Thermoplastic moulding compositions
Abstract
Abstract A thermoplastic moulding composition comprising: (1.) 80 to 20 parts by wt. of a thermoplastic polycarbonate based on a dihydroxy diaryl alkane, (2.) 20 to 80 parts by wt. of a graft polymer of 2.2. a monomer mixture, polymerized onto 2.1. a diene rubber with a glass transition temperature below -30° C., of 2.2.1. 95 to 50% by wt. of styrene, methyl methacrylate or a mixture thereof; and 2.2.2. 50 to 5% by wt. of acrylonitrile, methacrylonitrile or a mixture thereof, the ratio by wt. of rubber (2.1) to monomer mixture (2.2.) being in the range of from 80:20 and 10:90, and the moulding composition containing from 5 to 35% by wt. of the rubber (2.1.), and (3.) 5 to 75 parts by wt. of a copolymer which is chemically uniform in structure and which comprises: (3.1.) 93 to 50 parts by wt. of styrene, methyl methacrylate or a mixture thereof; (3.2.) 40 to 5 parts by weight of acrylonitrile, methacrylonitrile or a mixture thereof; and (3.3.) 2 to 30 parts by wt. of maleic acid anhydride.
Inventors
- 👤 Lothar Liebig
- 👤 Frank Wingler
- 👤 Dieter Margotte
- 👤 Werner Nouvertne
Bibliographic Details
Claims Analysis
Total Claims: 5References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1983-05-27 | 1983-11-26 | 1984-05-27 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1987-05-27 | 1987-11-26 | 1988-05-27 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1991-05-27 | 1991-11-26 | 1992-05-27 | $7700.00 | Window Closed / Lapsed |