Cardboard laminate for foodstuffs and method for production thereof

Assignee: ELOTRADE AG A SWISS CORP
•
Filing: 1980-02-01
•
Granted: 1981-11-17
•
Expires: 2000-02-01
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A laminate for use in cartons for sterilized milk, fruit juices etc. consists of a cardboard web, a layer of heat-sealable thermoplastic material, preferably polyethylene, on the side of the laminate which is to form the outer sides of the cartons, and three layers of plastic material on the other side. Of these three layers, the middle layer consists of polyvinylidene chloride and the two others both consist of a plastic material of the same type as on the outer side. The innermost of these layers may be colored.

Inventors

  • 👤 Tom Frydendal

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-01 15:06
CPC Classifications
B; B32; B32B; B32B27/00; B32B27/06; B32B27/10; B32B27/08; B32B27/32; B32B2307/00; B32B2307/70; B32B2307/724; B32B2307/7242; B32B2307/7244; B32B2317/00; B32B2317/12; B32B2323/00; B32B2323/04; B32B2439/00; B32B2439/70; Y; Y10; Y10T; Y10T428/00; Y10T428/24; Y10T428/24942; Y10T428/31504; Y10T428/31855; Y10T428/3188; Y10T428/31895; Y10T428/31899; Y10T428/31902; Y10T428/31906; Y10T428/31909; Y10T428/31913; Y10T428/3192

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 104 words
A method of preparing a substantially oxygen-proof cardboard laminate adapted for cartons for foodstuffs, said method comprising the following steps: a. forming a suitably shaped cardboard layer of from 235 to 450 g/m 2 ; b. extruding a layer of polyethylene of at least 10 g/m 2 on each side of said cardboard layer; c. supplying as an emulsion a layer of polyvinylidene chloride of at least 2 g/m 2 over one of the layers of polyethylene; d. drying the layer of polyvinylidene chloride; and e. extruding a further layer of polyethylene of at least 10 g/m 2 on the layer of polyvinylidene chloride.
Claim 2
Independent Claim 104 words
A method of preparing a substantially oxygen-proof cardboard laminate adapted for cartons for foodstuffs, said method comprising the following steps: a. forming a suitably shaped cardboard layer of from 235 to 450 g/m 2 ; b. extruding a layer of polyethylene of at least 10 g/m 2 on each side of said cardboard layer; c. supplying as an emulsion a layer of polyvinylidene chloride of at least 2 g/m 2 over one of the layers of polyethylene; d. drying the layer of polyvinylidene chloride; and e. extruding a further layer of polyethylene of at least 10 g/m 2 on the layer of polyvinylidene chloride.
Claim 3
Dependent Claim 22 words
The method described in claim 1, wherein the layer of polyvinylidene chloride contains an adhesion enhancing additive consisting of a polycondensated aldehyde.
Claim 4
Independent Claim 132 words
A method of preparing a substantially oxygen-proof cardboard laminate adapted for cartons for foodstuffs, said method comprising the following steps: a. forming a suitably shaped cardboard layer having a weight characteristic on the order of 340 g/m 2 ; b. extruding a layer of polyethylene on the order of 14 g/m 2 on one side of said cardboard layer; c. extruding a layer of colored polyethylene on the order of 25 g/m 2 on the other side of said cardboard layer; d. supplying as an emulsion a layer of polyvinylidene chloride on the order of 6 g/m 2 on the layer of colored polyethylene; e. drying the layer of polyvinylidene chloride; and f. extruding a further layer of polyethylene on the order of 35 g/m 2 on the layer of polyvinylidene chloride.
Claim 5
Independent Claim 132 words
A method of preparing a substantially oxygen-proof cardboard laminate adapted for cartons for foodstuffs, said method comprising the following steps: a. forming a suitably shaped cardboard layer having a weight characteristic on the order of 340 g/m 2 ; b. extruding a layer of polyethylene on the order of 14 g/m 2 on one side of said cardboard layer; c. extruding a layer of colored polyethylene on the order of 25 g/m 2 on the other side of said cardboard layer; d. supplying as an emulsion a layer of polyvinylidene chloride on the order of 6 g/m 2 on the layer of colored polyethylene; e. drying the layer of polyvinylidene chloride; and f. extruding a further layer of polyethylene on the order of 35 g/m 2 on the layer of polyvinylidene chloride.

References Cited (Backward Citations)

US3162543A Cited
US4048428A Cited
US3560227A Cited
US3976528A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1984-11-16 1985-05-18 1985-11-17 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1988-11-16 1989-05-18 1989-11-17 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1992-11-16 1993-05-18 1993-11-17 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag