Abstract

Abstract In a mold for shaping an apertured glass sheet comprising a shaping plate having a heat capacity more than that of the glass sheet per unit area and a shaping surface complementary to that desired for the glass sheet, areas having less heat capacity per unit area than that of the shaping plate are preferably obtained by cutting apertures in the shaping plate. These apertures or low heat capacity areas are located in the shaping plate in position to face corresponding apertures of the glass sheet to be shaped. When the shaping is performed by press bending the sheet between a pair of molds, preferably both press bending molds of press bending apparatus are apertured. The apertures or areas of low heat capacity in the molds are preferably slightly larger than the apertures in the glass sheet undergoing shaping to improve the stress pattern around the peripheral portion of the glass sheet apertures.

Inventors

  • 👤 Robert F. Pike

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-01 22:13
CPC Classifications
C; C03; C03B; C03B27/00; C03B27/04; C03B27/052; C03B23/00; C03B23/02; C03B23/023; C03B23/03; C03B23/031

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 112 words
In a method of bending and tempering a glass sheet having at least one aperture wherein the method includes the steps of heating the glass sheet to a temperature sufficient for subsequent bending and tempering; positioning the heated sheet on shaping surface of shaping means; bending the sheet by way of the shaping means; and cooling the bent sheet to impart at least a partial temper thereto, the improvement comprising the steps of: providing the shaping surface of the shaping means with an aperture consisting of a hole; and the positioning step includes the step of aligning the at least one aperture in the sheet and the aperture in the shaping surface.
Claim 2
Dependent Claim 112 words
In a method of bending and tempering a glass sheet having at least one aperture wherein the method includes the steps of heating the glass sheet to a temperature sufficient for subsequent bending and tempering; positioning the heated sheet on shaping surface of shaping means; bending the sheet by way of the shaping means; and cooling the bent sheet to impart at least a partial temper thereto, the improvement comprising the steps of: providing the shaping surface of the shaping means with an aperture consisting of a hole; and the positioning step includes the step of aligning the at least one aperture in the sheet and the aperture in the shaping surface.
Claim 3
Dependent Claim 48 words
The method as set forth in claim 1 wherein the shaping means includes opposed shaping molds having shaping surfaces of complementary shape for engaging opposite major surfaces of the glass sheet and one of the shaping surfaces is the shaping surface with the aperture consisting of a hole.
Claim 4
Dependent Claim 43 words
The method as set forth in claim 2 wherein the other shaping surface has an aperture consisting of a hole with the aperture in the shaping surfaces of the opposed shaping molds aligned with one another during the practice of the bending step.
Claim 5
Dependent Claim 39 words
The method as set forth in claim 2 or 3 further including the step of: interposing a layer of flexible, heat insulating, low heat capacity material between shaping molds and the glass sheet prior to practicing the bending step.

References Cited (Backward Citations)

US3279906A Cited
US3469963A Cited
US3367764A Cited
US3819351A Cited
US3960535A Cited
US4124367A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1985-03-15 1985-09-14 1986-03-16 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1989-03-15 1989-09-14 1990-03-16 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1993-03-15 1993-09-14 1994-03-16 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag