Method for forming color images

Assignee: Fujifilm Holdings Corp
•
Filing: 1979-04-13
•
Granted: 1980-10-21
•
Expires: 1999-04-13
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method for forming color images comprising processing a photographic element containing imagewise distributed silver in the presence of a polymer containing at least 30 mol % vinyl pyridines, a dye and an oxidizing agent to thereby oxidation-bleach the dye. Color images having excellent light fastness, heat resistance and humidity resistance are obtained.

Inventors

  • 👤 Shigeru Nakamura
  • 👤 Isao Shimamura
  • 👤 Taku Nakamura
  • 👤 Shinji Sakaguchi
  • 👤 Takushi Miyazako
  • 👤 Masatoshi Sugiysma
  • 👤 Akio Mitsui

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-06 12:49
CPC Classifications
G; G03; G03C; G03C7/00; G03C7/28; Y; Y10; Y10S; Y10S430/00; Y10S430/144

Claims Analysis

Total Claims: 17
Claim 1
Independent Claim 71 words
A method for forming color images which comprises exposing a color photographic light-sensitive element containing a dye, a polymer containing at least 30 mol% of a vinylpyridine represented by the formula: ##STR11## wherein R is a hydrogen atom or an alkyl group and silver halide, forming developed silver imagewise by development processing and then processing with an aqueous solution containing peroxoic acids or salt thereof to thereby oxidatively bleach said dye.
Claim 2
Independent Claim 71 words
A method for forming color images which comprises exposing a color photographic light-sensitive element containing a dye, a polymer containing at least 30 mol% of a vinylpyridine represented by the formula: ##STR11## wherein R is a hydrogen atom or an alkyl group and silver halide, forming developed silver imagewise by development processing and then processing with an aqueous solution containing peroxoic acids or salt thereof to thereby oxidatively bleach said dye.
Claim 3
Dependent Claim 18 words
The method for forming color images of claim 1, wherein said polymer is present in said photographic element.
Claim 4
Dependent Claim 20 words
The method for forming color images of claim 1, wherein said polymer contains at least 50 mol% of the vinylpyridine.
Claim 5
Dependent Claim 20 words
The method for forming color images of claim 1, wherein said vinylpyridine is selected from 2-vinylpyridine, 3-vinylpyridine, 4-vinylpyridine and 2-methyl-5-vinylpyridine.
Claim 6
Dependent Claim 32 words
The method of claim 1, wherein said oxidizing agent is present in a silver halide emulsion layer, in a layer adjacent a silver halide emulsion layer or in a separate processing solution.
Claim 7
Dependent Claim 40 words
The method of claim 5, wherein said oxidizing agent is present in the silver halide emulsion layer or a layer adjacent the silver halide emulsion layer and is present in an amount of about 0.01 to 0.2 mol/m 2 .
Claim 8
Dependent Claim 25 words
The method of claim 5, wherein said oxidizing agent is present in a separate processing solution in an amount of 1×10 -3 to 2 mols/l.
Claim 9
Dependent Claim 18 words
The method of claim 7, wherein said oxidizing agent solution has a pH of about 2 to 7.
Claim 10
Dependent Claim 26 words
The method of claim 1, wherein said polymer is present in said silver halide emulsion layer or in a layer adjacent said silver halide emulsion layer.
Claim 11
Dependent Claim 23 words
The method of claim 9, wherein said polymer is present in an amount of about 100 mg/m 2 to 10 g/m 2 .
Claim 12
Dependent Claim 30 words
The method of claim 1, wherein said dye is present in the silver halide emulsion layer, a layer adjacent said silver halide emulsion layer or in a separate processing solution.
Claim 13
Dependent Claim 31 words
The method of claim 11, wherein said dye is present in said silver halide emulsion layer or said adjacent layer in an amount of about 0.1 to 0.5 g/m 2 .
Claim 14
Dependent Claim 24 words
The method of claim 11, wherein said dye is present in a separate processing solution in an amount of 5 to about 50 g/l.
Claim 15
Dependent Claim 16 words
The method of claim 11, wherein said dye is an azo dye or an anthraquinone dye.
Claim 16
Dependent Claim 30 words
The method of claim 1, wherein said oxidizing agent has an oxidation-reduction potential higher than that of a silver(I)/silver(II) pair in the presence of polyvinylpyridine at the oxidative processing pH.
Claim 17
Dependent Claim 29 words
The method of claim 1, wherein said dye has an oxidation potential less than that of the silver(I)/silver(II) pair in the presence of polyvinylpyridine at the oxidative processing pH.

References Cited (Backward Citations)

US2564238A Cited
US3040012A Cited
US3259497A Cited
US3455690A Cited
US3716362A Cited
US3773509A Cited
US3772020A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1983-10-21 1984-04-21 1984-10-21 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1987-10-21 1988-04-21 1988-10-21 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1991-10-21 1992-04-21 1992-10-21 $7700.00 Window Closed / Lapsed