Claims Analysis
Total Claims: 18
Claim 1
Independent Claim
150 words
An improved refrigerator cabinet construction comprising, in laminated sequence, a metal outer layer, a foam layer, a composite release film and strongly bonded thereto an ABS layer in which the improvement comprises providing a strong bond between all but two of the various contiguous layers and a weak bond between the remaining pair of contiguous layers, the relative strengths of the bonds being such that when the laminate is cycled between room temperature and -22° C. causing differential thermal expansion of the layers in the laminate, only the weak bond is ruptured and the location of the weak bond being such that, in the event it were to be ruptured, the ABS layer and the portion of the laminate remaining adhered thereto would be re-processable to produce an ABS with a Gardner impact strength that is at least 85% of that of the original ABS sheet incorporated in the laminate.
Claim 2
Dependent Claim
150 words
An improved refrigerator cabinet construction comprising, in laminated sequence, a metal outer layer, a foam layer, a composite release film and strongly bonded thereto an ABS layer in which the improvement comprises providing a strong bond between all but two of the various contiguous layers and a weak bond between the remaining pair of contiguous layers, the relative strengths of the bonds being such that when the laminate is cycled between room temperature and -22° C. causing differential thermal expansion of the layers in the laminate, only the weak bond is ruptured and the location of the weak bond being such that, in the event it were to be ruptured, the ABS layer and the portion of the laminate remaining adhered thereto would be re-processable to produce an ABS with a Gardner impact strength that is at least 85% of that of the original ABS sheet incorporated in the laminate.
Claim 3
Dependent Claim
22 words
A refrigerator cabinet construction according to claim 1 in which the weak bond is between the composite release film and the foam.
Claim 4
Dependent Claim
82 words
A refrigerator cabinet construction according to claim 2 in which the composite release film comprises a first layer of a polar polymer that is compatible with ABS at least up to the 4% by weight level and does not degrade at temperatures below 270° C. and a second layer of a non-polar polymer that is incompatible with the ABS, the first and second layers having thicknesses of up to 4% and up to 0.9% respectively of the thickness of the ABS layer.
Claim 5
Dependent Claim
62 words
A refrigerator cabinet construction according to claim 3 wherein the thickness of the ABS sheet before thermoforming is from 3 to 8 mm and wherein the first layer of the composite release film comprises a polymer selected from nylon 6 and a nitrile copolymer containing from 55 to 90% by weight of a nitrile monomer, and the second layer is a polyolefin.
Claim 6
Dependent Claim
25 words
A refrigerator cabinet construction according to claim 2 in which the composite release film comprises a layer that is an effective barrier to halohydrocarbon gases.
Claim 7
Dependent Claim
22 words
A refrigerator cabinet construction according to claim 1 in which the weak bond is between contiguous layers of the composite release film.
Claim 8
Dependent Claim
58 words
A refrigerator cabinet construction according to claim 7 in which the composite release film comprises a first layer formed from a polar polymer that is compatible with ABS at least up to the 4% by weight level, and does not degrade at temperatures below 270° C. which layer, in the laminate, is bonded to the ABS inner layer.
Claim 9
Dependent Claim
36 words
A refrigerator cabinet construction according to claim 8 in which the composite release film is a bilayer in which one or both of the contiguous surfaces of the bilayer has been treated with an adhesion-reducing substance.
Claim 10
Dependent Claim
17 words
A refrigerator cabinet construction according to claim 9 in which the layers of the bilayer are identical.
Claim 11
Dependent Claim
44 words
A refrigerator cabinet construction according to claim 8 in which the first layer of the composite release film is a polymer selected from the group consisting of nitrile polymers containing from 55 to 90% by weight of a nitrile monomer, polyethylene terephthalate and polycaprolactam.
Claim 12
Dependent Claim
25 words
A refrigerator cabinet construction according to claim 7 in which the composite release fil comprises a layer that is an effective barrier to halohydrocarbon gases.
Claim 13
Dependent Claim
157 words
A refrigerator cabinet construction comprising a laminate of an ABS layer bonded to a composite release film comprising a first layer bonded to the ABS that is up to 4% of the thickness of the ABS layer and is formed from a polymer selected from polycaprolactam, polyethylene terephthalate and a nitrile polymer containing from 55 to 90% of an unsaturated nitrile monomer; and a second layer bonded to the first and having a thickness of up to 0.9% of the ABS inner layer thickness and formed from a olefin polymer, and bonded to said release film, a layer of a polyurethane foam which is in turn bonded to a metal outer layer, the bonding within the laminate being such that upon cycling between room temperature and -22° C. the differential thermal expansion of the layers in the laminate cause only the bond between the foam and the second layer of the composite release film to be ruptured.
Claim 14
Dependent Claim
157 words
A refrigerator cabinet construction comprising a laminate of an ABS layer bonded to a composite release film comprising a first layer bonded to the ABS that is up to 4% of the thickness of the ABS layer and is formed from a polymer selected from polycaprolactam, polyethylene terephthalate and a nitrile polymer containing from 55 to 90% of an unsaturated nitrile monomer; and a second layer bonded to the first and having a thickness of up to 0.9% of the ABS inner layer thickness and formed from a olefin polymer, and bonded to said release film, a layer of a polyurethane foam which is in turn bonded to a metal outer layer, the bonding within the laminate being such that upon cycling between room temperature and -22° C. the differential thermal expansion of the layers in the laminate cause only the bond between the foam and the second layer of the composite release film to be ruptured.
Claim 15
Dependent Claim
148 words
An improved refrigerator cabinet construction comprising a laminate of an ABS inner layer bonded to a composite release film comprising a first layer formed of a polymer selected from nitrile polymers containing from 55 to 90% by weight of a nitrile monomer, polyethylene terephthalate and polycaprolactam and a second layer bonded to the first and formed of an olefin polymer, and bonded to the second layer a foamed polyurethane layer which is in turn bonded to a metal outer layer, wherein one or both of the contiguous faces of the first and second layers of the composite release film has been treated with an adhesion reducing agent such that when the laminate is cycled between room temperature and -22° C., the differential thermal expansion of the layers in the laminate cause only the bond between the first and second layers of the composite release film to be ruptured.
Claim 16
Dependent Claim
148 words
An improved refrigerator cabinet construction comprising a laminate of an ABS inner layer bonded to a composite release film comprising a first layer formed of a polymer selected from nitrile polymers containing from 55 to 90% by weight of a nitrile monomer, polyethylene terephthalate and polycaprolactam and a second layer bonded to the first and formed of an olefin polymer, and bonded to the second layer a foamed polyurethane layer which is in turn bonded to a metal outer layer, wherein one or both of the contiguous faces of the first and second layers of the composite release film has been treated with an adhesion reducing agent such that when the laminate is cycled between room temperature and -22° C., the differential thermal expansion of the layers in the laminate cause only the bond between the first and second layers of the composite release film to be ruptured.
Claim 17
Dependent Claim
129 words
An improved refrigerator cabinet construction comprising a laminate of an ABS inner layer bonded to a composite release film comprising identical layers of a polymer selected from nitrile polymers containing from 55 to 90% by weight of a nitrile monomer, polyethylene terephthalate and polycaprolactam which is bonded to a polyurethane foam layer which in turn is bonded to a metal outer layer, wherein the one or both of the contiguous faces of the two layers of the composite release film has been treated with an adhesion reducing agent such that when the laminate is cycled between room temperature and -22° C., the differential thermal expansion of the layers in the laminate cause only the bond between the first and second layers of the composite release film to be ruptured.
Claim 18
Dependent Claim
129 words
An improved refrigerator cabinet construction comprising a laminate of an ABS inner layer bonded to a composite release film comprising identical layers of a polymer selected from nitrile polymers containing from 55 to 90% by weight of a nitrile monomer, polyethylene terephthalate and polycaprolactam which is bonded to a polyurethane foam layer which in turn is bonded to a metal outer layer, wherein the one or both of the contiguous faces of the two layers of the composite release film has been treated with an adhesion reducing agent such that when the laminate is cycled between room temperature and -22° C., the differential thermal expansion of the layers in the laminate cause only the bond between the first and second layers of the composite release film to be ruptured.