Abstract
Abstract Non-woven fabrics are prepared from synthetic fibers by impregnating the fibers with a liquid binder system containing a polymer of from 35 to 60 weight percent of a hard monomer, 0 to 45 weight percent of butadiene or isoprene, 10 to 50 weight percent of an acrylate having from 1 to 8 carbon atoms in the ester portion and 1 to 5 weight percent of an ethylenically unsaturated mono- or dicarboxylic acid.
Inventors
- 👤 James E. Schwartz
- 👤 Kent B. McReynolds
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-28 15:22
CPC Classifications
D; D04; D04H; D04H1/00; D04H1/40; D04H1/58; D04H1/64; D04H1/587; Y; Y10; Y10T; Y10T442/00; Y10T442/20; Y10T442/2861; Y10T442/2885
Claims Analysis
Total Claims: 6
Claim 1
Independent Claim
117 words
A method for making non-woven fabrics having a soft, cloth-like feel from synthetic fibers in which a polymer in the form of an aqueous dispersion is incorporated into a web of synthetic fibers, water is removed and the retained polymeric binder is cured which comprises impregnating the synthetic fibers with an aqueous binder system containing a polymer, the solids of which consist essentially of from 35 to 60 weight percent of a hard monomer, 0 to 45 weight percent of butadiene or isoprene, 10 to 50 weight percent of an acrylate ester having from 1 to 8 carbon atoms in the ester portion and 1 to 5 weight percent of an ethylenically unsaturated mono- or dicarboxylic acid.
Claim 2
Independent Claim
117 words
A method for making non-woven fabrics having a soft, cloth-like feel from synthetic fibers in which a polymer in the form of an aqueous dispersion is incorporated into a web of synthetic fibers, water is removed and the retained polymeric binder is cured which comprises impregnating the synthetic fibers with an aqueous binder system containing a polymer, the solids of which consist essentially of from 35 to 60 weight percent of a hard monomer, 0 to 45 weight percent of butadiene or isoprene, 10 to 50 weight percent of an acrylate ester having from 1 to 8 carbon atoms in the ester portion and 1 to 5 weight percent of an ethylenically unsaturated mono- or dicarboxylic acid.
Claim 3
Dependent Claim
10 words
Method of claim 1 wherein the hard monomer is styrene.
Claim 4
Dependent Claim
40 words
Method of claim 2 wherein the binder comprises from about 40 to 45 weight percent styrene, about 20 to 40 weight percent butadiene, about 15 to 35 weight percent butyl acrylate and about 2 to 4 weight percent itaconic acid.
Claim 5
Dependent Claim
11 words
Method of claim 3 wherein the synthetic fiber is a polyester.
Claim 6
Dependent Claim
10 words
Method of claim 3 wherein the synthetic fiber is polypropylene.
References Cited (Backward Citations)
US2976167A
Cited
US3256234A
Cited
US3142654A
Cited
US3202638A
Cited
US3397165A
Cited
US3720562A
Cited
US3784401A
Cited
US3920868A
Cited
US3944690A
Cited
US4176108A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1984-05-18 | 1984-11-17 | 1985-05-19 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1988-05-18 | 1988-11-17 | 1989-05-19 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1992-05-18 | 1992-11-17 | 1993-05-19 | $7700.00 | Window Closed / Lapsed |