US4286604A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Smoking materials
Assignee: Gallaher Ltd
•
Filing: 1977-10-03
•
Granted: 1981-09-01
•
Expires: 1997-10-03
Abstract
Abstract The invention is concerned with a tobacco substitute which is made by subjecting a strand of viscose fibres to a controlled pyrolysis until the organic residue contains at least 90% carbon by weight, and loading the carbon strand with ingredients for smoking.
Inventors
- 👤 Jacques Ehretsmann
- 👤 Robert D. Cowling
- 👤 Alfred D. Schweizer
- 👤 William M. Caldwell
- 👤 Dennis F. Boyd
- 👤 Robert J. Boyd
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-28 19:40
CPC Classifications
A; A24; A24B; A24B15/00; A24B15/10; A24B15/16; A24B15/165
Claims Analysis
Total Claims: 38
Claim 1
Independent Claim
95 words
A method of making a smoking product by subjecting a mass of viscose fibres to a controlled pyrolysis until the organic residue contains at least 90% carbon by weight, and loading the resulting fibrous mass with the ingredients for smoking, wherein at least one additive selected from the group consisting of a catalyst for the pyrolysis, a carrier for a stimulant additive, and a combustion modifying agent or its precursor is added to a bulk viscose mix and said fibres are spun from said mix whereby the additives are homogeneously dispersed throughout the individual fibres.
Claim 2
Independent Claim
95 words
A method of making a smoking product by subjecting a mass of viscose fibres to a controlled pyrolysis until the organic residue contains at least 90% carbon by weight, and loading the resulting fibrous mass with the ingredients for smoking, wherein at least one additive selected from the group consisting of a catalyst for the pyrolysis, a carrier for a stimulant additive, and a combustion modifying agent or its precursor is added to a bulk viscose mix and said fibres are spun from said mix whereby the additives are homogeneously dispersed throughout the individual fibres.
Claim 3
Independent Claim
81 words
A method of making a tobacco substitute smoking product fuel, said method comprising providing a mass of substantially round cross-section, crimped viscose fibers having a denier of between 5 and 20, and a length of between 20 and 100 mm, and subjecting the mass of viscose fibers to controlled pyrolysis until the organic residue contains at least 95% carbon by weight, an oxygen content of between 1 and 4% by weight, and a hydrogen content of less than 1% by weight.
Claim 4
Independent Claim
81 words
A method of making a tobacco substitute smoking product fuel, said method comprising providing a mass of substantially round cross-section, crimped viscose fibers having a denier of between 5 and 20, and a length of between 20 and 100 mm, and subjecting the mass of viscose fibers to controlled pyrolysis until the organic residue contains at least 95% carbon by weight, an oxygen content of between 1 and 4% by weight, and a hydrogen content of less than 1% by weight.
Claim 5
Dependent Claim
16 words
Method according to claim 2, wherein the fibers have between 6 and 8 crimps per cm.
Claim 6
Dependent Claim
19 words
Method according to claim 2, wherein the viscose fibers are in the form of a silver of staple fibers.
Claim 7
Dependent Claim
24 words
Method according to claim 4, wherein said sliver has, after the pyrolysis, a linear density of organic residue of between 1.5 and 7 g/m.
Claim 8
Dependent Claim
9 words
The product produced by the method of claim 5.
Claim 9
Dependent Claim
9 words
The product produced by the method of claim 2.
Claim 10
Dependent Claim
25 words
A wrapped continuous form tobacco substitute rod comprising a tobacco substitute smoking product fuel of claim 7 in continuous strand form and a wrap therefor.
Claim 11
Independent Claim
110 words
A method of making a tobacco substitute smoking product fuel, said method comprising providing a mass of viscose fibers and subjecting said viscose fibers to controlled pyrolysis until the organic residue contains at least 90% carbon by weight by the stepwise heating of said mass by first raising the temperature of said mass gradually from between 200° C. and 300° C. to between 400° C. and 550° C. to dry said mass and provide the major chemical transformation reactions of the viscose, and thereafter quickly raising the temperature of said mass to between 700° C. and 1200° C. for long enough to complete the transformation of the viscose to carbon.
Claim 12
Independent Claim
110 words
A method of making a tobacco substitute smoking product fuel, said method comprising providing a mass of viscose fibers and subjecting said viscose fibers to controlled pyrolysis until the organic residue contains at least 90% carbon by weight by the stepwise heating of said mass by first raising the temperature of said mass gradually from between 200° C. and 300° C. to between 400° C. and 550° C. to dry said mass and provide the major chemical transformation reactions of the viscose, and thereafter quickly raising the temperature of said mass to between 700° C. and 1200° C. for long enough to complete the transformation of the viscose to carbon.
Claim 13
Dependent Claim
23 words
Method of claim 9, wherein said mass is passed in strand form longitudinally, either continuously or in stepwise manner, through a pyrolysing oven.
Claim 14
Dependent Claim
29 words
Method according to claim 9, wherein the pyrolysis step is carried out in an oven in the presence of a non-reactive atmosphere which comprises nitrogen, steam, or mixture thereof.
Claim 15
Dependent Claim
9 words
The product produced by the method of claim 9.
Claim 16
Dependent Claim
25 words
A wrapped continuous form tobacco substitute rod comprising a tobacco substitute smoking product fuel of claim 12 in continuous strand form and a wrap therefor.
Claim 17
Independent Claim
69 words
A method of making a tobacco substitute smoking product fuel, said method comprising providing a mass of viscose fibers and subjecting said mass of viscose fibers to controlled pyrolysis in an oven in the presence of a non-reactive atmosphere which comprises nitrogen, steam, or a mixture thereof, and which also includes some recycled gaseous products of the pyrolysis, until the organic residue contains at least 90% carbon by weight.
Claim 18
Independent Claim
69 words
A method of making a tobacco substitute smoking product fuel, said method comprising providing a mass of viscose fibers and subjecting said mass of viscose fibers to controlled pyrolysis in an oven in the presence of a non-reactive atmosphere which comprises nitrogen, steam, or a mixture thereof, and which also includes some recycled gaseous products of the pyrolysis, until the organic residue contains at least 90% carbon by weight.
Claim 19
Independent Claim
66 words
A method of making a smoking product for use as a tobacco substitute, said method comprising providing a mass of viscose fibers having a nicotine component carrier homogeneously dispersed therein, thereafter subjecting the mass of viscose fibers to controlled pyrolysis until the organic residue contains at least 90% carbon by weight, and thereafter loading the pyrolysed product with the ingredients for smoking including a nicotine component.
Claim 20
Independent Claim
66 words
A method of making a smoking product for use as a tobacco substitute, said method comprising providing a mass of viscose fibers having a nicotine component carrier homogeneously dispersed therein, thereafter subjecting the mass of viscose fibers to controlled pyrolysis until the organic residue contains at least 90% carbon by weight, and thereafter loading the pyrolysed product with the ingredients for smoking including a nicotine component.
Claim 21
Dependent Claim
20 words
Method according to claim 15, wherein said carrier for said nicotine component comprises an alumino silicate, aluminum oxide or silica.
Claim 22
Independent Claim
67 words
A method of making a tobacco substitute smoking product fuel, said method comprising providing a bulk viscose mix, dispersing a carrier for a nicotine component within the bulk viscose mix, spinning the bulk viscose mix to produce viscose fibers having said nicotine component carrier dispersed therein, and subjecting a mass of viscose fibers to controlled pyrolysis until the organic residue contains at least 90% carbon by weight.
Claim 23
Independent Claim
67 words
A method of making a tobacco substitute smoking product fuel, said method comprising providing a bulk viscose mix, dispersing a carrier for a nicotine component within the bulk viscose mix, spinning the bulk viscose mix to produce viscose fibers having said nicotine component carrier dispersed therein, and subjecting a mass of viscose fibers to controlled pyrolysis until the organic residue contains at least 90% carbon by weight.
Claim 24
Independent Claim
64 words
A method for making a smoking tobacco substitute product fuel, said method comprising providing a mass of viscose fibers having homogeneously dispersed therein at least one inorganic combustion modifying agent, and thereafter subjecting the viscose fibers to controlled pyrolysis until the organic residue contains at least 90% carbon by weight to produce a pyrolysed product with said inorganic combustion modifying agent homogeneously dispersed therein.
Claim 25
Independent Claim
64 words
A method for making a smoking tobacco substitute product fuel, said method comprising providing a mass of viscose fibers having homogeneously dispersed therein at least one inorganic combustion modifying agent, and thereafter subjecting the viscose fibers to controlled pyrolysis until the organic residue contains at least 90% carbon by weight to produce a pyrolysed product with said inorganic combustion modifying agent homogeneously dispersed therein.
Claim 26
Independent Claim
79 words
A method for making a smoking tobacco substitute product fuel, said method comprising providing a mass of viscose fibers having homogeneously dispersed therein at least one inorganic combustion modifying agent precursor, and subjecting the viscose fibers to controlled pyrolysis until the organic residue contains at least 90% carbon by weight and said inorganic combustion modifying agent precursor is converted into an inorganic combustion modifying agent, to produce a pyrolysed product with said inorganic combustion modifying agent homogeneously dispersed therein.
Claim 27
Independent Claim
79 words
A method for making a smoking tobacco substitute product fuel, said method comprising providing a mass of viscose fibers having homogeneously dispersed therein at least one inorganic combustion modifying agent precursor, and subjecting the viscose fibers to controlled pyrolysis until the organic residue contains at least 90% carbon by weight and said inorganic combustion modifying agent precursor is converted into an inorganic combustion modifying agent, to produce a pyrolysed product with said inorganic combustion modifying agent homogeneously dispersed therein.
Claim 28
Dependent Claim
13 words
Method of claim 19, wherein said inorganic combustion modifying agent is calcium carbonate.
Claim 29
Dependent Claim
63 words
Method of claim 20, including the additional step of dispersing in said pyrolysed mass, a further combustion modifying agent which is at least one of ammonium dihydrogen phosphate; diammonium hydrogen phosphate; the mono-, di- and tri-phosphates of sodium and potassium; and the meta- and tetra-borates of sodium and potassium, by contacting said pyrolysed product with a solution of said further combustion modifying agent.
Claim 30
Dependent Claim
10 words
Method of claim 19, wherein said precursor is calcium formate.
Claim 31
Dependent Claim
10 words
Method of claim 19, wherein said precursor is calcium nitrate.
Claim 32
Dependent Claim
22 words
Method of claim 19, wherein said precursor is applied to said viscose fibers in the form of a solution of said precursor.
Claim 33
Independent Claim
138 words
A method for making a smoking tobacco substitute product fuel, said method comprising providing a mass of viscose fibers, applying calcium formate to said viscose fibers in the form of a calcium formate solution, to homogeneously disperse said calcium formate into said mass, thereafter subjecting said mass to controlled pyrolysis until the organic residue contains at least 90% carbon by weight, and said calcium formate is converted to calcium carbonate, to produce a pyrolysed product with said calcium carbonate homogeneously dispersed therein, and thereafter dispersing in the pyrolysed product a further combustion modifying agent which is at least one of ammonium dihydrogen phosphate, diammonium hydrogen phosphate, the mono-, di- and tri-phosphates of sodium and potassium, and the meta- and tetra-borates of sodium and potassium, by contacting said pyrolysed product with a solution of said further combustion modifying agent.
Claim 34
Independent Claim
138 words
A method for making a smoking tobacco substitute product fuel, said method comprising providing a mass of viscose fibers, applying calcium formate to said viscose fibers in the form of a calcium formate solution, to homogeneously disperse said calcium formate into said mass, thereafter subjecting said mass to controlled pyrolysis until the organic residue contains at least 90% carbon by weight, and said calcium formate is converted to calcium carbonate, to produce a pyrolysed product with said calcium carbonate homogeneously dispersed therein, and thereafter dispersing in the pyrolysed product a further combustion modifying agent which is at least one of ammonium dihydrogen phosphate, diammonium hydrogen phosphate, the mono-, di- and tri-phosphates of sodium and potassium, and the meta- and tetra-borates of sodium and potassium, by contacting said pyrolysed product with a solution of said further combustion modifying agent.
Claim 35
Dependent Claim
63 words
Method of claim 25, wherein said calcium formate and said further combustion modifying agent are dispsered on said fibers in said mass by dipping said mass in a solution of said calcium formate, and subsequently deliquoring and drying said fibers, and by dipping said pyrolysed mass in a solution of said further combustion modifying agent, and subsequently deliquoring and drying said pyrolysed mass.
Claim 36
Dependent Claim
41 words
A tobacco substitute smoking product fuel, said fuel comprising pyrolysed viscose fibers having a carbon content of at least 90% carbon by weight of the organic pyrolysis residue, and having calcium carbonate homogeneously dispersed therein as an inorganic combustion modifying agent.
Claim 37
Dependent Claim
41 words
A tobacco substitute smoking product fuel, said fuel comprising pyrolysed viscose fibers having a carbon content of at least 90% carbon by weight of the organic pyrolysis residue, and having calcium carbonate homogeneously dispersed therein as an inorganic combustion modifying agent.
Claim 38
Dependent Claim
46 words
The fuel according to claim 27, wherein said fuel additionally contains a further combustion modifying agent which is at least one of ammonium dihydrogen phosphate; diammonium hydrogen phosphate; and mono-, di- and tri-phosphates of sodium and potassium; and the meta- and tetra-borates of sodium and potassium.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1984-08-31 | 1985-03-02 | 1985-09-01 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1988-08-31 | 1989-03-02 | 1989-09-01 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1992-08-31 | 1993-03-02 | 1993-09-01 | $7700.00 | Window Closed / Lapsed |