Patent US3240715A successfully refreshed from Google Patents.
Patent US4299638A successfully refreshed from Google Patents.
← Back to Patent Explorer
US4299638A Expired / Lapsed US ⏱️ 0.0 years remaining

Method of bonding silicon ceramic members

Assignee: NGK Insulators Ltd
•
Filing: 1980-02-19
•
Granted: 1981-11-10
•
Expires: 2000-02-19
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Silicon ceramic articles having a complicated shape and a high strength can be obtained in a high dimensional accuracy by fitting a silicon ceramic member having a lower firing shrinkage into another silicon ceramic member having a higher firing shrinkage, and firing the resulting assembly to bond firmly both the members into one integral body. The silicon ceramic article can be used as gas turbine parts, engine parts and the like.

Inventors

  • 👤 Tadaaki Matsuhisa

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-29 12:17
CPC Classifications
F; F01; F01D; F01D5/00; F01D5/30; F01D5/3084; C; C04; C04B; C04B35/00; C04B35/515; C04B35/58; C04B35/584; C04B35/622; C04B35/626; C04B35/63; C04B35/632; C04B35/634; C04B35/63404; C04B35/63416; C04B35/64; C04B35/645; C04B37/00; C04B37/008; C04B2235/00; C04B2235/02; C04B2235/50; C04B2235/52; C04B2235/5208; C04B2235/5216; C04B2235/524; C04B2235/5244; C04B2235/65; C04B2235/656; C04B2235/6567; C04B2235/658; C04B2235/70; C04B2235/72; C04B2235/728; C04B2237/00; C04B2237/30; C04B2237/32; C04B2237/36; C04B2237/365; C04B2237/368; C04B2237/50; C04B2237/56; C04B2237/568

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 92 words
A method of bonding at least two silicon ceramic members with each other, comprising fitting a first silicon ceramic member into a second silicon ceramic member through a layer of powder, paste or slurry of metallic silicon, silicon nitride or silicon carbide interposed between both the members at the interface to form an assembly, the first silicon ceramic member having a firing shrinkage lower than that of the second silicon ceramic member, and firing the assembly so as to bond firmly the first and second silicon ceramic members into one integral body.
Claim 2
Independent Claim 92 words
A method of bonding at least two silicon ceramic members with each other, comprising fitting a first silicon ceramic member into a second silicon ceramic member through a layer of powder, paste or slurry of metallic silicon, silicon nitride or silicon carbide interposed between both the members at the interface to form an assembly, the first silicon ceramic member having a firing shrinkage lower than that of the second silicon ceramic member, and firing the assembly so as to bond firmly the first and second silicon ceramic members into one integral body.

References Cited (Backward Citations)

US1164739A Cited
US3564328A Cited
US4156051A Cited
DE2707835A1 Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1984-11-09 1985-05-11 1985-11-10 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1988-11-09 1989-05-11 1989-11-10 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1992-11-09 1993-05-11 1993-11-10 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag