Abstract

Abstract A process for applying a protective light-transmitting coating to a photoflash lamp comprising the steps of applying the protective coating to the lamp and curing the applied coating by exposure thereof to radiant energy and characterized by the improvement wherein the layer of coating applied to some portions of the photoflash lamp is thicker than the layer of coating applied to other portions of the photoflash lamp.

Inventors

  • 👤 John E. Tozier
  • 👤 John W. Shaffer

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-03 22:54
CPC Classifications
C; C03; C03C; C03C17/00; C03C17/001; C03C17/003; C03C17/005; B; B05; B05D; B05D1/00; B05D1/18; B05D1/30; C03C17/28; C03C17/32; F; F21; F21K; F21K5/00; F21K5/02; B05D1/002; B05D3/00; B05D3/06; B05D3/061; B05D3/065; B05D3/067

Claims Analysis

Total Claims: 12
Claim 1
Independent Claim 84 words
A process for coating a photoflash lamp with a UV-curable resin including the steps of applying varying amounts of UV-curable resin to different portions of the photoflash lamp and curing said UV-curable resin by impingement thereof with energy from a radiant energy source, said process characterized by the improvement wherein a different thickness of said UV-curable coating is applied to different portions of said photoflash lamp by a dip-coating process wherein said photoflash lamp is withdrawn from the coating composition at a non-uniform rate.
Claim 2
Dependent Claim 84 words
A process for coating a photoflash lamp with a UV-curable resin including the steps of applying varying amounts of UV-curable resin to different portions of the photoflash lamp and curing said UV-curable resin by impingement thereof with energy from a radiant energy source, said process characterized by the improvement wherein a different thickness of said UV-curable coating is applied to different portions of said photoflash lamp by a dip-coating process wherein said photoflash lamp is withdrawn from the coating composition at a non-uniform rate.
Claim 3
Dependent Claim 42 words
The process of claim 1 wherein said photoflash lamp includes an interconnecting tip portion, body portion and press portion with a coating of a greater thickness applied to said press portion than to said tip and body portions of said photoflash lamp.
Claim 4
Dependent Claim 54 words
The process of claim 1 wherein said photoflash lamp includes a tip portion, body portion and press portion with at least one of said portions being more failure-prone than the other portions and a thicker coating of UV-curable material applied to said failure-prone portion than to said other remaining portions of said photoflash lamp.
Claim 5
Dependent Claim 47 words
The process of claim 1 wherein said photoflash lamp includes tip, body and press portions with more than one of said portions prone to failure wherein a thicker coating of UV-curable material is applied to said failure-prone areas than to said remaining areas of said photoflash lamp.
Claim 6
Dependent Claim 46 words
The process of claim 1 wherein said applying of varying amounts of UV-curable coating is effected by a dip-coating process where said lamp is withdrawn from said coating at a non-uniform rate to provide a different thickness of coating on different portions of said photoflash lamp.
Claim 7
Dependent Claim 61 words
The process of claim 2 wherein said applying of varying amounts of UV-curable coating to different portions of said lamp is effected by a dip-coating process wherein said lamp is withdrawn from a coating at a non-uniform rate to provide an increased thickness of coating on said press portion as compared with said tip and body portions of said photoflash lamp.
Claim 8
Dependent Claim 79 words
In a process for applying a protective light-transmitting coating to the exterior surface of a photoflash lamp which includes the steps of varying the amount of coating applied to the various portions of the lamp and curing the applied protective light-transmitting coating, the improvement wherein dip-coating of the photoflash lamp is utilized to provide a different thickness of coating on different portions of the photoflash lamp by withdrawing said photoflash lamp from the coating composition at a non-uniform rate.
Claim 9
Dependent Claim 79 words
In a process for applying a protective light-transmitting coating to the exterior surface of a photoflash lamp which includes the steps of varying the amount of coating applied to the various portions of the lamp and curing the applied protective light-transmitting coating, the improvement wherein dip-coating of the photoflash lamp is utilized to provide a different thickness of coating on different portions of the photoflash lamp by withdrawing said photoflash lamp from the coating composition at a non-uniform rate.
Claim 10
Dependent Claim 54 words
In the process of claim 7 wherein said photoflash lamp includes tip, body and press portions with at least one of said portions being more failure-prone than the other portions, the improvement characterized by the application of a thicker layer of protective light-transmitting coating on said more failure-prone portions than on said other portions.
Claim 11
Dependent Claim 58 words
In the process of claim 7 wherein said photoflash lamp includes tip, body and press portions with said press portion being more prone to failure than said tip and body portions, the improvement wherein a thicker layer of protective light-transmitting coating is applied to said press portion than to said tip and body portions of said photoflash lamp.
Claim 12
Dependent Claim 56 words
In the process of claim 7 wherein said applying of a protective light-transmitting coating to the exterior surface of a photoflash lamp is effected by a dip-coating process, the improvement wherein said lamp is withdrawn from said coating at a non-uniform rate to provide a photoflash lamp with different lamp portions having a different coating thickness.

References Cited (Backward Citations)

DE1143708B Cited
US3953626A Cited
US3956540A Cited
US3956540B1 Cited
US4076489A Cited
US4207356A Cited
US4197333A Cited
US4232058A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1985-07-26 1986-01-25 1986-07-27 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1989-07-26 1990-01-25 1990-07-27 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1993-07-26 1994-01-25 1994-07-27 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag