Abstract
Abstract A method and apparatus for coating a glass container witb a layer of plastic whereby the container rotates about a horizontal axis and moves past a coating station. A plurality of liquid applicator nozzle means, positioned above the coating station, supply uncured plastic liquid to associated areas on the container. Means are provided for supplying predetermined quantities of uncured plastic liquid to respective ones of the nozzle means such that each nozzle means provides a coating of desired thickness and composition on its associated bottle area. The container is also rotated during the subsequent curing of the plastic.
Inventors
- 👤 Robert E. Waugh
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-04 05:17
CPC Classifications
C; C03; C03C; C03C17/00; C03C17/28; C03C17/32; C03C17/322; B; B05; B05B; B05B13/00; B05B13/02; B05B13/04; B05B13/0442; B05C; B05C13/00; B05C13/02; B05C13/025; B05C5/00; B05C5/002; Y; Y10; Y10T; Y10T428/00; Y10T428/13; Y10T428/131; Y10T428/1317; Y10T428/1321
Claims Analysis
Total Claims: 8
Claim 1
Independent Claim
136 words
A method of coating a glass container with a layer of plastic comprising: (a) rotating the container about a horizontal axis, (b) simultaneously applying uncured plastic liquid to a plurality of container surface areas by flow coating said plastic liquid from multiple nozzle means positioned along the length of the container and fixed stationarily with respect to that length, each said nozzle means having a multiple number of application tubes, the amount of uncured plastic liquid applied to each surface area by each nozzle means being independent of the amount of uncured plastic liquid applied to any other surface area, and resulting in an integral coating on the container which after cure resists wear during use and shattering of the bottle when dropped, and (c) curing said plastic liquid which has been applied to said container.
Claim 2
Independent Claim
136 words
A method of coating a glass container with a layer of plastic comprising: (a) rotating the container about a horizontal axis, (b) simultaneously applying uncured plastic liquid to a plurality of container surface areas by flow coating said plastic liquid from multiple nozzle means positioned along the length of the container and fixed stationarily with respect to that length, each said nozzle means having a multiple number of application tubes, the amount of uncured plastic liquid applied to each surface area by each nozzle means being independent of the amount of uncured plastic liquid applied to any other surface area, and resulting in an integral coating on the container which after cure resists wear during use and shattering of the bottle when dropped, and (c) curing said plastic liquid which has been applied to said container.
Claim 3
Dependent Claim
17 words
The method of claim 1 further comprising: (d) continuing to rotate the container as the plastic cures.
Claim 4
Dependent Claim
30 words
The method of claim 2 wherein said uncured plastic liquid is a liquid polyurethane having a polyether polyol component and an aliphatic diisocyanate component and which cures under infrared irradiation.
Claim 5
Dependent Claim
20 words
The method of claim 3 wherein the container is primed with a silane prior to being coated with said polyurethane.
Claim 6
Independent Claim
187 words
A method of coating a glass bottle with a layer of polyurethane comprising: (a) cleaning the bottle to be coated, (b) applying a silane primer to the bottle, (c) mixing a polyether polyol component and an aliphatic diisocyanate component to produce an uncured polyurethane coating composition, (d) metering a predetermined amount of said polyurethane coating compositon into each of four separate nozzle means each having a multiple number of applicator tubes and being positioned along the length of the bottle and fixed stationarily with respect to that length, (e) coating onto the primed bottle from each of said nozzle means as the bottle is rotated about a horizontal axis beneath said nozzle means to flow coat four adjacent zones of the bottle with said polyurethane coating composition to provide an integral coating, (f) heating the coated bottle for a period of time sufficient to cure said polyurethane coating composition while slowly rotating said bottle during heating, and (g) cooling the coated bottle, whereby there is produced a bottle uniformly coated with an integral polyurethane coating which resists wear during use and shattering of the bottle when dropped.
Claim 7
Independent Claim
187 words
A method of coating a glass bottle with a layer of polyurethane comprising: (a) cleaning the bottle to be coated, (b) applying a silane primer to the bottle, (c) mixing a polyether polyol component and an aliphatic diisocyanate component to produce an uncured polyurethane coating composition, (d) metering a predetermined amount of said polyurethane coating compositon into each of four separate nozzle means each having a multiple number of applicator tubes and being positioned along the length of the bottle and fixed stationarily with respect to that length, (e) coating onto the primed bottle from each of said nozzle means as the bottle is rotated about a horizontal axis beneath said nozzle means to flow coat four adjacent zones of the bottle with said polyurethane coating composition to provide an integral coating, (f) heating the coated bottle for a period of time sufficient to cure said polyurethane coating composition while slowly rotating said bottle during heating, and (g) cooling the coated bottle, whereby there is produced a bottle uniformly coated with an integral polyurethane coating which resists wear during use and shattering of the bottle when dropped.
Claim 8
Dependent Claim
25 words
The method of claim 5 wherein said primed bottle is preheated to 110°-130° F. before said polyurethane coating composition is cast onto the primed bottle.
References Cited (Backward Citations)
US2756647A
Cited
GB766673A
Cited
US3107183A
Cited
US3296999A
Cited
US3331521A
Cited
US3431889A
Cited
US3477870A
Cited
US3805985A
Cited
US3825141A
Cited
US3825142A
Cited
US3802380A
Cited
US3734765A
Cited
JPS4881688A
Cited
US3802908A
Cited
US3823032A
Cited
US3953626A
Cited
US3912100A
Cited
US3921575A
Cited
US3875893A
Cited
US3950199A
Cited
US4009301A
Cited
US3972435A
Cited
US4034708A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1983-06-10 | 1983-12-10 | 1984-06-10 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1987-06-10 | 1987-12-10 | 1988-06-10 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1991-06-10 | 1991-12-10 | 1992-06-10 | $7700.00 | Window Closed / Lapsed |