Polyols derived from 4,4,4-trichloro-1,2-epoxybutane and/or epihalohydrin for use in the production of heat sealable foams
Abstract
Abstract The instant invention is directed to a polyol having a molecular weight of 2,000 to 8,000 which is especially suited for use in the production of heat sealable foams, comprising the adduct obtained by sequentially reacting: (a) a polyhydroxyl initiator, with a functionality of 2 to 5 and a weight average molecular weight as determined by gel permeation chromatography of from 62 to 200; with (b) 10 to 90%, by weight, based on the total oxide present in (b)+(c)+(d), a first alkylene oxide; and subsequently reacting the product with (c) 10 to 80%, by weight, based on the total oxide present in (b)+(c)+(d), 4,4,4-trichloro-1,2-epoxybutane and/or epihalohydrin; and subsequently reacting the product with (d) 10 to 60%, by weight, based on the total oxide present in (b)+(c)+(d), a second alkylene oxide.
Inventors
- 👤 Barry A. Phillips
- 👤 Keith G. Spitler
- 👤 Richard E. Keegan
Bibliographic Details
Claims Analysis
Total Claims: 9References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1983-11-18 | 1984-05-19 | 1984-11-18 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1987-11-18 | 1988-05-19 | 1988-11-18 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1991-11-18 | 1992-05-19 | 1992-11-18 | $7700.00 | Window Closed / Lapsed |