Method of beneficiating phosphate ores
Assignee: IMC Fertilizer Inc
•
Filing: 1978-03-10
•
Granted: 1980-02-19
•
Expires: 1998-03-10
Abstract
Abstract A method is disclosed for beneficiating a phosphate ore matrix containing apatite, siliceous gangue, and an alkaline earth metal carbonate mineral impuritywhich includes the steps of washing and sizing the ore, subjecting it to a gravity separation, a conventional "double float" flotation, and a phosphate-carbonate flotation separation to provide a phosphate ore concentrate having a high BPL content and a relatively low concentration of alkaline earth metal carbonate mineral impurity.
Inventors
- 👤 James E. Lawver
- 👤 Robert E. Snow
- 👤 Walter O. McClintock
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-08 23:02
CPC Classifications
B; B03; B03B; B03B7/00; B03D; B03D1/00; B03D1/02; B03D1/021; B03D1/08; B03D1/085; Y; Y10; Y10S; Y10S209/00; Y10S209/902
Claims Analysis
Total Claims: 24
Claim 1
Independent Claim
281 words
A method for beneficiating a phosphate ore matrix containing apatite, siliceous gangue, and an alkaline earth metal carbonate mineral impurity, comprising the steps of (a) washing and sizing the ore matrix to substantially deslime the matrix and to remove particles larger than from about 2 mesh to about 5 mesh, thereby forming a deslimed ore matrix; (b) splitting the deslimed ore matrix at about 12 to about 20 mesh to form a pebble fraction having a particle size greater than about 12 to about 20 mesh and a middle ore fraction having a particle size less than about 12 to about 20 mesh; (c) subjecting the pebble fraction to a gravity separation wherein a portion of the less dense alkaline earth metal carbonate mineral impurity is separated from the apatite, thereby producing a low-carbonate fraction; (d) splitting the middle ore fraction at about 24 mesh to about 32 mesh to form a coarse fraction having a particle size greater than about 24 mesh to about 32 mesh and a fine fraction having a particle size smaller than about 24 mesh to about 32 mesh; (e) combining the coarse fraction with the pebble fraction to enter the gravity separation of step (c); (f) comminuting, sizing and desliming the low-carbonate fraction to a deslimed particle size of less than about 24 to about 32 mesh, thereby forming a flotation feed containing discreet particles of apatite and siliceous gangue; (g) subjecting the flotation feed to a "double float" flotation, thereby forming a low silica intermediate flotation concentrate; and (h) subjecting the low silica intermediate flotation concentrate to a flotation to remove alkaline earth metal carbonate mineral impurity therefrom and to form a phosphate concentrate.
Claim 2
Independent Claim
281 words
A method for beneficiating a phosphate ore matrix containing apatite, siliceous gangue, and an alkaline earth metal carbonate mineral impurity, comprising the steps of (a) washing and sizing the ore matrix to substantially deslime the matrix and to remove particles larger than from about 2 mesh to about 5 mesh, thereby forming a deslimed ore matrix; (b) splitting the deslimed ore matrix at about 12 to about 20 mesh to form a pebble fraction having a particle size greater than about 12 to about 20 mesh and a middle ore fraction having a particle size less than about 12 to about 20 mesh; (c) subjecting the pebble fraction to a gravity separation wherein a portion of the less dense alkaline earth metal carbonate mineral impurity is separated from the apatite, thereby producing a low-carbonate fraction; (d) splitting the middle ore fraction at about 24 mesh to about 32 mesh to form a coarse fraction having a particle size greater than about 24 mesh to about 32 mesh and a fine fraction having a particle size smaller than about 24 mesh to about 32 mesh; (e) combining the coarse fraction with the pebble fraction to enter the gravity separation of step (c); (f) comminuting, sizing and desliming the low-carbonate fraction to a deslimed particle size of less than about 24 to about 32 mesh, thereby forming a flotation feed containing discreet particles of apatite and siliceous gangue; (g) subjecting the flotation feed to a "double float" flotation, thereby forming a low silica intermediate flotation concentrate; and (h) subjecting the low silica intermediate flotation concentrate to a flotation to remove alkaline earth metal carbonate mineral impurity therefrom and to form a phosphate concentrate.
Claim 3
Dependent Claim
45 words
The method of claim 1, further comprising the steps of (i) subjecting the fine fraction from step (d) to attrition scrubbing and desliming to form a carbonate-reduced fine fraction; (j) subjecting the carbonate-reduced fine fraction to a "double-float" flotation, thereby forming a "double float" concentrate.
Claim 4
Dependent Claim
15 words
The method of claim 2 wherein the alkaline earth metal carbonate mineral impurity is dolomite.
Claim 5
Dependent Claim
15 words
The method of claim 2 wherein the alkaline earth metal carbonate mineral impurity is calcite.
Claim 6
Dependent Claim
59 words
The method of claim 2 wherein the gravity separation is a heavy media separation employing an aqueous suspension of magnetite or ferrosilicon having a specific gravity of from about 1.8 to about 2.5 as the heavy medium, and wherein the flotation to remove alkaline earth metal carbonate mineral impurity from the low-silica intermediate flotation concentrate is a "carbonate" flotation.
Claim 7
Dependent Claim
36 words
The method of claim 2 further comprising the step of subjecting the "double float" concentrate of step (J) to a flotation to remove akaline earth metal carbonate mineral impurities therefrom and to form a phosphate concentrate.
Claim 8
Dependent Claim
52 words
The method of claim 6 wherein the gravity separation is a heavy media separation employing an aqueous suspension of magnetite or ferrosilicon having a specific gravity of from about 1.8 to about 2.5 as the heavy medium, and wherein the flotations to remove alkaline earth metal carbonate mineral impurity are "carbonate" flotations.
Claim 9
Dependent Claim
65 words
The method of claim 1 wherein the alkaline earth metal carbonate mineral impurity is dolomite; the deslimed ore fraction is split at about 16 mesh in step (b); the middle ore fraction is split at about 28 mesh in step (d); and the flotation feed produced in step (f) is comminuted, sized and deslimed to a deslimed particle size of less than about 28 mesh.
Claim 10
Dependent Claim
52 words
The method of claim 8 wherein the gravity separation is a heavy media separation employing an aqueous suspension of magnetite or ferrosilicon having a specific gravity of from about 1.8 to about 2.5 as the heavy medium, and the flotation to remove alkaline earth metal carbonate mineral impurity is a "carbonate" flotation.
Claim 11
Dependent Claim
14 words
The method of claim 1 wherein the alkaline earth metal carbonate impurity is calcite.
Claim 12
Dependent Claim
47 words
The method of claim 1 wherein the gravity separation is a heavy media separation employing an aqueous suspension of magnetite or ferrosilicon having a specific gravity of from about 1.8 to about 2.5 as the heavy medium, and the flotation of step (h) is a "carbonate" flotation.
Claim 13
Independent Claim
250 words
A method for beneficiating a phosphate ore matrix containing apatite, siliceous gangue, and an alkaline earth metal carbonate mineral impurity, comprising the steps of (a) washing and sizing the ore matrix to substantially deslime the matrix and to remove particles larger than from about 2 mesh to about 5 mesh thereby forming a deslimed ore matrix; (b) splitting the deslimed ore matrix at about 12 to about 20 mesh to form a pebble fraction having a particle size greater than about 12 to about 20 mesh and a middle ore fraction having a particle size less than about 12 to about 20 mesh; (c) subjecting the pebble fraction to a gravity separation wherein a portion of the less dense alkaline earth metal carbonate mineral impurity is separated from the apatite, thereby producing a low carbonate fraction; (d) splitting the middle ore fraction at about 24 mesh to about 32 mesh to form a coarse fraction having a particle size greater than about 24 mesh to about 32 mesh and a fine fraction having a particle size smaller than about 24 mesh to about 32 mesh; (e) combining the coarse fraction with the pebble fraction to enter the gravity separation of step (c); (f) comminuting, sizing and desliming the low-carbonate fraction to a deslimed particle size of less tha about 24 to about 32 mesh,thereby forming a flotation feed; (g) subjecting the flotation feed to a flotation to remove alkaline earth metal carbonate impurity therefrom and to form a phosphate concentrate.
Claim 14
Independent Claim
250 words
A method for beneficiating a phosphate ore matrix containing apatite, siliceous gangue, and an alkaline earth metal carbonate mineral impurity, comprising the steps of (a) washing and sizing the ore matrix to substantially deslime the matrix and to remove particles larger than from about 2 mesh to about 5 mesh thereby forming a deslimed ore matrix; (b) splitting the deslimed ore matrix at about 12 to about 20 mesh to form a pebble fraction having a particle size greater than about 12 to about 20 mesh and a middle ore fraction having a particle size less than about 12 to about 20 mesh; (c) subjecting the pebble fraction to a gravity separation wherein a portion of the less dense alkaline earth metal carbonate mineral impurity is separated from the apatite, thereby producing a low carbonate fraction; (d) splitting the middle ore fraction at about 24 mesh to about 32 mesh to form a coarse fraction having a particle size greater than about 24 mesh to about 32 mesh and a fine fraction having a particle size smaller than about 24 mesh to about 32 mesh; (e) combining the coarse fraction with the pebble fraction to enter the gravity separation of step (c); (f) comminuting, sizing and desliming the low-carbonate fraction to a deslimed particle size of less tha about 24 to about 32 mesh,thereby forming a flotation feed; (g) subjecting the flotation feed to a flotation to remove alkaline earth metal carbonate impurity therefrom and to form a phosphate concentrate.
Claim 15
Dependent Claim
40 words
The method of claim 12 further comprising the steps of subjecting the flotation feed from step (f) to a conventional amine flotation to form an intermediate flotation concentrate, and subjecting the intermediate flotation concentrate to the flotation of step (g).
Claim 16
Dependent Claim
52 words
The method of claim 13 wherein the gravity separation is a heavy media separation employing an aqueous suspension of magnetite or ferrosilicon having a specific gravity of from about 1.8 to about 2.5 as the heavy medium, and the flotation to remove alkaline earth metal carbonate mineral impurity is a "carbonate" flotation.
Claim 17
Dependent Claim
47 words
The method of claim 12 wherein the gravity separation is a heavy media separation employing an aqueous suspension of magnetite or ferrosilicon having a specific gravity of from about 1.8 to about 2.5 as the heavy medium, and the flotation of step (g) is a "carbonate" flotation.
Claim 18
Independent Claim
249 words
A method for beneficiating a phosphate ore matrix containing apatite, siliceous gangue, and an alkaline earth metal carbonate mineral impurity, comprising the steps of (a) washing and sizing the ore matrix to substantially deslime the matrix and to remove particles larger than from about 2 mesh to about 5 mesh, thereby forming a deslimed ore matrix; (b) splitting the deslimed ore matrix at about 12 to about 20 mesh to form a pebble fraction having a particle size greater than about 12 to about 20 mesh and a middle ore fraction having a particle size less than about 12 to about 20 mesh; (c) subjecting the pebble fraction to a gravity separation wherein a portion of the less dense alkaline earth metal carbonate mineral impurity is separated from the apatite, thereby producing a low-carbonate fraction; (d) splitting the middle ore fraction at about 24 mesh to about 32 mesh to form a coarse fraction having a particle size greater than about 24 mesh to about 32 mesh and a fine fraction having a particle size smaller than about 24 mesh to about 32 mesh; (e) combining the coarse fraction with the low-carbonate fraction from the gravity separation of step (c); (f) comminuting, sizing and desliming the low-carbonate fraction to a deslimed particle size of less than about 24 to about 32 mesh, thereby forming a flotation feed; (g) subjecting the flotation feed to a flotation to remove alkaline earth metal carbonate mineral impurity and to form a phosphate concentrate.
Claim 19
Independent Claim
249 words
A method for beneficiating a phosphate ore matrix containing apatite, siliceous gangue, and an alkaline earth metal carbonate mineral impurity, comprising the steps of (a) washing and sizing the ore matrix to substantially deslime the matrix and to remove particles larger than from about 2 mesh to about 5 mesh, thereby forming a deslimed ore matrix; (b) splitting the deslimed ore matrix at about 12 to about 20 mesh to form a pebble fraction having a particle size greater than about 12 to about 20 mesh and a middle ore fraction having a particle size less than about 12 to about 20 mesh; (c) subjecting the pebble fraction to a gravity separation wherein a portion of the less dense alkaline earth metal carbonate mineral impurity is separated from the apatite, thereby producing a low-carbonate fraction; (d) splitting the middle ore fraction at about 24 mesh to about 32 mesh to form a coarse fraction having a particle size greater than about 24 mesh to about 32 mesh and a fine fraction having a particle size smaller than about 24 mesh to about 32 mesh; (e) combining the coarse fraction with the low-carbonate fraction from the gravity separation of step (c); (f) comminuting, sizing and desliming the low-carbonate fraction to a deslimed particle size of less than about 24 to about 32 mesh, thereby forming a flotation feed; (g) subjecting the flotation feed to a flotation to remove alkaline earth metal carbonate mineral impurity and to form a phosphate concentrate.
Claim 20
Dependent Claim
39 words
The method of claim 16 furthercomprising the steps of subjecting the flotation feed from step (f) to a conventional amine flotation to form an intermediate flotation concentrate, and subjecting the intermediate flotation concentrate to the flotation of step (g).
Claim 21
Dependent Claim
52 words
The method of claim 17 wherein the gravity separation is a heavy media separation employing an aqueous suspension of magnetite or ferrosilicon having a specific gravity of from about 1.8 to about 2.5 as the heavy medium, and the flotation to remove alkaline earth metal carbonate mineral impurity is a "carbonate" flotation.
Claim 22
Dependent Claim
40 words
The method of claim 16 further comprising the steps of subjecting the flotation feed from step (f) to a "double float" flotation to form an intermediate flotation concentrate and subjecting the intermediate flotation concentrate to the flotation of step (g).
Claim 23
Dependent Claim
52 words
The method of claim 19 wherein the gravity separation is a heavy media separation employing the aqueous suspension of magnetite or ferrosilicon having a specific gravity of from about 1.8 to about 2.5 as the heavy medium, and the flotation to remove alkaline earth metal carbonate mineral impurity is a "carbonate" flotation.
Claim 24
Dependent Claim
47 words
The method of claim 16 wherein the gravity separation is a heavy media separation employing an aqueous suspension of magnetite or ferrosilicon having a specific gravity of from about 1.8 to about 2.5 as the heavy medium, and the flotation of step (g) is a "carbonate" flotation.
References Cited (Backward Citations)
CA653588A
Cited
US2158220A
Cited
US2384825A
Cited
US2385079A
Cited
US2599530A
Cited
US2526519A
Cited
US2668617A
Cited
US2610738A
Cited
US2676705A
Cited
US2763371A
Cited
US2914173A
Cited
US3259242A
Cited
US3348675A
Cited
US3388793A
Cited
US3454159A
Cited
US3462017A
Cited
US3534854A
Cited
US3750963A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1983-02-18 | 1983-08-20 | 1984-02-19 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1987-02-18 | 1987-08-20 | 1988-02-19 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1991-02-18 | 1991-08-20 | 1992-02-19 | $7700.00 | Window Closed / Lapsed |