Abstract

Abstract Ferric ions may be removed very selectively from aqueous solutions by means of a metal-chelating resin consisting of the acid-quaternized form of a cross-linked polymer produced by the condensation of a phenolic component comprising one or more phenols, formaldehyde, and a diamino component comprising one or more di-(secondary amino) compounds under neutral conditions. The resin is prepared by treating the cross-linked polymer with an aqueous solution of a strong mineral acid.

Inventors

  • 👤 Jonathan H. Hodgkin

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-28 22:54
CPC Classifications
C; C08; C08G; C08G14/00; C08G14/02; C08G14/04; C08G14/12; B; B01; B01J; B01J45/00; C08G14/06; C22; C22B; C22B3/00; C22B3/20; C22B3/42; Y; Y02; Y02P; Y02P10/00; Y02P10/20; Y10; Y10S; Y10S210/00; Y10S210/902; Y10S210/911; Y10S210/912

Claims Analysis

Total Claims: 16
Claim 1
Independent Claim 46 words
A metal-chelating resin, selective for ferric ions and consisting of the acid-quaternized form of cross-linked polymer produced by the condensation of a phenolic component comprising one or more phenols, formaldehyde, and a diamino component consisting essentially of one or more di(secondary amino) compounds under neutral conditions.
Claim 2
Dependent Claim 46 words
A metal-chelating resin, selective for ferric ions and consisting of the acid-quaternized form of cross-linked polymer produced by the condensation of a phenolic component comprising one or more phenols, formaldehyde, and a diamino component consisting essentially of one or more di(secondary amino) compounds under neutral conditions.
Claim 3
Dependent Claim 13 words
A resin as claimed in claim 1, quaternized with a strong mineral acid.
Claim 4
Dependent Claim 13 words
A resin as claimed in claim 2, wherein the acid is sulphuric acid.
Claim 5
Dependent Claim 31 words
A resin as claimed in claim 1, wherein the diamino component comprises one or more di-(secondary amino) compounds in which each secondary amino group forms part of a saturated heterocyclic ring.
Claim 6
Dependent Claim 14 words
A resin as claimed in claim 4, wherein amino component is piperazine or 4,4'-bipiperidine.
Claim 7
Dependent Claim 41 words
A resin as claimed in claim 1, wherein the phenolic component comprises one or more compounds selected from the group consisting of hydroxybenzene and hydroxybenzenes having C 1 to C 3 alkyl substituents in the 3 and/or 3 and 5 positions.
Claim 8
Dependent Claim 21 words
A resin as claimed in claim 6, wherein the phenolic component is selected from the group consisting of hydroxybenzene and 3-ethyl-1-hydroxybenzene.
Claim 9
Dependent Claim 23 words
A resin as claimed in claim 1, wherein the phenolic component includes a bisphenol, bisphenol sulphide or bisphenol sulphoxide as a crosslinking agent.
Claim 10
Dependent Claim 47 words
A resin as claimed in claim 1, wherein the diamino component is piperazine and the polymer has the structure ##STR2## where R' and R'" are independently lower (C 1 -C 3 ) alkyl groups or hydrogen atoms and R" is a hydrogen atom or a crosslinking group.
Claim 11
Independent Claim 67 words
A method for preparing an iron-selective metal-chelating resin which comprises treating a cross-linked polymer, with an aqueous solution of a strong mineral acid, said polymer having been prepared by condensing approximately equimolar quantities of a phenolic component comprising one or more phenols, and a diamino component consisting essentially of one or more di-(secondary amino) compounds with approximately twice the molar quantity of formaldehyde under Mannich reaction conditions.
Claim 12
Independent Claim 67 words
A method for preparing an iron-selective metal-chelating resin which comprises treating a cross-linked polymer, with an aqueous solution of a strong mineral acid, said polymer having been prepared by condensing approximately equimolar quantities of a phenolic component comprising one or more phenols, and a diamino component consisting essentially of one or more di-(secondary amino) compounds with approximately twice the molar quantity of formaldehyde under Mannich reaction conditions.
Claim 13
Dependent Claim 19 words
A method as claimed in claim 10, wherein the aqueous acid is sulphuric acid of about 2 N concentration.
Claim 14
Dependent Claim 26 words
A method for the selective removal of ferric ions from an aqueous solution which comprises contacting the solution with a resin as claimed in claim 1.
Claim 15
Dependent Claim 22 words
A method as claimed in claim 12, wherein the iron-loaded resin is subsequently treated with a complexing agent to remove the iron.
Claim 16
Dependent Claim 14 words
A method as claimed in claim 13, wherein the complexing agent is hydrochloric acid.

References Cited (Backward Citations)

US2036916A Cited
US2033092A Cited
US2316714A Cited
US2636019A Cited
US2807594A Cited
US2890095A Cited
US2997460A Cited
US3606988A Cited
US3878136A Cited
US3975268A Cited
US4190709A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1984-08-17 1985-02-16 1985-08-18 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1988-08-17 1989-02-16 1989-08-18 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1992-08-17 1993-02-16 1993-08-18 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag