Patent US4233275A successfully refreshed from Google Patents.
← Back to Patent Explorer
US4233275A Expired / Lapsed US ⏱️ 0.0 years remaining

Process and apparatus for purifying raw coal gas

Assignee: Hitachi Ltd
•
Filing: 1978-12-01
•
Granted: 1980-11-11
•
Expires: 1998-12-01
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A high temperature, high pressure raw coal gas containing hydrogen sulfide, ammonia, and tarry matter, is purified by contacting the raw coal gas with solid particles thereby cooling the raw coal gas to a temperature suitable for hydrogen sulfide removal and at the same time depositing the tarry matter onto the solid particles by condensation to recover the tarry matter from the raw coal gas, removing the hydrogen sulfide from the cooled and substantially tar-free coal gas, expanding the raw coal gas to a pressure suitable for ammonia decomposition, heating the expanded raw coal gas to a temperature suitable for ammonia decomposition by heat obtained by combusting the recovered tarry matter on the solid particles, thereby regenerating the solid particles for reuse, and then decomposing ammonia in the raw coal gas, thereby removing ammonia therefrom. A process for efficiently purifying raw coal gas by removing tarry matter, hydrogen sulfide and ammonia, including effectively utilizing the recovered tarry matter to produce heat while also effectively utilizing the energy obtained by expanding the coal gas through a pressure-reducing means such as an expansion turbine.

Inventors

  • 👤 Shoichi Kimura
  • 👤 Toshihiko Takahashi
  • 👤 Zensuke Tamura

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-31 20:44
CPC Classifications
C; C10; C10K; C10K1/00; C10K1/34; C10K1/04; C10K1/20

Claims Analysis

Total Claims: 17
Claim 1
Independent Claim 214 words
A process for purifying a high pressure raw coal gas having a temperature in the range of 800° C. or greater and containing tarry matter, hydrogen sulfide and ammonia, which comprises: contacting the raw coal gas with solid particles having a lower temperature than the raw coal gas, thereby cooling the raw coal gas to a temperature in the range of 550°-800° C., and thereby simultaneously removing tarry matter from the raw coal gas by condensing and depositing the tarry matter on the solid particles; thereafter contacting the raw coal gas having a temperature within the range of 550°-800° C., from which the tarry matter has been removed, with solid particles that will absorb hydrogen sulfide to thereby remove the hydrogen sulfide from the raw coal gas; burning the removed tarry matter to produce heat of combustion; thereafter heating the raw coal gas, from which the tarry matter and hydrogen sulfide have been removed, to a temperature in the range of 700°-900° C. with the heat of combustion produced by the burning of the removed tarry matter; and thereafter contacting the raw coal gas at a temperature within the range of 700°-900° C. from which the tarry matter and hydrogen sulfide have been removed, with an ammonia decomposition catalyst to decompose and remove ammonia.
Claim 2
Dependent Claim 214 words
A process for purifying a high pressure raw coal gas having a temperature in the range of 800° C. or greater and containing tarry matter, hydrogen sulfide and ammonia, which comprises: contacting the raw coal gas with solid particles having a lower temperature than the raw coal gas, thereby cooling the raw coal gas to a temperature in the range of 550°-800° C., and thereby simultaneously removing tarry matter from the raw coal gas by condensing and depositing the tarry matter on the solid particles; thereafter contacting the raw coal gas having a temperature within the range of 550°-800° C., from which the tarry matter has been removed, with solid particles that will absorb hydrogen sulfide to thereby remove the hydrogen sulfide from the raw coal gas; burning the removed tarry matter to produce heat of combustion; thereafter heating the raw coal gas, from which the tarry matter and hydrogen sulfide have been removed, to a temperature in the range of 700°-900° C. with the heat of combustion produced by the burning of the removed tarry matter; and thereafter contacting the raw coal gas at a temperature within the range of 700°-900° C. from which the tarry matter and hydrogen sulfide have been removed, with an ammonia decomposition catalyst to decompose and remove ammonia.
Claim 3
Dependent Claim 63 words
A process according to claim 1, wherein the solid particles with the tarry matter deposited thereon, after being used for cooling the raw coal gas to the temperature suitable for the reaction of removal of hydrogen sulfide, are contacted with hot air to burn the tarry matter and regenerate the solid particles for reuse in recovering tarry matter from the raw coal gas.
Claim 4
Dependent Claim 111 words
A process according to claim 1, wherein the raw coal gas is contacted with solid particles cooled by air to a temperature lower than that of the raw coal gas, thereby cooling the raw coal gas to a temperature in the range of 550°-800° C. while simultaneously recovering tarry matter contained in the raw coal gas on the solid particles by condensation and deposition, the solid particles with the tarry matter deposited thereon are regenerated by burning the tarry matter on the solid particles, and the regenerated particles are cooled through contact with air, and reused in cooling the raw coal gas and recovering tarry matter from the raw coal gas.
Claim 5
Dependent Claim 104 words
A process according to claim 1, wherein the raw coal gas is cooled to a temperature within the range of 550°-800° C. by contact with a cooling pipe in the presence of the solid particles, thereby simultaneously recovering tarry matter on the solid particles by condensation and deposition, the raw coal gas freed from hydrogen sulfide is heated to a temperature in the range of 700°-900° C. by the heat of combustion produced by burning the tarry matter deposited on the solid particles, thereby regenerating the solid particles, and the regenerated solid particles are reused in recovering tarry matter from the raw coal gas.
Claim 6
Dependent Claim 66 words
A process according to claim 1, wherein the raw coal gas is further cooled by contact with a cooling pipe in the presence of the solid particles, thereby substantially removing tarry matter in the raw coal gas by condensing and depositing the tarry matter on the solid particles, and the cooled raw coal gas is thereafter heated to a temperature in the range of 550°-800° C.
Claim 7
Dependent Claim 39 words
A process according to claim 5, wherein the cooled raw coal gas is heated to a temperature within the range of 550°-800° C. by the heat of combustion produced by burning the tarry matter deposited on the solid particles.
Claim 8
Dependent Claim 41 words
A process according to claim 5, wherein the solid particles with the tarry matter deposited thereon by condensation are contacted with hot air and burned, thereby regenerating the solid particles for reuse in recovering tarry matter from the raw coal gas.
Claim 9
Dependent Claim 37 words
A process according to claim 1, wherein the pressure of the raw coal gas freed from hydrogen sulfide is reduced, and then the raw coal gas is heated to a temperature within the range of 700°-900° C.
Claim 10
Dependent Claim 22 words
A process according to claim 8, wherein the pressure of the raw coal gas freed from hydrogen sulfide is reduced by expansion.
Claim 11
Dependent Claim 22 words
A process according to claim 9, wherein the energy produced by the expansion of the raw coal gas is converted to power.
Claim 12
Dependent Claim 53 words
A process according to claim 8, wherein the raw coal gas freed from hydrogen sulfide and after the pressure reduction and the heating, is admixed with air, and a portion of combustible gases therein is combusted by oxidation thereby heating the raw coal gas to a temperature within the range of 700°-900° C.
Claim 13
Dependent Claim 55 words
A process according to claim 1, wherein the hydrogen sulfide removal reaction is carried out by contacting the raw coal gas with solid absorber particles of or containing iron oxide and the ammonia decomposition reaction is carried out by contacting the raw coal gas with a catalyst containing iron in a state of reduced iron.
Claim 14
Dependent Claim 22 words
A process according to claim 1, wherein the solid particles are alumina particles or a mixture of alumina particles and silica particles.
Claim 15
Dependent Claim 47 words
A process according to claim 12, wherein the hydrogen sulfide removal reaction is carried out at a temperature of 550° to 800° C., and the ammonia decomposition reaction at a temperature of 700° to 900° C. under a pressure of not more than 15 kg/cm 2 .
Claim 16
Dependent Claim 23 words
A process according to claim 14, wherein the hydrogen sulfide removal reaction is carried out at a temperature of 600° to 750° C.
Claim 17
Dependent Claim 21 words
A process according to claim 15, wherein the hydrogen sulfide removal reaction is carried out at a temperature of 650° C.

References Cited (Backward Citations)

US2837398A Cited
US3822337A Cited
US3812236A Cited
US4089809A Cited
US4155990A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1983-11-11 1984-05-12 1984-11-11 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1987-11-11 1988-05-12 1988-11-11 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1991-11-11 1992-05-12 1992-11-11 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag