Abstract
Abstract Impact resistant polymeric compositions are composed of a blend of a high nitrile resin and a hydrophobic nylon. The high nitrile resins useful in this invention are those produced by polymerizing a major proportion of a monounsaturated nitrile, e.g. acrylonitrile, and a minor proportion of another monovinyl monomer component, e.g. methyl acrylate, copolymerizable therewith optionally in the presence of a preformed rubber. The hydrophobic nylons useful in this invention comprise nylon-11, nylon-12 anc cyclic nylons.
Inventors
- 👤 Wayne T. Wiggins
- 👤 Gerald P. Coffey
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-27 22:04
CPC Classifications
C; C08; C08L; C08L25/00; C08L25/02; C08L25/04; C08L25/08; C08L25/12; C08L33/00; C08L33/18; C08L33/20; C08L51/00; C08L51/04; C08L77/00; C08L77/02
Claims Analysis
Total Claims: 15
Claim 1
Independent Claim
347 words
A polymer composition comprising a blend of (i) a polymer produced by polymerizing a major proportion of a monounsaturated nitrile, a minor proportion of another monovinyl monomer copolymerizable therewith optionally in the presence of a diene rubber, and (ii) a polyamide selected from the group consisting of nylon-11, nylon-12 and cyclic nylons wherein said cyclic nylon is prepared by reacting a dicarboxylic acid or acid chloride thereof with a diamine where at least one of said reactants is a cyclic compound, wherein (i) is a high nitrile copolymer prepared by the polymerization of 100 parts by weight of (a) from 60% to 90% by weight of at least one nitrile having the structure: ##STR15## wherein R is hydrogen, a lower alkyl group having from 1 to 4 carbon atoms, or a halogen, and (B) from 10% to 40% by weight based on the combined weights of (A) and (B) of at least one member selected from the group consisting of (1) an ester having the structure: ##STR16## wherein R is hydrogen, an alkyl group having from 1 to 30 carbon atoms, or a halogen, and R 2 is an alkyl group having from 1 to 6 carbon atoms, (2) an alpha-olefin having the structure: ##STR17## wherein R 3 and R 4 are alkyl groups having from 1 to 7 carbon atoms, (3) a vinyl ether selected from the group consisting of methyl vinyl ether, ethyl vinyl ether, the propyl vinyl ethers, and the butyl vinyl ethers, (4) vinyl acetate, (5) styrene, and (6) indene, in the presence of from 0 to 40 parts by weight of (C) a rubbery polymer of a conjugated diene monomer selected from the group consisting of butadiene and isoprene and a comonomer selected from the group consisting of styrene, a monomer having the structure: ##STR18## wherein R has the foregoing designation, and an ester having the structure: ##STR19## wherein R 1 and R 2 have the foregoing respective designations, said rubbery polymer containing from 50% to 100% by weight of polymerized conjugated diene and from 0% to 40% by weight of comonomer.
Claim 2
Dependent Claim
347 words
A polymer composition comprising a blend of (i) a polymer produced by polymerizing a major proportion of a monounsaturated nitrile, a minor proportion of another monovinyl monomer copolymerizable therewith optionally in the presence of a diene rubber, and (ii) a polyamide selected from the group consisting of nylon-11, nylon-12 and cyclic nylons wherein said cyclic nylon is prepared by reacting a dicarboxylic acid or acid chloride thereof with a diamine where at least one of said reactants is a cyclic compound, wherein (i) is a high nitrile copolymer prepared by the polymerization of 100 parts by weight of (a) from 60% to 90% by weight of at least one nitrile having the structure: ##STR15## wherein R is hydrogen, a lower alkyl group having from 1 to 4 carbon atoms, or a halogen, and (B) from 10% to 40% by weight based on the combined weights of (A) and (B) of at least one member selected from the group consisting of (1) an ester having the structure: ##STR16## wherein R is hydrogen, an alkyl group having from 1 to 30 carbon atoms, or a halogen, and R 2 is an alkyl group having from 1 to 6 carbon atoms, (2) an alpha-olefin having the structure: ##STR17## wherein R 3 and R 4 are alkyl groups having from 1 to 7 carbon atoms, (3) a vinyl ether selected from the group consisting of methyl vinyl ether, ethyl vinyl ether, the propyl vinyl ethers, and the butyl vinyl ethers, (4) vinyl acetate, (5) styrene, and (6) indene, in the presence of from 0 to 40 parts by weight of (C) a rubbery polymer of a conjugated diene monomer selected from the group consisting of butadiene and isoprene and a comonomer selected from the group consisting of styrene, a monomer having the structure: ##STR18## wherein R has the foregoing designation, and an ester having the structure: ##STR19## wherein R 1 and R 2 have the foregoing respective designations, said rubbery polymer containing from 50% to 100% by weight of polymerized conjugated diene and from 0% to 40% by weight of comonomer.
Claim 3
Dependent Claim
17 words
The blend of claim 1 wherein (i) contains between 70 and 80 parts by weight of (A).
Claim 4
Dependent Claim
9 words
The blend of claim 1 wherein (A) is acrylonitrile.
Claim 5
Dependent Claim
10 words
The blend of claim 1 wherein (B) is methyl acrylate.
Claim 6
Dependent Claim
17 words
The blend of claim 1 wherein (i) contains from 5 to 15 parts by weight of (C).
Claim 7
Dependent Claim
14 words
The blend of claim 1 wherein the blend contains a major proportion of (ii).
Claim 8
Dependent Claim
16 words
The blend of claim 5 wherein the blend contains 75% to 95% by weight of (ii).
Claim 9
Dependent Claim
9 words
The blend of claim 1 wherein (ii) is nylon-10.
Claim 10
Dependent Claim
9 words
The blend of claim 1 wherein (ii) is nylon-11.
Claim 11
Dependent Claim
11 words
The blend of claim 1 wherein (ii) is a cyclic nylon.
Claim 12
Dependent Claim
14 words
The blend of claim 1 wherein the blend contains a major proportion of (i).
Claim 13
Dependent Claim
14 words
The blend of claim 11 wherein the blend contains 75% to 95% of (i).
Claim 14
Dependent Claim
93 words
The blend of claim 10 wherein the cyclic nylon is prepared by the polycondensation of: (a) a diamine of the formula ##STR20## wherein Z is a bond or an alkylene chain of from one to six carbon atoms which may be optionally substituted by one or more methyl groups, and wherein each cyclohexane ring may optionally be substituted by one or more methyl groups; (b) a dicarboxylic acid or acid chloride of the formula ##STR21## wherein x is 1 to 16 and Y is selected from the group consisting of OH and Cl.
Claim 15
Dependent Claim
56 words
The blend of claim 10 wherein the cyclic nylon is prepared either by reacting a diamine with a dicarboxylic acid or acid chloride of the formula: ##STR22## wherein x and Y are defined above, or by reacting a dicarboxylic acid or acid chloride with a diamine of the formula: ##STR23## wherein x is 1 to 16.
References Cited (Backward Citations)
US3134746A
Cited
US3267175A
Cited
US4000216A
Cited
US4079024A
Cited
JPS50112954A
Cited
US4221879A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1984-12-21 | 1985-06-22 | 1985-12-22 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1988-12-21 | 1989-06-22 | 1989-12-22 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1992-12-21 | 1993-06-22 | 1993-12-22 | $7700.00 | Window Closed / Lapsed |