Abstract

Abstract Piezoelectric ceramics are provided consisting of a ternary system composition of PbTiO3-PbZrO3-La(Mn1-4 alpha Ni3 alpha W alpha )O3 where alpha is in the range of 3/40</= alpha </=1/4.

Inventors

  • 👤 Hiroshi Satomura
  • 👤 Katsuyoshi Takano

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 06:56
CPC Classifications
H; H10; H10N; H10N30/00; H10N30/80; H10N30/85; H10N30/853; C; C04; C04B; C04B35/00; C04B35/01; C04B35/48; C04B35/49; C04B35/491

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 126 words
A ternary system piezoelectric ceramic compound represented by a molecular formula xLa(Mn.sub.1-4α Ni.sub.3α W.sub.α)O.sub.3 - yPbTiO.sub.3 - zPbZrO.sub.3 having a composition within the area defined by the points A, B, C, D, E, F and G in the ternary diagram of FIG. 1 the coordinates of said points being: ______________________________________ A (x=0.005, y=0.565, z=0.43) B (x=0.005, y=0.295, z=0.70) C (x=0.05, y=0.25, z=0.70) D (x=0.10, y=0.30, z=0.60) E (x=0.10, y=0.45, z=0.45) F (x=0.08, y=0.51, z=0.41) G (x=0.05, y=0.55, z=0.40) ______________________________________ where x, y and z represent molar fractions of constituents of said piezoelectric ceramic compound respectively and x+y+z is equal to unity, the molar fraction α in (Mn 1-4 α Ni 3 α W.sub.α) of the x-constituent of said piezoelectric ceramic compound being within the range 3/40≦α≦1/4.
Claim 2
Dependent Claim 126 words
A ternary system piezoelectric ceramic compound represented by a molecular formula xLa(Mn.sub.1-4α Ni.sub.3α W.sub.α)O.sub.3 - yPbTiO.sub.3 - zPbZrO.sub.3 having a composition within the area defined by the points A, B, C, D, E, F and G in the ternary diagram of FIG. 1 the coordinates of said points being: ______________________________________ A (x=0.005, y=0.565, z=0.43) B (x=0.005, y=0.295, z=0.70) C (x=0.05, y=0.25, z=0.70) D (x=0.10, y=0.30, z=0.60) E (x=0.10, y=0.45, z=0.45) F (x=0.08, y=0.51, z=0.41) G (x=0.05, y=0.55, z=0.40) ______________________________________ where x, y and z represent molar fractions of constituents of said piezoelectric ceramic compound respectively and x+y+z is equal to unity, the molar fraction α in (Mn 1-4 α Ni 3 α W.sub.α) of the x-constituent of said piezoelectric ceramic compound being within the range 3/40≦α≦1/4.

References Cited (Backward Citations)

US3533951A Cited
DE2063420A1 Cited
JPS4721519U Cited
GB1401389A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1983-09-02 1984-03-03 1984-09-02 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1987-09-02 1988-03-03 1988-09-02 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1991-09-02 1992-03-03 1992-09-02 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag