Methods of imaging photopolymerizable materials containing diester polyether

Assignee: EIDP Inc
•
Filing: 1980-12-04
•
Granted: 1981-12-29
•
Expires: 2000-12-04
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A photopolymerizable element, preferably a lithographic plate, is provided. This element comprises a substrate bearing a photopolymerizable layer having a weight of about 1 to about 90 mg/dm 2 , said layer comprising: (1) at least one ethylenically unsaturated diester polyhydroxy polyether of the formula ##STR1## wherein R is H or CH 3 ; R 4 is H or an alkyl of 1-4 carbon atoms; n is 1-15; p is 0 or 1; and, when p is 1, R 5 is H or CH 3 , and R 6 is H, CH 3 or C 2 H 5 ; (2) an organic, radiation-sensitive, free-radical generating system comprising 2,4,5-triarylimidazolyl dimer and p-aminophenyl ketone; and (3) a macromolecular, organic, polymeric binder. A polymeric image is formed by imagewise exposing the layer to actinic radiation and then developing the resulting image such as by removing unexposed portions of the layer with a solvent.

Inventors

  • 👤 William J. Chambers
  • 👤 Christina N. Lazaridis

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 15:53
CPC Classifications
G; G03; G03F; G03F7/00; G03F7/004; G03F7/027; G03F7/028; G03F7/031

Claims Analysis

Total Claims: 7
Claim 1
Independent Claim 183 words
A method of producing a polymeric image comprising: (a) applying to a substrate a layer having a dry weight of 10-70 mg/dm 2 of a photopolymerizable composition comprising: (1) 10-79 percent by weight based on the total photopolymerizable layer of at least one ethylenically unsaturated diester polyhydroxy polyether of the formula ##STR6## wherein R is H or CH 3 ; R 4 is H or an alkyl of 1-4 carbon atoms; n is 1-15; p is 0 or 1; and when p is 1, R 5 is H or CH 3 , and R 6 is H, CH 3 or C 2 H 5 ; (2) 1-10 percent by weight, based on the total photopolymerizable layer, of an organic, radiation-sensitive, free-radical generating system comprising at least one 2,4,5-triarylimidazolyl dimer and at least one p-aminophenyl ketone; and (3) 20-80 percent by weight, based on the total photopolymerizable layer, of a macromolecular, organic, polymeric binder; (b) imagewise exposing a portion of the photopolymerizable layer to actinic radiation whereby the ethylenically unsaturated diester compound is polymerized in the radiation-struck areas; and (c) developing the resulting image.
Claim 2
Independent Claim 183 words
A method of producing a polymeric image comprising: (a) applying to a substrate a layer having a dry weight of 10-70 mg/dm 2 of a photopolymerizable composition comprising: (1) 10-79 percent by weight based on the total photopolymerizable layer of at least one ethylenically unsaturated diester polyhydroxy polyether of the formula ##STR6## wherein R is H or CH 3 ; R 4 is H or an alkyl of 1-4 carbon atoms; n is 1-15; p is 0 or 1; and when p is 1, R 5 is H or CH 3 , and R 6 is H, CH 3 or C 2 H 5 ; (2) 1-10 percent by weight, based on the total photopolymerizable layer, of an organic, radiation-sensitive, free-radical generating system comprising at least one 2,4,5-triarylimidazolyl dimer and at least one p-aminophenyl ketone; and (3) 20-80 percent by weight, based on the total photopolymerizable layer, of a macromolecular, organic, polymeric binder; (b) imagewise exposing a portion of the photopolymerizable layer to actinic radiation whereby the ethylenically unsaturated diester compound is polymerized in the radiation-struck areas; and (c) developing the resulting image.
Claim 3
Dependent Claim 21 words
The method of claim 1 wherein R 4 is hydrogen, p is 1, and R 5 and R 6 are methyl.
Claim 4
Dependent Claim 21 words
The method of claim 2 wherein n is 1-4 and the actinic radiation contains wavelengths in the range of 2000-8000 A.
Claim 5
Dependent Claim 34 words
The method of claim 3 wherein the photopolymerizable layer is exposed to the actinic radiation through an image-bearing transparency, and the image is developed by removing unexposed portions of the layer with a solvent.
Claim 6
Dependent Claim 21 words
The method of claim 3 wherein the molar ratio of 2,4,5-triarylimidazolyl dimer to p-aminophenyl ketone is in the range of 0.5-1.1.
Claim 7
Dependent Claim 45 words
The method of claim 5 wherein the photopolymerizable layer is exposed to the actinic radiation through an image-bearing transparency, the image is developed by removing unexposed portions of the layer with a solvent, and the actinic radiation contains wavelengths in the range of 2500-5000 A.

References Cited (Backward Citations)

GB1042520A Cited
US3549367A Cited
GB1312492A Cited
US3661576A Cited
DE2541133A1 Cited
US3984244A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1984-12-28 1985-06-29 1985-12-29 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1988-12-28 1989-06-29 1989-12-29 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1992-12-28 1993-06-29 1993-12-29 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag