← Back to Patent Explorer
US4313981A Expired / Lapsed US ⏱️ 0.0 years remaining

Method of forming a roll protective layer

Assignee: Ricoh Co Ltd
•
Filing: 1980-08-25
•
Granted: 1982-02-02
•
Expires: 2000-08-25
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method is disclosed of protecting a rubber roller or roll which is supplied with oil during use, by coating its end faces. Unless the coating protects the end face in a satisfactory manner, the oil penetrates into the end face to degrade the rubber roller. In accordance with the invention, the end face is inwardly bevelled or tapered in the axial direction, and a protective layer for the end face is formed simultaneously as a protective layer for the peripheral surface of the roller.

Inventors

  • 👤 Ryoichi Namiki

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-27 13:05
CPC Classifications
G; G03; G03G; G03G15/00; G03G15/20; G03G15/2003; G03G15/2014; G03G15/2053

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 176 words
A method of forming a protective layer on an offset preventing roller for use in an electrophotographic copying machine, the roller being of the type having a cylindrical core metal, for protection of the surface of the roller from an offset preventing liquid, comprising the steps of providing, on the cylindrical core metal, a roll surface layer to be protected of a silicone rubber having a uniform diameter intermediate portion of a selected thickness and end portions at each end tapered in the axial direction of the roll from the intermediate portion to the core metal and terminating inwardly of the respective ends of the cylindrical core metal, rotating the cylindrical core roller and surface layer and spraying an oil-resistant fluorine-containing silicone rubber coating over the surface layer while rotating the cylindrical core roller to form a protective layer over the entire surface layer including said end portions and the cylindrical core metal beyond each end of said surface layer, and then applying room temperature vulcanized silicone rubber to the protective layer as an anti-offset layer.
Claim 2
Independent Claim 176 words
A method of forming a protective layer on an offset preventing roller for use in an electrophotographic copying machine, the roller being of the type having a cylindrical core metal, for protection of the surface of the roller from an offset preventing liquid, comprising the steps of providing, on the cylindrical core metal, a roll surface layer to be protected of a silicone rubber having a uniform diameter intermediate portion of a selected thickness and end portions at each end tapered in the axial direction of the roll from the intermediate portion to the core metal and terminating inwardly of the respective ends of the cylindrical core metal, rotating the cylindrical core roller and surface layer and spraying an oil-resistant fluorine-containing silicone rubber coating over the surface layer while rotating the cylindrical core roller to form a protective layer over the entire surface layer including said end portions and the cylindrical core metal beyond each end of said surface layer, and then applying room temperature vulcanized silicone rubber to the protective layer as an anti-offset layer.
Claim 3
Dependent Claim 38 words
A method according to claim 1, wherein the roll surface layer is formed with a bevelled portion and with a step portion of a thickness less than half the thickness of the intermediate portion of the surface layer.
Claim 4
Dependent Claim 48 words
A method according to claim 1, wherein each end of the surface layer is provided with a bevelled portion and a portion extending at substantially right angles to the surface of said core metal of a thickness which is less than half the thickness of said surface layer.
Claim 5
Independent Claim 195 words
A method of forming a protective layer on an offset preventing roller for use in an electrophotographic copying machine, the roller being of the type having a cylindrical core metal, for protection of the surface of the roller from an offset preventing liquid, comprising the steps of providing, on the cylindrical core metal, a roll surface layer to be protected of a silicone rubber, said silicone rubber having a uniform thickness and diameter intermediate portion of a selected thickness and end portions at each end, each of said end portions being tapered in the axial direction of the roll from the intermediate portion to the core metal and terminating inwardly of the respective end of the core metal in a boundary portion of constant thickness extending along the cylindrical core metal, rotating the cylindrical core roller, spraying an oil-resistant fluorine-containing silicone coating of silicone over the surface layer while rotating the cylindrical core roller to form a protective layer over the entire surface including the end portions and extending over the core metal beyond each end of said surface layer, and them applying room temperature vulcanized rubber to the protective layer as an anti-offset layer.
Claim 6
Independent Claim 195 words
A method of forming a protective layer on an offset preventing roller for use in an electrophotographic copying machine, the roller being of the type having a cylindrical core metal, for protection of the surface of the roller from an offset preventing liquid, comprising the steps of providing, on the cylindrical core metal, a roll surface layer to be protected of a silicone rubber, said silicone rubber having a uniform thickness and diameter intermediate portion of a selected thickness and end portions at each end, each of said end portions being tapered in the axial direction of the roll from the intermediate portion to the core metal and terminating inwardly of the respective end of the core metal in a boundary portion of constant thickness extending along the cylindrical core metal, rotating the cylindrical core roller, spraying an oil-resistant fluorine-containing silicone coating of silicone over the surface layer while rotating the cylindrical core roller to form a protective layer over the entire surface including the end portions and extending over the core metal beyond each end of said surface layer, and them applying room temperature vulcanized rubber to the protective layer as an anti-offset layer.

References Cited (Backward Citations)

CA636311A Cited
US710327A Cited
US1669942A Cited
US1576726A Cited
US1926312A Cited
US3435500A Cited
US3467009A Cited
US3686731A Cited
US3737963A Cited
US3971115A Cited
US3988817A Cited
US3941635A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1985-02-01 1985-08-03 1986-02-02 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1989-02-01 1989-08-03 1990-02-02 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1993-02-01 1993-08-03 1994-02-02 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag