Method for producing cobalt metal powder

Assignee: GTE Sylvania Inc
•
Filing: 1979-05-14
•
Granted: 1980-07-29
•
Expires: 1999-05-14
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Fine particle size cobalt metal powder is prepared by treating an aqueous solution of a soluble cobaltic ammine halide with a sufficient amount of a soluble metallic hydroxide to form a cobalt containing precipitate. The precipitate is separated from the solution and reduced in a reducing atmosphere to produce metallic cobalt.

Inventors

  • 👤 Richard G. W. Gingerich
  • 👤 Clarence D. Vanderpool
  • 👤 Mary A. Fedorchak
  • 👤 Joseph E. Ritsko
  • 👤 Michael J. Cheresnowsky

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-03 14:55
CPC Classifications
C; C22; C22B; C22B23/00; C22B23/04; C22B23/0453; C22B23/0461; C22B23/0469; B; B22; B22F; B22F9/00; B22F9/16; B22F9/18; B22F9/20; B22F9/22; C01; C01G; C01G51/00; C01G51/20

Claims Analysis

Total Claims: 15
Claim 1
Independent Claim 54 words
A method for producing fine cobalt metal powder comprising treating an aqueous solution of a soluble cobaltic ammine halide with a sufficient amount of a soluble metallic hydroxide to form a cobalt containing precipitate, separating the cobalt containing precipitate from the resulting solution, reducing said cobalt containing precipitate to form fine particles of cobalt.
Claim 2
Independent Claim 54 words
A method for producing fine cobalt metal powder comprising treating an aqueous solution of a soluble cobaltic ammine halide with a sufficient amount of a soluble metallic hydroxide to form a cobalt containing precipitate, separating the cobalt containing precipitate from the resulting solution, reducing said cobalt containing precipitate to form fine particles of cobalt.
Claim 3
Dependent Claim 19 words
A method according to claim 1 wherein said aqueous solution comprises greater than about 5 percent by weight cobalt.
Claim 4
Dependent Claim 29 words
A method according to claim 1 wherein said soluble cobaltic ammine halide is selected from the group consisting of cobaltic hexammine halide and cobaltic pentammine halide and mixtures thereof.
Claim 5
Dependent Claim 19 words
A method according to claim 1 wherein said aqueous solution comprises greater than about 15 percent by weight cobalt.
Claim 6
Dependent Claim 20 words
A method according to claim 1 wherein said metallic hydroxide is an alkali metal hydroxide or alkaline earth metal hydroxide.
Claim 7
Dependent Claim 15 words
A method according to claim 5 wherein said metallic hydroxide is an alkali metal hydroxide.
Claim 8
Dependent Claim 16 words
A method according to claim 6 wherein said metallic hydroxide is sodium hydroxide or potassium hydroxide.
Claim 9
Dependent Claim 32 words
A method according to claim 7 wherein said aqueous solution is treated by adding metallic hydroxide to said solution until said solution has a pH of from about 10 to about 12.
Claim 10
Dependent Claim 29 words
A method according to claim 8 wherein metallic hydroxide is present in an amount at least equal to a stoichiometric amount to permit the formation of cobalt oxide hydrate.
Claim 11
Dependent Claim 31 words
A method according to claim 8 wherein said addition is carried out at a temperature greater than about 50° C. and for a period of time greater than about 15 minutes.
Claim 12
Dependent Claim 37 words
A method according to claim 8 wherein said addition is carried out a temperature greater than about 60° C. up to the boiling point of said solution for a period of time greater than about 30 minutes.
Claim 13
Dependent Claim 19 words
A method according to claim 8 wherein said cobalt containing precipitate comprises a black cobalt hydrate in amorphous form.
Claim 14
Dependent Claim 25 words
A method according to claim 12 werein said cobalt containing precipitate is reducible to cobalt particles having a particle size less than about 2 microns.
Claim 15
Dependent Claim 43 words
A method according to claim 1 wherein said aqueous solution of a soluble cobaltic ammine complex is formed from an aqueous solution comprising cobaltous and cobaltic ion by adding ammonia hydroxide to said solution and oxidizing the cobaltous ion to the cobaltic ion.

References Cited (Backward Citations)

DE1583864C Cited
US2826499A Cited
US2879137A Cited
DE2319703A1 Cited
US3928530A Cited
US3933976A Cited
US4108640A Cited
US4093450A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1983-07-29 1984-01-28 1984-07-29 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1987-07-29 1988-01-28 1988-07-29 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1991-07-29 1992-01-28 1992-07-29 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag