Aqueously-swelling water stopper and a process of stopping water thereby
Assignee: Hayakawa Rubber Co Ltd
•
Filing: 1981-01-21
•
Granted: 1982-12-28
•
Expires: 2001-01-21
Abstract
Abstract The disclosed water stopper and water stopping process use an aqueously-swelling water-stopping composition consisting of 10 to 40 weight % of rubber whose main ingredient is reclaimed rubber, 10 to 20 weight % of silicic compound, 10 to 60 weight % of bentonite, and 10 to 40 weight % of plasticizer. The aforesaid water-stopping composition may be extruded into an elongated water stopper with or without a core therein, which water stopper can be inserted into a joint gap or other gap of structural members to stop water at the gap.
Inventors
- 👤 Yoshinobu Ishido
- 👤 Hideo Tanaka
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-05 19:44
CPC Classifications
C; C09; C09K; C09K3/00; C09K3/10; E; E04; E04B; E04B1/00; E04B1/62; E04B1/66; E04B1/68; E04B1/6801; E04B1/6813; C09K2003/1034; C09K2003/104; C09K2200/00; C09K2200/02; C09K2200/0243; C09K2200/0252; C09K2200/0256; C09K2200/06; C09K2200/0607; C09K2200/061; C09K2200/0615; C09K2200/0617; C09K2200/0642; Y; Y10; Y10S; Y10S277/00; Y10S277/934; Y10S277/935; Y10S277/944
Claims Analysis
Total Claims: 7
Claim 1
Independent Claim
80 words
Aqueously-swelling water-stopping composition consisting of 10 to 40 weight % of rubber whose main ingredient is reclaimed rubber blended with less than 30 weight % of virgin rubber, 10 to 20 weight % of silicic compound, 10 to 60 weight % of bentonite, said silicic compound and bentonite acting as fillers and said silicic compound being selected from the group consisting of silicic acid anhydride, hydrous silicic acid, and calcium silicate, and 10 to 40 weight % of rubber plasticizer.
Claim 2
Dependent Claim
82 words
Aqueously-swelling water-stopping composition consisting of 10 to 40 weight % of reclaimed rubber; 10 to 30 weight % of virgin rubber, said reclaimed rubber and virgin rubber being present in a total amount of 10 to 40 weight %; 10 to 20 weight % of silicic compound, said silicic compund being selected from the group consisting of silicic acid anhydride, hydrous silicic acid, and calcium silicate; 10 to 60 weight % of bentonite; and 10 to 40 weight % of rubber plasticizer.
Claim 3
Dependent Claim
18 words
Aqueously-swelling water-stopping composition as set forth in claim 1, wherein said plasticizer is a plasticizer for reclaimed rubber.
Claim 4
Dependent Claim
78 words
An extruded water stopper made of aqueously-swelling water-stopping composition consisting of 10 to 40 weight % of rubber whose main ingredient is reclaimed rubber blended with less than 30 weight % of virgin rubber; 10 to 20 weight % of silicic compound, said silicic compound being selected from the group consisting of silicic acid anhydride, hydrous silicic acid, and calcium silicate carbon; 10 to 60 weight % of bentonite; and 10 to 40 weight % of rubber plasticizer.
Claim 5
Dependent Claim
27 words
Aqueously-swelling water-stopping composition as set forth in claim 1, wherein said reclaimed rubber is selected from the group consiting of reclaimed butyl rubber and reclaimed tire rubber.
Claim 6
Dependent Claim
34 words
Aqueously-swelling water-stopping composition as set forth in claim 1, wherein said virgin rubber is selected from the group consisting of butyl rubber, butyl halide rubber, polyisobutylene rubber, ethylene propylene-diene terpolymer rubber and ethylene-propylene rubber.
Claim 7
Dependent Claim
33 words
Aqueously-swelling water-stopping composition as set forth in claim 1, wherein said rubber plasticizer is selected from the group consisting of mineral oil softeners, vegetable oil softeners, fatty acids, esters, phosphates, and paraffinic derivates.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1985-12-27 | 1986-06-28 | 1986-12-28 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1989-12-27 | 1990-06-28 | 1990-12-28 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1993-12-27 | 1994-06-28 | 1994-12-28 | $7700.00 | Window Closed / Lapsed |