axial surface of the mold, by moving the slide means axially of the hollow member toward the fixed mold surface, the improvement characterized in that: (a) the slide means, which are defined by multi-part first and second slides telescoped on one another, are moved axially in supporting relationship with the other side wall of the channel-shaped part through different stroke lengths and at different stroke speeds; and (b) with the first radially inwardly most disposed slide being moved farther and faster than the second radially outwardly most disposed slide to produce a rolling movement of the material of the channel-shaped part with the radially inwardly most disposed material thereof moving farthest and being welded to the material of the channel-shaped part lying on the fixed mold surface.
Claim 2
Dependent Claim 245 words
In the method of producing a chime projecting radially outwardly on a blow-molded hollow member of thermoplastic material by forming the chime directly from the still hot hollow member by actuation of axially movable slide means toward an axially aligned fixed mold surface of a divided blow mold after the two mold halves have been brought together and after a plastic parison gripped between the mold halves has been inflated to a given shape to form the hollow member with a radially outwardly projecting annular channel-shaped part having one side wall thereof lying against the fixed mold surface, its other side wall lying against the slide means and the bottom outer wall lying against a radially outwardly disposed axial surface of the mold, by moving the slide means axially of the hollow member toward the fixed mold surface, the improvement characterized in that: (a) the slide means, which are defined by multi-part first and second slides telescoped on one another, are moved axially in supporting relationship with the other side wall of the channel-shaped part through different stroke lengths and at different stroke speeds; and (b) with the first radially inwardly most disposed slide being moved farther and faster than the second radially outwardly most disposed slide to produce a rolling movement of the material of the channel-shaped part with the radially inwardly most disposed material thereof moving farthest and being welded to the material of the channel-shaped part lying on the fixed mold surface.
Claim 3
Dependent Claim 31 words
The improvement in the method according to claim 1 characterized in that: (a) the second slide is moved at no more than half of the stroke speed of the first slide.
Claim 4
Dependent Claim 25 words
The improvement in the method according to either of claims 1 or 2 characterized in that: (a) the chime is formed with a hollow interior.
Claim 5
Dependent Claim 24 words
The improvement in the method according to claim 3 further characterized by: (a) simultaneously forming said chime adjacent both ends of the hollow member.
Claim 6
Dependent Claim 200 words
In the method of producing a chime projecting radially outwardly on a blow molded hollow member of thermoplastic material immediately after the forming of the hollow member in a molding apparatus with end walls and a side wall of the hollow member having a radially outwardly projecting annular channel-shaped part extending circumferentially around the hollow member and defined by a radially outwardly spaced outer wall and two axially spaced connecting side walls connecting the axially spaced ends of the outer wall to the side wall of the hollow member, the improvement characterized by: (a) moving the radially inner end of one of the connecting side walls axially toward and into contact with the aligned radial inner end of the other connecting side wall at a first speed; (b) simultaneously, and independently of the radial inner end of the one connecting side wall supporting and moving the adjacent portion of the remaining part of the one connecting side wall toward the other connecting side wall at a second speed less than said first speed; and (c) pressing the contacting radial inner ends of the connecting side walls against each other to weld them together to form said radially outwardly projecting chime.
Claim 7
Dependent Claim 200 words
In the method of producing a chime projecting radially outwardly on a blow molded hollow member of thermoplastic material immediately after the forming of the hollow member in a molding apparatus with end walls and a side wall of the hollow member having a radially outwardly projecting annular channel-shaped part extending circumferentially around the hollow member and defined by a radially outwardly spaced outer wall and two axially spaced connecting side walls connecting the axially spaced ends of the outer wall to the side wall of the hollow member, the improvement characterized by: (a) moving the radially inner end of one of the connecting side walls axially toward and into contact with the aligned radial inner end of the other connecting side wall at a first speed; (b) simultaneously, and independently of the radial inner end of the one connecting side wall supporting and moving the adjacent portion of the remaining part of the one connecting side wall toward the other connecting side wall at a second speed less than said first speed; and (c) pressing the contacting radial inner ends of the connecting side walls against each other to weld them together to form said radially outwardly projecting chime.
Claim 8
Dependent Claim 49 words
The improvement in the method according to claims 5 further characterized by: (a) moving the adjacent portion of the remaining part of the one connecting side wall at a speed no greater than half the speed of movement of the radial inner end of the one connecting side wall.
Claim 9
Dependent Claim 63 words
The improvement in the method according to claim 5 characterized in that: (a) the material in the one connecting side wall is moved toward the other connecting side wall without significant compression of any of the material of the channel-shaped part by a rolling action of the material in the one connecting side wall and in the adjacent part of the outer wall.
Claim 10
Dependent Claim 46 words
The improvement in the method according to claim 5 further characterized by: (a) maintaining at least part of the outer wall spaced from the side wall of the hollow member during movement of the one connecting side wall to form a chime having a hollow interior.
Claim 11
Dependent Claim 94 words
The improvement in the method according to claim 8 characterized in that: (a) the wall material of the hollow member and the channel-shaped part immediately after the blow molding operation has a thickness varying from a minimum to a maximum as measured at different points about its circumference; and (b) the material of the channel-shaped part greater than the minimum thickness is directed into the hollow interior of the chime during its formation to produce a chime having an outer shape and size which is constant about the entire circumference of the hollow member.
Claim 12
Dependent Claim 26 words
The improvement in the method according to claim 8 further characterized by: (a) forming radially inwardly directed indentations in the outer side wall of the chime.
Claim 13
Dependent Claim 26 words
The improvement in the method according to claim 8 further characterized by: (a) forming axially directed indentations in the one connecting side wall of the chime.
Claim 14
Dependent Claim 21 words
The improvement in the method according to claim 8 further characterized by: (a) cutting off the outer wall of the chime.
Claim 15
Dependent Claim 63 words
The improvement in the method according to claim 8 further characterized by: (a) forming the chime adjacent one end of the hollow member with one of the connecting side walls radially aligned with said one end of the hollow member; and (b) cutting off said connecting side wall together with the adjacent end of the hollow member for insertion of a separate cover.

References Cited (Backward Citations)

GB911228A Cited
GB1001672A Cited
US4036926A Cited
US4022345A Cited
US4117062A Cited
US4228122A Cited
US4228916A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1986-03-28 1986-09-27 1987-03-29 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1990-03-28 1990-09-27 1991-03-29 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1994-03-28 1994-09-27 1995-03-29 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.