Process for the production of high grade carbonaceous binders

Assignee: Rain Carbon Germany GmbH
•
Filing: 1981-08-11
•
Granted: 1982-07-13
•
Expires: 2001-08-11
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A process is described for the production of high grade carbonaceous binders, wherein an aromatic high grade carbonaceous material is produced from 5-40% by weight of reduced or low ash coal or similar carbon containing raw materials by treatment with 20-80% by weight of high-boiling aromatic solvents, derived from coal, and 15-50% by weight of high-boiling aromatic solvents, derived from mineral oil, at temperatures of 300°-420° C. and for a reaction period of 1-4 hours, at a reaction pressure of up to 50 bar, and is optionally freed from low-boiling components.

Inventors

  • 👤 Jurgen Stadelhofer
  • 👤 Heinz-Gerhard Franck
  • 👤 Helmut Kohler
  • 👤 Heinrich Louis

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-08 22:43
CPC Classifications
C; C10; C10C; C10C3/00; C10C1/00; Y; Y10; Y10T; Y10T428/00; Y10T428/30

Claims Analysis

Total Claims: 7
Claim 1
Independent Claim 78 words
A process for the production of high grade carbonaceous binders, comprising producing an aromatic high grade carbonaceous material by treating from 5-40% by weight of low ash coal or similar carbon-containing raw materials with 20-80% by weight of high-boiling aromatic solvents, derived from coal, and 15-50% by weight of high-boiling aromatic solvents, derived from mineral oil, at temperatures of 300°-420° C. and for a reaction period of 1-4 hours, at a reaction pressure of up to 50 bar.
Claim 2
Dependent Claim 78 words
A process for the production of high grade carbonaceous binders, comprising producing an aromatic high grade carbonaceous material by treating from 5-40% by weight of low ash coal or similar carbon-containing raw materials with 20-80% by weight of high-boiling aromatic solvents, derived from coal, and 15-50% by weight of high-boiling aromatic solvents, derived from mineral oil, at temperatures of 300°-420° C. and for a reaction period of 1-4 hours, at a reaction pressure of up to 50 bar.
Claim 3
Dependent Claim 13 words
The process of claim 1 wherein the solvents are freed of low-boiling components.
Claim 4
Dependent Claim 28 words
The process according to claim 1, wherein the product obtained is homogeneously mixed with 0-60% by weight of hard pitch, derived from mineral oil or derived from coal.
Claim 5
Dependent Claim 13 words
A binder composition produced by the method of claims 1, 2 or 3.
Claim 6
Dependent Claim 16 words
An electrode impregnated with a binder produced by the method of claims 1, 2 or 3.
Claim 7
Independent Claim 36 words
A method of making a graphite electrode suitable for use in the electro-thermal refinement of metal ores comprising impregnating a carbon lattice with the binder composition produced by the method of claims 1, 2 or 3.

References Cited (Backward Citations)

DE1105379B Cited
US3849287A Cited
US3966585A Cited
US4072599A Cited
US4040941A Cited
US4188235A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1985-07-12 1986-01-11 1986-07-13 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1989-07-12 1990-01-11 1990-07-13 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1993-07-12 1994-01-11 1994-07-13 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag