Patent US4352332A successfully refreshed from Google Patents.
← Back to Patent Explorer
US4352332A Expired / Lapsed US ⏱️ 0.0 years remaining

Fluidized bed incineration of waste

Assignee: EI TECHNOLOGY Inc
•
Filing: 1980-06-19
•
Granted: 1982-10-05
•
Expires: 2000-06-19
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Apparatus and methods for fluidized bed incineration of waste containing phosphorus wherein the bed comprises lime or limestone which negates heretofore existing problems incident to the presence of phosphorus.

Inventors

  • 👤 Virgil F. Baston

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-02 10:14
CPC Classifications
G; G21; G21F; G21F9/00; G21F9/04; G21F9/06; G21F9/14; F; F23; F23G; F23G5/00; F23G5/30; F23G2209/00; F23G2209/18

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 142 words
A method of treating waste including phosphorus without precipitating difficulties due to creation of phosphoric acid, coating of parts causing reduced efficiency and contamination of bed particles comprising the steps of: introducing fuel into a vessel; introducing air into the vessel adequate to support fluidization and combustion; introducing waste comprising phosphorus material into the vessel; providing the vessel with a fluidized bed material comprising calcium and a vapor space above the fluidized bed; elevating the temperature of the fluidized bed to an elevated level within a range on the order of 750° C. to 950° C.; elevating the temperature of the vapor space to an elevated level within a range on the order of 600° C. to 900° C.; causing the waste to be placed in the bed simultaneously causing incineration of waste and formation of dry solid stable inert calcium phosphate.
Claim 2
Independent Claim 142 words
A method of treating waste including phosphorus without precipitating difficulties due to creation of phosphoric acid, coating of parts causing reduced efficiency and contamination of bed particles comprising the steps of: introducing fuel into a vessel; introducing air into the vessel adequate to support fluidization and combustion; introducing waste comprising phosphorus material into the vessel; providing the vessel with a fluidized bed material comprising calcium and a vapor space above the fluidized bed; elevating the temperature of the fluidized bed to an elevated level within a range on the order of 750° C. to 950° C.; elevating the temperature of the vapor space to an elevated level within a range on the order of 600° C. to 900° C.; causing the waste to be placed in the bed simultaneously causing incineration of waste and formation of dry solid stable inert calcium phosphate.
Claim 3
Dependent Claim 25 words
A method according to claim 1 further comprising removing the calcium phosphate from the bed material and replenishing the spent calcium in the fluidized bed.
Claim 4
Dependent Claim 30 words
A method according to claim 1 wherein the providing step comprises introducing into the vessel a composition selected from the group consisting of CaO, CaCO 3 and Ca(OH) 2 .
Claim 5
Independent Claim 142 words
A method of treating waste including tributyl phosphate to negate harmful side effects, comprising the steps of: introducing air, fuel and solvent radioactive waste containing tributyl phosphate into a vessel; providing the vessel with a fluidized bed material comprising calcium in the form of lime, limestone and/or slaked lime and a vapor space above the fluidized bed elevating the temperature of the fluidized bed to an elevated level within a range on the order of 750° C. to 950° C.; elevating the temperature of the vapor space to an elevated level within a range on the order of 600° C. to 900° C.; causing the fuel and radioactive waste to be placed in the bed and the air to be passed through the bed concurrently causing incineration of waste and formation of dry solid stable inert calcium phosphate from the tributyl phosphate.
Claim 6
Independent Claim 142 words
A method of treating waste including tributyl phosphate to negate harmful side effects, comprising the steps of: introducing air, fuel and solvent radioactive waste containing tributyl phosphate into a vessel; providing the vessel with a fluidized bed material comprising calcium in the form of lime, limestone and/or slaked lime and a vapor space above the fluidized bed elevating the temperature of the fluidized bed to an elevated level within a range on the order of 750° C. to 950° C.; elevating the temperature of the vapor space to an elevated level within a range on the order of 600° C. to 900° C.; causing the fuel and radioactive waste to be placed in the bed and the air to be passed through the bed concurrently causing incineration of waste and formation of dry solid stable inert calcium phosphate from the tributyl phosphate.

References Cited (Backward Citations)

US3556024A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1985-10-04 1986-04-05 1986-10-05 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1989-10-04 1990-04-05 1990-10-05 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1993-10-04 1994-04-05 1994-10-05 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag