Patent US4320114A successfully refreshed from Google Patents.
US4320114A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Manufacture of aqueous polyvinylpyrrolidone-iodine solutions
Assignee: BASF SE
•
Filing: 1980-08-27
•
Granted: 1982-03-16
•
Expires: 2000-08-27
Abstract
Abstract Aqueous solutions of polyvinylpyrrolidone-iodine, generally referred to as PVP-iodine, which is finding increasing use because of its germicidal, bactericidal, fungicidal and disinfectant properties.
Inventors
- 👤 Walter Denzinger
- 👤 Karl Herrle
- 👤 Hans-Uwe Schenck
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-01 20:24
CPC Classifications
C; C08; C08F; C08F126/00; C08F126/06; C08F126/10; A; A01; A01N; A01N59/00; A01N59/12; A61; A61K; A61K33/00; A61K33/18; A61K47/00; A61K47/50; A61K47/51; A61K47/56; A61K47/58
Claims Analysis
Total Claims: 12
Claim 1
Independent Claim
244 words
A process for the preparation of a stable aqueous solution of PVP-iodine which comprises: mixing in an aqueous medium (a) PVP as an aqueous solution of from 10 to 60% strength by weight, wherein said PVP has a K value of from 8 to 50 and has been prepared in the form of an aqueous solution by the steps of (1) polymerizing vinylpyrrolidone in an organic solvent which is an aromatic hydrocarbon or a lower aliphatic monohydric alcohol of 1 to 4 carbon atoms at a concentration of monomer of from 10 to 80% by weight and in the presence of a free radical initiator which is an organic per-compound selected from the group consisting of alkyl hydroperoxides and dialkyl peroxides of 1 to 8 carbon atoms per alkyl and per esters in an amount of about 0.1 to 5% by weight, based on vinylpyrrolidone, (2) mixing the resulting solution of PVP in the organic solvent with water, (3) distilling off the organic solvent to give an aqueous solution of PVP, and (4) treating the aqueous solution of PVP with steam in the amount of from 20 to 200% of steam based on the weight of PVP; with (b) iodine in an amount of from 5 to 60% by weight, based on PVP; and with (c) a compound which provides iodide ions in an amount of from 10 to 200% by weight, calculated as iodide ions and based on the amount of iodine employed.
Claim 2
Dependent Claim
244 words
A process for the preparation of a stable aqueous solution of PVP-iodine which comprises: mixing in an aqueous medium (a) PVP as an aqueous solution of from 10 to 60% strength by weight, wherein said PVP has a K value of from 8 to 50 and has been prepared in the form of an aqueous solution by the steps of (1) polymerizing vinylpyrrolidone in an organic solvent which is an aromatic hydrocarbon or a lower aliphatic monohydric alcohol of 1 to 4 carbon atoms at a concentration of monomer of from 10 to 80% by weight and in the presence of a free radical initiator which is an organic per-compound selected from the group consisting of alkyl hydroperoxides and dialkyl peroxides of 1 to 8 carbon atoms per alkyl and per esters in an amount of about 0.1 to 5% by weight, based on vinylpyrrolidone, (2) mixing the resulting solution of PVP in the organic solvent with water, (3) distilling off the organic solvent to give an aqueous solution of PVP, and (4) treating the aqueous solution of PVP with steam in the amount of from 20 to 200% of steam based on the weight of PVP; with (b) iodine in an amount of from 5 to 60% by weight, based on PVP; and with (c) a compound which provides iodide ions in an amount of from 10 to 200% by weight, calculated as iodide ions and based on the amount of iodine employed.
Claim 3
Dependent Claim
27 words
The process of claim 1, wherein a PVP which has been produced by polymerization in the presence of a dialkyl peroxide as the organic initiator is used.
Claim 4
Dependent Claim
28 words
The process of claim 1, wherein the polymer solution obtained from the polymerization is employed directly, after dilution with water, for the preparation of the aqueous PVP-iodine solution.
Claim 5
Dependent Claim
20 words
The process of claim 1, wherein the polymer solution first obtained from the polymerization is subjected to a steam distillation.
Claim 6
Dependent Claim
20 words
The process of claim 1, wherein sodium iodide or potassium iodide is used as the compound which provides iodide ions.
Claim 7
Dependent Claim
28 words
The process of claim 1, wherein a solution of PVP and of the compound which provides iodide ions is first prepared, to which the iodine is then added.
Claim 8
Dependent Claim
32 words
The process of claim 1, wherein the free iodine is produced in the solution, from the compound which provides iodide ions and is present in excess, by reaction with an oxidizing agent.
Claim 9
Dependent Claim
14 words
The process of claim 7, wherein hydrogen peroxide is used as the oxidizing agent.
Claim 10
Dependent Claim
43 words
The process of claim 1, wherein the polymerization of vinylpyrrolidone takes place in the presence of from 0.01 to 10 ppm of a complex compound of a heavy metal of atomic number from 23 to 29 or its salt with an organic acid.
Claim 11
Dependent Claim
21 words
The process of claim 1, wherein the pH of the aqueous solution of PVP and iodine is from 2 to 7.
Claim 12
Dependent Claim
11 words
The process of claim 1, wherein the organic solvent is toluene.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1985-03-15 | 1985-09-14 | 1986-03-16 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1989-03-15 | 1989-09-14 | 1990-03-16 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1993-03-15 | 1993-09-14 | 1994-03-16 | $7700.00 | Window Closed / Lapsed |