Patent US4638495A successfully refreshed from Google Patents.
Patent US4367986A successfully refreshed from Google Patents.
← Back to Patent Explorer
US4367986A Expired / Lapsed US ⏱️ 0.0 years remaining

Method for improving the strength of a water-saturated soft soil

Assignee: Chiyoda Corp
•
Filing: 1981-10-08
•
Granted: 1983-01-11
•
Expires: 2001-10-08
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A water-saturated soft soil is efficiently improved in its strength by incorporating therein an additive composed of ingredients A and B; the ingredient A comprises gypsum and the ingredient B comprises a mixture of 40-55% by weight of a Portland cement and 60-45% by weight of a water-granulated iron blast furnace slag having a particle size almost equal to or smaller than that of the Portland cement. The ratio by weight of the ingredient A to the ingredient B ranges from 10/90 to 30/70 and the total amount of the ingredients A and B used for the soft soil is sufficient to strengthen the soft soil.

Inventors

  • 👤 Hajime Miyoshi
  • 👤 Ikuo Okabayashi
  • 👤 Etsuo Asanagi

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 12:40
CPC Classifications
C; C09; C09K; C09K17/00; C09K17/02; C09K17/04

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 101 words
A method for improving the strength of a water-saturated soft soil, which comprises admixing the soft soil with an ingredient A comprising gypsum and an ingredient B comprising a mixture of 40-55% by weight of a Portland cement and 60-45% by weight of a water-granulated iron blast furnace slag, the slag having a particle size almost the same as or less than that of the cement, the ratio by weight of the ingredient A to the ingredient B being within the range from 10/90 to 30/70, and the soft soil being admixed with the ingredient A simultaneously with the ingredient B.
Claim 2
Independent Claim 101 words
A method for improving the strength of a water-saturated soft soil, which comprises admixing the soft soil with an ingredient A comprising gypsum and an ingredient B comprising a mixture of 40-55% by weight of a Portland cement and 60-45% by weight of a water-granulated iron blast furnace slag, the slag having a particle size almost the same as or less than that of the cement, the ratio by weight of the ingredient A to the ingredient B being within the range from 10/90 to 30/70, and the soft soil being admixed with the ingredient A simultaneously with the ingredient B.
Claim 3
Dependent Claim 26 words
A method according to claim 1, wherein the total amount of the ingredients A and B is 50-50 kg per cubic meter of the soft soil.
Claim 4
Dependent Claim 14 words
A method according to claim 1, wherein the Portland cement is Ordinary Portland cement.

References Cited (Backward Citations)

US1748839A Cited
US2182714A Cited
US2947643A Cited
US3947284A Cited
US4209335A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1986-01-10 1986-07-12 1987-01-11 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1990-01-10 1990-07-12 1991-01-11 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1994-01-10 1994-07-12 1995-01-11 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag