Patent US4357459A successfully refreshed from Google Patents.
← Back to Patent Explorer
US4357459A Expired / Lapsed US ⏱️ 0.0 years remaining

Resins based on α-methyl styrene, styrene and a phenol

Assignee: Ingredion Inc
•
Filing: 1980-08-25
•
Granted: 1982-11-02
•
Expires: 2000-08-25
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Resins suitable for adhesives are based on α-methyl styrene, styrene and phenol in certain percentages, viz. 25 to 63, 35 to 73 and 2 to 15 percent by weight, respectively, Combinations of resin, ethylene vinyl acetate copolymer or thermoelastomer and optionally a wax or tackifying oil yield excellent adhesives, in particular hot-melt adhesives.

Inventors

  • 👤 Yves Runavot
  • 👤 Georges Billault
  • 👤 Jacques Salvetat

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-29 04:44
CPC Classifications
C; C09; C09J; C09J165/00; C08; C08F; C08F212/00; C08F212/02; C08F212/04; C08F212/06; C08F212/12; C08G; C08G61/00; C08G61/02; C09J125/00; C09J125/02; Y; Y10; Y10T; Y10T442/00; Y10T442/20; Y10T442/2738; Y10T442/2746

Claims Analysis

Total Claims: 3
Claim 1
Independent Claim 80 words
A resin having an average molecular weight of 400 to 2,000, which is useful in adhesives, based on a α-methyl styrene, styrene and a phenol as constituents, characterized in that the weight percentages of α-methyl styrene, styrene and a phenol with a structural formula ##STR2## in which R is hydrogen or a C 1 -C 12 alkyl group, which compounds are substantially the sole constituents, range from 25 to 63, from 35 to 73 and from 2 to 15 respectively.
Claim 2
Dependent Claim 80 words
A resin having an average molecular weight of 400 to 2,000, which is useful in adhesives, based on a α-methyl styrene, styrene and a phenol as constituents, characterized in that the weight percentages of α-methyl styrene, styrene and a phenol with a structural formula ##STR2## in which R is hydrogen or a C 1 -C 12 alkyl group, which compounds are substantially the sole constituents, range from 25 to 63, from 35 to 73 and from 2 to 15 respectively.
Claim 3
Dependent Claim 29 words
A resin according to claim 1, in which the weight percentages of the constituents range from 25 to 57, from 40 to 72 and from 3 to 10 respectively.

References Cited (Backward Citations)

US2247402A Cited
US2502003A Cited
US2600782A Cited
US2636905A Cited
US4032486A Cited
US4107144A Cited
JPS54150492A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1985-11-01 1986-05-03 1986-11-02 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1989-11-01 1990-05-03 1990-11-02 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1993-11-01 1994-05-03 1994-11-02 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag