Abstract A water-saturated soft soil is efficiently improved in its strength by incorporating thereinto an additive composed of ingredients A, B and C; the ingredient A comprises gypsum, the ingredient B comprises a mixture of 40-55% by weight of a Portland cement and 60-45% by weight of a water-granulated iron blast furnace slag having a particle size almost equal to or smaller than that of the Portland cement and the ingredient C comprises a water-soluble ferrous salt. The ratio by weight of the ingredient A to the ingredient B ranges from 10/90 to 30/70 and the total amount of the ingredients A and B used for the soft soil is sufficient to strengthen the soft soil. The ingredient C is used in an amount sufficient to react with hydrogen sulfide contained in the soft soil to be treated.
A method for improving the strength of a water-saturated soft soil with unpleasant odor, which comprises admixing the soft soil with an ingredient A comprising gypsum, an ingredient B comprising a mixture of 40-55% by weight of a Portland cement and 60-45% by weight of a water-granulated iron blast furnace slag and a deodorizing ingredient C comprising a water-soluble ferrous salt, the slag having a particle size almost the same as or less than that of the cement, the ratio by weight of the ingredient A to the ingredient B being within the range from 10/90 to 30/70, and the order of adding the ingredients A, B and C being such that the soft soil is admixed with the ingredient A before or simultaneously with the ingredient B and that the ingredient C is added prior to addition of the ingredient B.
Claim 2
Independent Claim
142 words
A method for improving the strength of a water-saturated soft soil with unpleasant odor, which comprises admixing the soft soil with an ingredient A comprising gypsum, an ingredient B comprising a mixture of 40-55% by weight of a Portland cement and 60-45% by weight of a water-granulated iron blast furnace slag and a deodorizing ingredient C comprising a water-soluble ferrous salt, the slag having a particle size almost the same as or less than that of the cement, the ratio by weight of the ingredient A to the ingredient B being within the range from 10/90 to 30/70, and the order of adding the ingredients A, B and C being such that the soft soil is admixed with the ingredient A before or simultaneously with the ingredient B and that the ingredient C is added prior to addition of the ingredient B.
Claim 3
Dependent Claim
18 words
A method according to claim 1, wherein the ingredient C is an aqueous solution of the ferrous salt.
Claim 4
Dependent Claim
13 words
A method according to claim 2, wherein the ferrous salt is ferrous sulfate.
Claim 5
Dependent Claim
26 words
A method according to claim 1, wherein the total amount of the ingredients A and B is 50-150 kg per cubic meter of the soft soil.
Claim 6
Dependent Claim
14 words
A method according to claim 1, wherein the Portland cement is Ordinary Portland cement.