Patent US4372987A successfully refreshed from Google Patents.
← Back to Patent Explorer
US4372987A Expired / Lapsed US ⏱️ 0.0 years remaining

Method of producing a multilayer anti-reflection coating

Assignee: D Swarovski KG
•
Filing: 1981-03-09
•
Granted: 1983-02-08
•
Expires: 2001-03-09
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method of producing a multilayer anti-reflection coating with an interference effect for optical purposes, and optical bodies with a multilayer anti-reflection coating is described, of which at least one layer has a low refractive index, at least one other layer has a medium refractive index, and--if necessary--other layers have a high refractive index, and whereby the layer of medium refractive value is produced by depositing a mixture of tantalic oxide and aluminum oxide by means of an electron gun in a vacuum in a reactive atmosphere.

Inventors

  • 👤 Peter Ganner
  • 👤 Theodor Wallner

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-04 07:50
CPC Classifications
C; C03; C03C; C03C17/00; C03C17/34; C03C17/3411; C03C17/3429; C03C17/3447; C03C17/3452; C03C17/22; C03C17/23; C03C17/245; C03C17/3417; C03C2217/00; C03C2217/20; C03C2217/21; C03C2217/218; C03C2217/23; C03C2218/00; C03C2218/10; C03C2218/15; C03C2218/152

Claims Analysis

Total Claims: 7
Claim 1
Independent Claim 90 words
A method of producing a multilayer anti-reflection coating with an interference effect for optical purposes upon a substrate, of which at least one layer of the coating has a low refractive index, below n=1.65, and at least one other layer of the coating has a medium refractive index, from n=1.65 to n=1.80, comprising producing the layer of medium refractive value in a vacuum in a reactive atmosphere by depositing upon said substrate a mixture of tantalic oxide and aluminum oxide which has been vaporized by means of an electron gun.
Claim 2
Independent Claim 90 words
A method of producing a multilayer anti-reflection coating with an interference effect for optical purposes upon a substrate, of which at least one layer of the coating has a low refractive index, below n=1.65, and at least one other layer of the coating has a medium refractive index, from n=1.65 to n=1.80, comprising producing the layer of medium refractive value in a vacuum in a reactive atmosphere by depositing upon said substrate a mixture of tantalic oxide and aluminum oxide which has been vaporized by means of an electron gun.
Claim 3
Dependent Claim 26 words
A method according to claim 1 characterized in that at least one of the layers of medium refractive value is the layer next to the substrate.
Claim 4
Dependent Claim 66 words
A method according to claim 1 or 2 characterized in that a first layer of medium refractive value out of a mixture of tantalic oxide and aluminum oxide in a thickness of λ/4, a second layer of high refractive value, above n=1.80, in a thickness of λ/2 and a third layer of low refractive value in a thickness of λ/4 are deposited consecutively on the substrate.
Claim 5
Dependent Claim 52 words
A method according to claim 1 or 2 characterized in that a first layer of medium refractive value out of a mixture of tantalic oxide and aluminum oxide in a thickness of λ/4 and a second layer of low refractive value in a thickness of λ/4 are deposited consecutively on a substrate.
Claim 6
Dependent Claim 39 words
A method according to claim 1 or 2 characterized in that the layer of medium refractive value is formed by depositing a mixture of 25 to 95 wt. % tantalic oxide and 5 to 75 wt. % aluminum oxide.
Claim 7
Dependent Claim 42 words
A method according to claim 3 characterized in that the first layer is a mixture of approximately 30-40 wt. % tantalic oxide and approximately 60-70 wt. % aluminum oxide, the second layer is tantalic oxide and the third layer is magnesium fluoride.

References Cited (Backward Citations)

US3185020A Cited
US3604784A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1986-02-07 1986-08-09 1987-02-08 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1990-02-07 1990-08-09 1991-02-08 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1994-02-07 1994-08-09 1995-02-08 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag