Patent US4362677A successfully refreshed from Google Patents.
← Back to Patent Explorer
US4362677A Expired / Lapsed US ⏱️ 0.0 years remaining

Method of producing ethylene-vinyl alcohol copolymer hollow fiber membranes

Assignee: Kuraray Co Ltd
•
Filing: 1981-06-04
•
Granted: 1982-12-07
•
Expires: 2001-06-04
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A hollow fiber membrane made of an ethylene-vinyl alcohol copolymer is provided, which is characterized in that, when observed in a dry state with an electron microscope, the hollow fiber membrane has at least one dense, active layer (or skin layer) on the inside and/or outside surface thereof and further a three-layered structure comprising two layers respectively contacting the inside and outside surfaces and each consisting of a plurality of particles bonded together and having particle sizes of 0.01 to 2 microns and a substantially particle-free homogeneous layer lying between the two layers. A method of producing such hollow fiber membranes is also provided comprising spinning a spinning solution prepared by dissolving an ethylene-vinyl alcohol copolymer in a solvent mainly consisting of dimethyl sulfoxide, dimethylacetamide, pyrrolidone, N-methylpyrrolidone or a mixture of these through a spinneret for hollow fiber production while simultaneously introducing a coagulating liquid through the central aperture of said spinneret, passing the spun fiber through a gaseous atmosphere such that the fiber is drawn to 3 to 30 times its original length, and coagulating the fiber in a coagulation bath at a temperature within the range specified below: When 15</=C</=40, -15</=T</=1/4C+10 where C is polymer concentration (weight %) and T is coagulation temperature ( DEG C.).

Inventors

  • 👤 Shuzo Yamashita
  • 👤 Taku Tanaka
  • 👤 Hirokuni Tanii
  • 👤 Akira Kubotsu
  • 👤 Syuji Kawai

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 16:04
CPC Classifications
D; D01; D01F; D01F6/00; D01F6/28; D01F6/30; B; B01; B01D; B01D69/00; B01D69/08; B01D71/00; B01D71/06; B01D71/38; B01D71/381; D01D; D01D5/00; D01D5/24; D01F6/34; Y; Y10; Y10T; Y10T428/00; Y10T428/29; Y10T428/2913; Y10T428/2933; Y10T428/2935; Y10T428/2973; Y10T428/2975

Claims Analysis

Total Claims: 9
Claim 1
Independent Claim 117 words
A method for producing a hollow fiber membrane of ethylene-vinyl alcohol copolymer, which comprises spinning a spinning solution prepared by dissolving an ethylene-vinyl alcohol copolymer in a solvent selected from the group consisting of dimethyl sulfoxide, dimethylacetamide, pyrrolidone, N-methyl-pyrrolidone or mixtures thereof through a spinneret for hollow fiber production while introducing a coagulating liquid through the central aperture of said spinneret, passing the spun fiber through a gaseous atmosphere while drawing the fiber 3 to 30 times its original length, and subsequently coagulating the fiber in a coagulation bath at a temperature within the range satisfying the following relationship: when 15≦C≦40, -15≦T≦1/4C+3.5 where C is the polymer concentration (weight %) and T is the coagulation temperature (°C.).
Claim 2
Independent Claim 117 words
A method for producing a hollow fiber membrane of ethylene-vinyl alcohol copolymer, which comprises spinning a spinning solution prepared by dissolving an ethylene-vinyl alcohol copolymer in a solvent selected from the group consisting of dimethyl sulfoxide, dimethylacetamide, pyrrolidone, N-methyl-pyrrolidone or mixtures thereof through a spinneret for hollow fiber production while introducing a coagulating liquid through the central aperture of said spinneret, passing the spun fiber through a gaseous atmosphere while drawing the fiber 3 to 30 times its original length, and subsequently coagulating the fiber in a coagulation bath at a temperature within the range satisfying the following relationship: when 15≦C≦40, -15≦T≦1/4C+3.5 where C is the polymer concentration (weight %) and T is the coagulation temperature (°C.).
Claim 3
Dependent Claim 46 words
A method as claimed in claim 1, wherein said coagulating liquid to be introduced into the central aperture of the spinneret is a solution whose solvent is the same as the solvent for the spinning solution and which contains 40 to 70% by weight of water.
Claim 4
Dependent Claim 25 words
A method as defined in claim 1 wherein the ethylene-vinyl alcohol copolymer additionally contains up to and including 15 mole % of another copolymerizable comonomer.
Claim 5
Dependent Claim 27 words
A method as defined in claim 1 wherein up to and including 30 mole % of the functional hydroxyl groups in the vinyl alcohol units are acetalized.
Claim 6
Dependent Claim 20 words
A method as defined in claim 1 wherein the fiber is drawn from 5 to 20 times its original length.
Claim 7
Dependent Claim 19 words
A method as defined in claim 1 wherein the ethylene-vinyl alcohol copolymer is cross-linked either before or after spinning.
Claim 8
Dependent Claim 17 words
A method as defined in claim 1 wherein the solvent for the spinning solution is dimethyl sulfoxide.
Claim 9
Dependent Claim 26 words
A method as defined in claim 1 wherein the distance between the spinneret and the surface of the coagulation bath is about 3 to 50 mm.

References Cited (Backward Citations)

FR1586563A Cited
FR2196184B1 Cited
FR2199014B1 Cited
US4134837A Cited
FR2314215B1 Cited
FR2324337B1 Cited
FR2401949A1 Cited
US4220543A Cited
FR2435276A1 Cited
US4269713A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1985-12-06 1986-06-07 1986-12-07 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1989-12-06 1990-06-07 1990-12-07 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1993-12-06 1994-06-07 1994-12-07 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag