Patent US4370027A successfully refreshed from Google Patents.
← Back to Patent Explorer
US4370027A Expired / Lapsed US ⏱️ 0.0 years remaining

Anti-reflection film with an ion-penetration prevention layer

Assignee: Nikon Corp
•
Filing: 1981-01-09
•
Granted: 1983-01-25
•
Expires: 2001-01-09
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract In an anti-reflection film comprising a low refractive index substance and a high refractive index substance alternately layered on a glass substrate, the layers of the high refractive index substance is formed of a transition metal oxide which interacts with the Na + or the Pb ++ ions in the glass substrate to produce a light scattering product, and at least one of the layers of transition metal oxide is substituted for by a layer formed of a substance having a higher packing density than that of the high refractive index and the low refractive index substance.

Inventors

  • 👤 Masatoshi Sato
  • 👤 Yosuke Takahashi

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 13:22
CPC Classifications
G; G02; G02B; G02B1/00; G02B1/10; G02B1/11; G02B1/113; G02B1/115

Claims Analysis

Total Claims: 13
Claim 1
Independent Claim 108 words
An anti-reflection film on a glass substrate containing Na + or Pb ++ ions, comprising: a low refractive index substance layer disposed on said glass substrate; a high packing density layer formed of a substance of which a packing density is so high as to prevent penetration of said ions, said high packing density layer being disposed on said low refractive index substance layer; and plural pairs of layers A and B superimposed on said high packing density layer in the order of ABAB from the high packing density layer, where A is a low refractive index substance layer; and B is a high refractive index substance layer.
Claim 2
Dependent Claim 108 words
An anti-reflection film on a glass substrate containing Na + or Pb ++ ions, comprising: a low refractive index substance layer disposed on said glass substrate; a high packing density layer formed of a substance of which a packing density is so high as to prevent penetration of said ions, said high packing density layer being disposed on said low refractive index substance layer; and plural pairs of layers A and B superimposed on said high packing density layer in the order of ABAB from the high packing density layer, where A is a low refractive index substance layer; and B is a high refractive index substance layer.
Claim 3
Dependent Claim 134 words
An anti-reflection film on a glass substrate containing Na + or Pb ++ ions, comprising: first, second, third and fourth low refractive index substance layers; first high refractive index substance layer formed of a transition metal oxide; and first and second high packing density layers of a substance of which a packing density is so high as to prevent penetration of said ions, the layers being superimposed on said glass substrate in the order, from the substrate, of said first low refractive index substance layer, said first high packing density layer, said second low refractive index layer, said second high packing density layer, said third low refractive index substance layer, said first high refractive index substance layer, and said fourth low refractive index substance layer being disposed in this order on said glass substrate.
Claim 4
Dependent Claim 134 words
An anti-reflection film on a glass substrate containing Na + or Pb ++ ions, comprising: first, second, third and fourth low refractive index substance layers; first high refractive index substance layer formed of a transition metal oxide; and first and second high packing density layers of a substance of which a packing density is so high as to prevent penetration of said ions, the layers being superimposed on said glass substrate in the order, from the substrate, of said first low refractive index substance layer, said first high packing density layer, said second low refractive index layer, said second high packing density layer, said third low refractive index substance layer, said first high refractive index substance layer, and said fourth low refractive index substance layer being disposed in this order on said glass substrate.
Claim 5
Dependent Claim 49 words
An anti-reflection film according to claim 2, further comprising: a second high refractive index substance layer formed of a transition metal oxide and disposed on said fourth low refractive index substance layer; and a fifth low refractive index substance layer disposed on said second high refractive index substance layer.
Claim 6
Dependent Claim 98 words
An anti-reflection film on a glass substrate containing Na + and Pb ++ ions, comprising: a low refractive index substance layer disposed on said glass substrate; an ion-penetration preventing layer formed of one of Al 2 O 3 and SiO 2 for preventing penetration of said ions and disposed on said low refractive index substance layer; and plural pairs of layers A and B superimposed on said ion-penetration preventing layer in the order of ABAB therefrom, where A is a low refractive index substance layer and B is a high refractive index layer of a transition metal oxide.
Claim 7
Dependent Claim 98 words
An anti-reflection film on a glass substrate containing Na + and Pb ++ ions, comprising: a low refractive index substance layer disposed on said glass substrate; an ion-penetration preventing layer formed of one of Al 2 O 3 and SiO 2 for preventing penetration of said ions and disposed on said low refractive index substance layer; and plural pairs of layers A and B superimposed on said ion-penetration preventing layer in the order of ABAB therefrom, where A is a low refractive index substance layer and B is a high refractive index layer of a transition metal oxide.
Claim 8
Dependent Claim 119 words
An anti-reflection film on a glass substrate containing Na + and Pb ++ ions, comprising: first, second, third and fourth low refractive index substance layers; a first high refractive index substance layer formed of a transition metal oxide; and first and second ion-penetration preventing layers formed of one of Al 2 O 3 and SiO 2 for preventing penetration of said ions the layers being superimposed in the order, from the substrate, of said first low refractive index substance layer, said first ion-penetration preventing layer, said second low refractive index substance layer, said second ion-penetration preventing layer, said third low refractive index substance layer, said first high refractive index substance layer, and said fourth low refractive index substance layer.
Claim 9
Dependent Claim 119 words
An anti-reflection film on a glass substrate containing Na + and Pb ++ ions, comprising: first, second, third and fourth low refractive index substance layers; a first high refractive index substance layer formed of a transition metal oxide; and first and second ion-penetration preventing layers formed of one of Al 2 O 3 and SiO 2 for preventing penetration of said ions the layers being superimposed in the order, from the substrate, of said first low refractive index substance layer, said first ion-penetration preventing layer, said second low refractive index substance layer, said second ion-penetration preventing layer, said third low refractive index substance layer, said first high refractive index substance layer, and said fourth low refractive index substance layer.
Claim 10
Dependent Claim 132 words
An anti-reflection film on a glass substrate containing Na + or Pb ++ ions, comprising: a low refractive index substance layer disposed on said glass substrate; a high packing density layer formed of a substance of which the packing density is so high as to prevent penetration of said ions, said high packing density layer being disposed on said low refractive index substance layer; and plural pairs of a low refractive index substance layer and a high refractive index substance layer, said pairs being disposed alternately on said high packing density layer so that said low refractive index substance layer of one of said plural pairs located nearest to said high packing density layer is disposed on the same, said high refractive index substance layers being formed of a transition metal oxide.
Claim 11
Dependent Claim 132 words
An anti-reflection film on a glass substrate containing Na + or Pb ++ ions, comprising: a low refractive index substance layer disposed on said glass substrate; a high packing density layer formed of a substance of which the packing density is so high as to prevent penetration of said ions, said high packing density layer being disposed on said low refractive index substance layer; and plural pairs of a low refractive index substance layer and a high refractive index substance layer, said pairs being disposed alternately on said high packing density layer so that said low refractive index substance layer of one of said plural pairs located nearest to said high packing density layer is disposed on the same, said high refractive index substance layers being formed of a transition metal oxide.
Claim 12
Dependent Claim 124 words
An anti-reflection film on a glass substrate containing Na + or Pb ++ ions, comprising: a low refractive index substance layer disposed on said glass substrate; an ion-penetration preventing layer formed of one of Al 2 O 3 and SiO 2 for preventing penetration of said ions and disposed on said low refractive index substance layer; and plural pairs of a low refractive index substance layer and a high refractive index substance layer, said pairs being disposed alternately on said high packing density layer so that said low refractive index substance layer of one of said plural pairs located nearest to said high packing density layer is disposed on the same, said high refractive index substance layers being formed of a transition metal oxide.
Claim 13
Dependent Claim 124 words
An anti-reflection film on a glass substrate containing Na + or Pb ++ ions, comprising: a low refractive index substance layer disposed on said glass substrate; an ion-penetration preventing layer formed of one of Al 2 O 3 and SiO 2 for preventing penetration of said ions and disposed on said low refractive index substance layer; and plural pairs of a low refractive index substance layer and a high refractive index substance layer, said pairs being disposed alternately on said high packing density layer so that said low refractive index substance layer of one of said plural pairs located nearest to said high packing density layer is disposed on the same, said high refractive index substance layers being formed of a transition metal oxide.

References Cited (Backward Citations)

US3423147A Cited
US3738732A Cited
US3649359A Cited
US3781090A Cited
US4128303A Cited
US4132959A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1986-01-24 1986-07-26 1987-01-25 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1990-01-24 1990-07-26 1991-01-25 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1994-01-24 1994-07-26 1995-01-25 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag