Abstract

Abstract This invention is directed to a process for stabilizing polyvinyl chloride molding mixtures which comprises admixing (a) from about 0.2 to 5 parts by weight of a sodium aluminosilicate of small particle size; (b) from about 0.05 to 1.5 parts by weight of one or more calcium salts of fatty acids; (c) from about 0.05 to 0.5 parts by weight of one or more zinc salts of fatty acids; (d) from about 0.2 to 2.0 parts by weight of partial esters of polyols and fatty acids; and (e) from about 0.1 to 10 parts by weight of thioglycolic acid esters of polyols and/or thioglycolic acid esters of monofunctional alcohols per 100 parts by weight of polyvinyl chloride or copolymer of vinyl chloride.

Inventors

  • 👤 Kurt Worschech
  • 👤 Peter Wedl
  • 👤 Frido Loffelholz
  • 👤 Bernd Wegemund
  • 👤 Werner Erwied

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 12:51
CPC Classifications
C; C07; C07D; C07D209/00; C07D209/02; C07D209/04; C07D209/30; C07D209/42; C07C; C07C271/00; C07C271/06; C07C271/08; C07C271/10; C07C271/22; C07D207/00; C07D207/02; C07D207/30; C07D207/34; C07D207/36; C08; C08K; C08K5/00; C08K5/04; C08K5/09; C08K5/10; C08K5/101; C08K5/103; C08K5/36; C08K5/38

Claims Analysis

Total Claims: 31
Claim 1
Independent Claim 52 words
A process for stabilizing polyvinyl chloride molding mixtures, which comprises admixing (a) from about 0.2 to 5 parts by weight of a synthetic, crystalline sodium zeolite A of small particle size and containing from about 13 to 25 percent by weight of water of crystallization, which has the composition 0.7-1.1Na.sub.2 O.Al.sub.2 O.sub.3.1.3-2.4SiO.sub.2
Claim 2
Dependent Claim 52 words
A process for stabilizing polyvinyl chloride molding mixtures, which comprises admixing (a) from about 0.2 to 5 parts by weight of a synthetic, crystalline sodium zeolite A of small particle size and containing from about 13 to 25 percent by weight of water of crystallization, which has the composition 0.7-1.1Na.sub.2 O.Al.sub.2 O.sub.3.1.3-2.4SiO.sub.2
Claim 3
Dependent Claim 167 words
with respect to the anhydrous form; (b) from about 0.05 to 1.5 parts by weight of one or more calcium salts of fatty acids with from 8 to 22 carbon atoms; (c) from about 0.05 to 0.5 parts by weight of one or more zinc salts of fatty acids with from 8 to 22 carbon atoms; (d) from about 0.2 to 2.0 parts by weight of partial esters of polyols with from 2 to 6 carbon atoms and from 2 to 6 hydroxyl groups and fatty acids with from 8 to 22 carbon atoms, which contain an average of at least one free polyol-hydroxyl group per molecule and have an OH-number of from about 140 to 580; and (e) from about 0.1 to 10 parts by weight of thioglycolic acid esters of polyols with from 2 to 6 hydroxyl groups and/or thioglycolic acid esters of monofunctional alcohols with from 8 to 22 carbon atoms with 100 parts by weight of polyvinyl chloride or copolymer of vinyl chloride.
Claim 4
Dependent Claim 167 words
with respect to the anhydrous form; (b) from about 0.05 to 1.5 parts by weight of one or more calcium salts of fatty acids with from 8 to 22 carbon atoms; (c) from about 0.05 to 0.5 parts by weight of one or more zinc salts of fatty acids with from 8 to 22 carbon atoms; (d) from about 0.2 to 2.0 parts by weight of partial esters of polyols with from 2 to 6 carbon atoms and from 2 to 6 hydroxyl groups and fatty acids with from 8 to 22 carbon atoms, which contain an average of at least one free polyol-hydroxyl group per molecule and have an OH-number of from about 140 to 580; and (e) from about 0.1 to 10 parts by weight of thioglycolic acid esters of polyols with from 2 to 6 hydroxyl groups and/or thioglycolic acid esters of monofunctional alcohols with from 8 to 22 carbon atoms with 100 parts by weight of polyvinyl chloride or copolymer of vinyl chloride.
Claim 5
Dependent Claim 37 words
The process of claim 1, wherein a total of from about 1 to 100 parts by weight of components (a) to (e) are added per 100 parts by weight of polyvinyl chloride or copolymer of polyvinyl chloride.
Claim 6
Dependent Claim 37 words
The process of claim 1, wherein a total of from about 2 to 5 parts by weight of components (a) to (e) are added per 100 parts by weight of polyvinyl chloride of copolymer of vinyl chloride.
Claim 7
Dependent Claim 23 words
The process of claim 1, wherein the sodium zeolite A of component (a) has a particle size of from about 0.1 to 20μ.
Claim 8
Dependent Claim 34 words
The process of claim 1, wherein the sodium zeolite A of component (a) is a zeolite 4A containing water of crystallization with a water content of from about 18 to 25 percent by weight.
Claim 9
Dependent Claim 19 words
The process of claim 1, wherein component (d) comprises partial esters having an acid number less than about 15.
Claim 10
Dependent Claim 15 words
The process of claim 6, wherein the hydroxyl number is from about 170 to 540.
Claim 11
Dependent Claim 13 words
The process of claim 6, wherein the acid number is less than 8.
Claim 12
Dependent Claim 23 words
The process of claim 1, wherein component (e) comprises thioglycolates of aliphatic linear or branched monoalcohols and/or mono- and/or di-thioglycolates of said polyols.
Claim 13
Dependent Claim 74 words
The process of claim 1, wherein component (d) comprises a pentaerythritol partial ester of fatty acids having from 8 to 22 carbon atoms with a pentaerythritol to fatty acid molar ratio of from about 1:1 to 1:2 and component (e) comprises a thioglycolic acid ester of a monofunctional alcohol having from 8 to 18 carbon atoms, a monothioglycolic acid ester of aliphatic diols of from 2 to 6 carbon atoms, or a glyceryl monothioglycolate.
Claim 14
Dependent Claim 84 words
The process of claim 1 for stabilizing polyvinyl chloride molding mixtures to be used for the manufacture of tubing and profiles by extrusion method, wherein from about 0.5 to 1 part by weight of paraffin with a melting point of from about 50 ° to 110° C. and/or from about 0.5 to 1 part by weight of a fatty acid having from about 8 to 22 carbon atoms, is also admixed per 100 parts by weight of polyvinyl chloride or copolymer of vinyl chloride.
Claim 15
Dependent Claim 67 words
The process of claim 1 for stabilizing polyvinyl chloride molding mixtures to be used for the manufacture of hollowware by the extrusion blow method, wherein from about 0.5 to 5 parts by weight of epoxidized soybean oil and from about 0.1 to 0.8 parts by weight of high molecular ester wax, are also admixed per 100 parts by weight of polyvinyl chloride or copolymer of vinyl chloride.
Claim 16
Dependent Claim 76 words
The process of claim 1 for stabilizing polyvinyl molding mixtures to be used for the preparation of foils by the rolling calender method, wherein from about 0.5 to 5 parts by weight of epoxidized soybean oil, from about 0.1 to 1 part by weight of high-molecular ester wax, and 0.2 to 0.5 parts by weight of α-phenylindole or benzoyl-stearoyl methane are also admixed per 100 parts by weight of polyvinyl chloride or copolymer of vinyl chloride.
Claim 17
Dependent Claim 105 words
The process of claim 11, wherein (a) from about 1 to 2 parts by weight of said sodium zeolite A; (b) from about 0.8 to 1.2 parts by weight of said calcium salt or salts; (c) from about 0.1 to 0.4 parts by weight of said zinc salt or salts; (d) from about 0.3 to 0.5 parts by weight of said partial esters; (e) from about 0.2 to 0.5 parts by weight of said thioglycolic acid esters; and (f) from about 0.5 to 1 part by weight of the paraffin, are admixed per 100 parts by weight of polyvinyl chloride or copolymer of vinyl chloride.
Claim 18
Dependent Claim 207 words
A stabilizer composition of polyvinyl chloride molding mixtures which comprises (a) from about 4 to 100 parts by weight of a synthetic, crystalline sodium zeolite A of small particle size and containing from about 13 to 25 percent by weight of water of crystallization, which has the composition 0.7-1.1 Na.sub.2 O.Al.sub.2 O.sub.3.1.3-2.4 SiO.sub.2 with respect to the anhydrous form; (b) from about 1 to 30 parts by weight of one or more calcium salts of fatty acids with from 8 to 22 carbon atoms; (c) from about 1 to 10 parts by weight of one or more zinc salts of fatty acids with from 8 to 22 carbon atoms; (d) from about 4 to 40 parts by weight of partial esters of polyols with from 2 to 6 carbon atoms and from 2 to 6 hydroxyl groups and fatty acids with from 8 to 22 carbon atoms, which contain an average of at least one free polyol-hydroxyl group per molecule and have an OH-number of from about 140 to 580; and (e) from about 2 to 20 parts by weight of thioglycolic acid esters of polyols with from 2 to 6 hydroxyl groups and/or thioglycolic acid esters of monofunctional alcohols with from 8 to 22 carbon atoms.
Claim 19
Dependent Claim 207 words
A stabilizer composition of polyvinyl chloride molding mixtures which comprises (a) from about 4 to 100 parts by weight of a synthetic, crystalline sodium zeolite A of small particle size and containing from about 13 to 25 percent by weight of water of crystallization, which has the composition 0.7-1.1 Na.sub.2 O.Al.sub.2 O.sub.3.1.3-2.4 SiO.sub.2 with respect to the anhydrous form; (b) from about 1 to 30 parts by weight of one or more calcium salts of fatty acids with from 8 to 22 carbon atoms; (c) from about 1 to 10 parts by weight of one or more zinc salts of fatty acids with from 8 to 22 carbon atoms; (d) from about 4 to 40 parts by weight of partial esters of polyols with from 2 to 6 carbon atoms and from 2 to 6 hydroxyl groups and fatty acids with from 8 to 22 carbon atoms, which contain an average of at least one free polyol-hydroxyl group per molecule and have an OH-number of from about 140 to 580; and (e) from about 2 to 20 parts by weight of thioglycolic acid esters of polyols with from 2 to 6 hydroxyl groups and/or thioglycolic acid esters of monofunctional alcohols with from 8 to 22 carbon atoms.
Claim 20
Dependent Claim 25 words
The stabilizer composition of claim 15, wherein the sodium zeolite A of component (a) has a particle size of from about 0.1 to 20 μ.
Claim 21
Dependent Claim 35 words
The stabilizer composition of claim 15, wherein the sodium zeolite A of component (a) is a zeolite 4A containing water of crystallization with a water content of from about 18 to 25 percent by weight.
Claim 22
Dependent Claim 20 words
The stabilizer composition of claim 15, wherein component (d) comprises partial esters having an acid number less than about 15.
Claim 23
Dependent Claim 16 words
The stabilizer composition of claim 18, wherein the hydroxyl number is from about 150 to 540.
Claim 24
Dependent Claim 14 words
The stabilizer composition of claim 18, wherein the acid number is less than 8.
Claim 25
Dependent Claim 24 words
The stabilizer composition of claim 15, wherein component (e) comprises thioglycolates of aliphatic linear or branched monoalcohols and/or mono- and/or di-thioglycolates of said polyols.
Claim 26
Dependent Claim 69 words
The stabilizer composition of claim 15, wherein component (d) comprises a pentaerythritol partial ester of fatty acids having from 8 to 22 carbon atoms with a pentaerythritol:fatty acid molar ratio of from about 1:1 to 1:2 and component (e) comprises a thioglycolate of a monofunctional alcohol having from 8 to 18 carbon atoms, a monothioglycolate of aliphatic diols of from 2 to 6 carbon atoms, or a glyceryl monothioglycolate.
Claim 27
Dependent Claim 213 words
In a process for stabilizing polyvinyl chloride molding mixtures which comprises admixing a stabilizing amount of stabilizer with 100 parts by weight of polyvinyl chloride or copolymer of vinyl chloride the improvement consisting of using (a) from about 0.2 to 5 parts by weight of a synthetic, crystalline sodium zeolite A of small particle size and containing from about 13 to 25 percent by weight of water of crystallization, which has the composition 0.7-1.1 Na.sub.2 O.Al.sub.2 O.sub.3.1.3-2.4 SiO.sub.2 with respect to the anhydrous form; (b) from about 0.05 to 1.5 parts by weight of one or more calcium salts of fatty acids with from 8 to 22 carbon atoms; (c) from about 0.2 to 2.0 parts by weight of partial esters of polyols with from 2 to 6 carbon atoms and from 2 to 6 hydroxyl groups and fatty acids with from 8 to 22 carbon atoms, which contain an average of at least one free polyol-hydroxyl group per molecule and have an OH-number of from about 140 to 580; and (e) from about 0.1 to 10 parts by weight of polyols with from 2 to 6 hydroxyl groups and/or thioglycolic acid esters of such polyols and/or thioglycolis acid esters of monofunctional alcohols with from 8 to 22 carbon atoms for said stabilizer.
Claim 28
Dependent Claim 213 words
In a process for stabilizing polyvinyl chloride molding mixtures which comprises admixing a stabilizing amount of stabilizer with 100 parts by weight of polyvinyl chloride or copolymer of vinyl chloride the improvement consisting of using (a) from about 0.2 to 5 parts by weight of a synthetic, crystalline sodium zeolite A of small particle size and containing from about 13 to 25 percent by weight of water of crystallization, which has the composition 0.7-1.1 Na.sub.2 O.Al.sub.2 O.sub.3.1.3-2.4 SiO.sub.2 with respect to the anhydrous form; (b) from about 0.05 to 1.5 parts by weight of one or more calcium salts of fatty acids with from 8 to 22 carbon atoms; (c) from about 0.2 to 2.0 parts by weight of partial esters of polyols with from 2 to 6 carbon atoms and from 2 to 6 hydroxyl groups and fatty acids with from 8 to 22 carbon atoms, which contain an average of at least one free polyol-hydroxyl group per molecule and have an OH-number of from about 140 to 580; and (e) from about 0.1 to 10 parts by weight of polyols with from 2 to 6 hydroxyl groups and/or thioglycolic acid esters of such polyols and/or thioglycolis acid esters of monofunctional alcohols with from 8 to 22 carbon atoms for said stabilizer.
Claim 29
Dependent Claim 26 words
A molding mixture having a polymer with a preponderant content of vinyl chloride units which comprises a stabilizing amount of a stabilizer composition of claim 15.
Claim 30
Dependent Claim 12 words
The molding mixture of claim 24 wherein heavymetal containing stabilizers are absent.
Claim 31
Dependent Claim 64 words
The stabilizer composition of claim 15 which comprises from about 5 to 20 parts by weight of component (a); from about 2 to 10 parts by weight of component (b); from about 1 to 5 parts by weight of component (c); from about 3 to 10 parts by weight of component (d); and from about 1 to 5 parts by weight of component (e).

References Cited (Backward Citations)

US4000100A Cited
US4220570A Cited
US4202806A Cited
US4178282A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1985-07-05 1986-01-04 1986-07-06 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1989-07-05 1990-01-04 1990-07-06 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1993-07-05 1994-01-04 1994-07-06 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag