Abstract

Abstract A method is disclosed for beneficiating a phosphate ore matrix containing apatite, siliceous gangue, and an alkaline earth metal carbonate mineral impuritywhich includes the steps of washing and sizing the ore, subjecting it to a gravity separation, a conventional "double float" flotation, and a phosphate-carbonate flotation separation to provide a phosphate ore concentrate having a high BPL content and a relatively low concentration of alkaline earth metal carbonate mineral impurity.

Inventors

  • 👤 James E. Lawver
  • 👤 Robert E. Snow
  • 👤 Walter O. McClintock

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-08 22:41
CPC Classifications
B; B03; B03B; B03B7/00; B03D; B03D1/00; B03D1/02; B03D1/021; B03D1/08; B03D1/085; Y; Y10; Y10S; Y10S209/00; Y10S209/902

Claims Analysis

Total Claims: 24
Claim 1
Independent Claim 281 words
A method for beneficiating a phosphate ore matrix containing apatite, siliceous gangue, and an alkaline earth metal carbonate mineral impurity, comprising the steps of (a) washing and sizing the ore matrix to substantially deslime the matrix and to remove particles larger than from about 2 mesh to about 5 mesh, thereby forming a deslimed ore matrix; (b) splitting the deslimed ore matrix at about 12 to about 20 mesh to form a pebble fraction having a particle size greater than about 12 to about 20 mesh and a middle ore fraction having a particle size less than about 12 to about 20 mesh; (c) subjecting the pebble fraction to a gravity separation wherein a portion of the less dense alkaline earth metal carbonate mineral impurity is separated from the apatite, thereby producing a low-carbonate fraction; (d) splitting the middle ore fraction at about 24 mesh to about 32 mesh to form a coarse fraction having a particle size greater than about 24 mesh to about 32 mesh and a fine fraction having a particle size smaller than about 24 mesh to about 32 mesh; (e) combining the coarse fraction with the pebble fraction to enter the gravity separation of step (c); (f) comminuting, sizing and desliming the low-carbonate fraction to a deslimed particle size of less than about 24 to about 32 mesh, thereby forming a flotation feed containing discreet particles of apatite and siliceous gangue; (g) subjecting the flotation feed to a "double float" flotation, thereby forming a low silica intermediate flotation concentrate; and (h) subjecting the low silica intermediate flotation concentrate to a flotation to remove alkaline earth metal carbonate mineral impurity therefrom and to form a phosphate concentrate.
Claim 2
Independent Claim 281 words
A method for beneficiating a phosphate ore matrix containing apatite, siliceous gangue, and an alkaline earth metal carbonate mineral impurity, comprising the steps of (a) washing and sizing the ore matrix to substantially deslime the matrix and to remove particles larger than from about 2 mesh to about 5 mesh, thereby forming a deslimed ore matrix; (b) splitting the deslimed ore matrix at about 12 to about 20 mesh to form a pebble fraction having a particle size greater than about 12 to about 20 mesh and a middle ore fraction having a particle size less than about 12 to about 20 mesh; (c) subjecting the pebble fraction to a gravity separation wherein a portion of the less dense alkaline earth metal carbonate mineral impurity is separated from the apatite, thereby producing a low-carbonate fraction; (d) splitting the middle ore fraction at about 24 mesh to about 32 mesh to form a coarse fraction having a particle size greater than about 24 mesh to about 32 mesh and a fine fraction having a particle size smaller than about 24 mesh to about 32 mesh; (e) combining the coarse fraction with the pebble fraction to enter the gravity separation of step (c); (f) comminuting, sizing and desliming the low-carbonate fraction to a deslimed particle size of less than about 24 to about 32 mesh, thereby forming a flotation feed containing discreet particles of apatite and siliceous gangue; (g) subjecting the flotation feed to a "double float" flotation, thereby forming a low silica intermediate flotation concentrate; and (h) subjecting the low silica intermediate flotation concentrate to a flotation to remove alkaline earth metal carbonate mineral impurity therefrom and to form a phosphate concentrate.
Claim 3
Dependent Claim 45 words
The method of claim 1, further comprising the steps of (i) subjecting the fine fraction from step (d) to attrition scrubbing and desliming to form a carbonate-reduced fine fraction; (j) subjecting the carbonate-reduced fine fraction to a "double-float" flotation, thereby forming a "double float" concentrate.
Claim 4
Dependent Claim 15 words
The method of claim 2 wherein the alkaline earth metal carbonate mineral impurity is dolomite.
Claim 5
Dependent Claim 15 words
The method of claim 2 wherein the alkaline earth metal carbonate mineral impurity is calcite.
Claim 6
Dependent Claim 59 words
The method of claim 2 wherein the gravity separation is a heavy media separation employing an aqueous suspension of magnetite or ferrosilicon having a specific gravity of from about 1.8 to about 2.5 as the heavy medium, and wherein the flotation to remove alkaline earth metal carbonate mineral impurity from the low-silica intermediate flotation concentrate is a "carbonate" flotation.
Claim 7
Dependent Claim 36 words
The method of claim 2 further comprising the step of subjecting the "double float" concentrate of step (J) to a flotation to remove akaline earth metal carbonate mineral impurities therefrom and to form a phosphate concentrate.
Claim 8
Dependent Claim 52 words
The method of claim 6 wherein the gravity separation is a heavy media separation employing an aqueous suspension of magnetite or ferrosilicon having a specific gravity of from about 1.8 to about 2.5 as the heavy medium, and wherein the flotations to remove alkaline earth metal carbonate mineral impurity are "carbonate" flotations.
Claim 9
Dependent Claim 65 words
The method of claim 1 wherein the alkaline earth metal carbonate mineral impurity is dolomite; the deslimed ore fraction is split at about 16 mesh in step (b); the middle ore fraction is split at about 28 mesh in step (d); and the flotation feed produced in step (f) is comminuted, sized and deslimed to a deslimed particle size of less than about 28 mesh.
Claim 10
Dependent Claim 52 words
The method of claim 8 wherein the gravity separation is a heavy media separation employing an aqueous suspension of magnetite or ferrosilicon having a specific gravity of from about 1.8 to about 2.5 as the heavy medium, and the flotation to remove alkaline earth metal carbonate mineral impurity is a "carbonate" flotation.
Claim 11
Dependent Claim 14 words
The method of claim 1 wherein the alkaline earth metal carbonate impurity is calcite.
Claim 12
Dependent Claim 47 words
The method of claim 1 wherein the gravity separation is a heavy media separation employing an aqueous suspension of magnetite or ferrosilicon having a specific gravity of from about 1.8 to about 2.5 as the heavy medium, and the flotation of step (h) is a "carbonate" flotation.
Claim 13
Independent Claim 250 words
A method for beneficiating a phosphate ore matrix containing apatite, siliceous gangue, and an alkaline earth metal carbonate mineral impurity, comprising the steps of (a) washing and sizing the ore matrix to substantially deslime the matrix and to remove particles larger than from about 2 mesh to about 5 mesh thereby forming a deslimed ore matrix; (b) splitting the deslimed ore matrix at about 12 to about 20 mesh to form a pebble fraction having a particle size greater than about 12 to about 20 mesh and a middle ore fraction having a particle size less than about 12 to about 20 mesh; (c) subjecting the pebble fraction to a gravity separation wherein a portion of the less dense alkaline earth metal carbonate mineral impurity is separated from the apatite, thereby producing a low carbonate fraction; (d) splitting the middle ore fraction at about 24 mesh to about 32 mesh to form a coarse fraction having a particle size greater than about 24 mesh to about 32 mesh and a fine fraction having a particle size smaller than about 24 mesh to about 32 mesh; (e) combining the coarse fraction with the pebble fraction to enter the gravity separation of step (c); (f) comminuting, sizing and desliming the low-carbonate fraction to a deslimed particle size of less tha about 24 to about 32 mesh,thereby forming a flotation feed; (g) subjecting the flotation feed to a flotation to remove alkaline earth metal carbonate impurity therefrom and to form a phosphate concentrate.
Claim 14
Independent Claim 250 words
A method for beneficiating a phosphate ore matrix containing apatite, siliceous gangue, and an alkaline earth metal carbonate mineral impurity, comprising the steps of (a) washing and sizing the ore matrix to substantially deslime the matrix and to remove particles larger than from about 2 mesh to about 5 mesh thereby forming a deslimed ore matrix; (b) splitting the deslimed ore matrix at about 12 to about 20 mesh to form a pebble fraction having a particle size greater than about 12 to about 20 mesh and a middle ore fraction having a particle size less than about 12 to about 20 mesh; (c) subjecting the pebble fraction to a gravity separation wherein a portion of the less dense alkaline earth metal carbonate mineral impurity is separated from the apatite, thereby producing a low carbonate fraction; (d) splitting the middle ore fraction at about 24 mesh to about 32 mesh to form a coarse fraction having a particle size greater than about 24 mesh to about 32 mesh and a fine fraction having a particle size smaller than about 24 mesh to about 32 mesh; (e) combining the coarse fraction with the pebble fraction to enter the gravity separation of step (c); (f) comminuting, sizing and desliming the low-carbonate fraction to a deslimed particle size of less tha about 24 to about 32 mesh,thereby forming a flotation feed; (g) subjecting the flotation feed to a flotation to remove alkaline earth metal carbonate impurity therefrom and to form a phosphate concentrate.
Claim 15
Dependent Claim 40 words
The method of claim 12 further comprising the steps of subjecting the flotation feed from step (f) to a conventional amine flotation to form an intermediate flotation concentrate, and subjecting the intermediate flotation concentrate to the flotation of step (g).
Claim 16
Dependent Claim 52 words
The method of claim 13 wherein the gravity separation is a heavy media separation employing an aqueous suspension of magnetite or ferrosilicon having a specific gravity of from about 1.8 to about 2.5 as the heavy medium, and the flotation to remove alkaline earth metal carbonate mineral impurity is a "carbonate" flotation.
Claim 17
Dependent Claim 47 words
The method of claim 12 wherein the gravity separation is a heavy media separation employing an aqueous suspension of magnetite or ferrosilicon having a specific gravity of from about 1.8 to about 2.5 as the heavy medium, and the flotation of step (g) is a "carbonate" flotation.
Claim 18
Independent Claim 249 words
A method for beneficiating a phosphate ore matrix containing apatite, siliceous gangue, and an alkaline earth metal carbonate mineral impurity, comprising the steps of (a) washing and sizing the ore matrix to substantially deslime the matrix and to remove particles larger than from about 2 mesh to about 5 mesh, thereby forming a deslimed ore matrix; (b) splitting the deslimed ore matrix at about 12 to about 20 mesh to form a pebble fraction having a particle size greater than about 12 to about 20 mesh and a middle ore fraction having a particle size less than about 12 to about 20 mesh; (c) subjecting the pebble fraction to a gravity separation wherein a portion of the less dense alkaline earth metal carbonate mineral impurity is separated from the apatite, thereby producing a low-carbonate fraction; (d) splitting the middle ore fraction at about 24 mesh to about 32 mesh to form a coarse fraction having a particle size greater than about 24 mesh to about 32 mesh and a fine fraction having a particle size smaller than about 24 mesh to about 32 mesh; (e) combining the coarse fraction with the low-carbonate fraction from the gravity separation of step (c); (f) comminuting, sizing and desliming the low-carbonate fraction to a deslimed particle size of less than about 24 to about 32 mesh, thereby forming a flotation feed; (g) subjecting the flotation feed to a flotation to remove alkaline earth metal carbonate mineral impurity and to form a phosphate concentrate.
Claim 19
Independent Claim 249 words
A method for beneficiating a phosphate ore matrix containing apatite, siliceous gangue, and an alkaline earth metal carbonate mineral impurity, comprising the steps of (a) washing and sizing the ore matrix to substantially deslime the matrix and to remove particles larger than from about 2 mesh to about 5 mesh, thereby forming a deslimed ore matrix; (b) splitting the deslimed ore matrix at about 12 to about 20 mesh to form a pebble fraction having a particle size greater than about 12 to about 20 mesh and a middle ore fraction having a particle size less than about 12 to about 20 mesh; (c) subjecting the pebble fraction to a gravity separation wherein a portion of the less dense alkaline earth metal carbonate mineral impurity is separated from the apatite, thereby producing a low-carbonate fraction; (d) splitting the middle ore fraction at about 24 mesh to about 32 mesh to form a coarse fraction having a particle size greater than about 24 mesh to about 32 mesh and a fine fraction having a particle size smaller than about 24 mesh to about 32 mesh; (e) combining the coarse fraction with the low-carbonate fraction from the gravity separation of step (c); (f) comminuting, sizing and desliming the low-carbonate fraction to a deslimed particle size of less than about 24 to about 32 mesh, thereby forming a flotation feed; (g) subjecting the flotation feed to a flotation to remove alkaline earth metal carbonate mineral impurity and to form a phosphate concentrate.
Claim 20
Dependent Claim 39 words
The method of claim 16 furthercomprising the steps of subjecting the flotation feed from step (f) to a conventional amine flotation to form an intermediate flotation concentrate, and subjecting the intermediate flotation concentrate to the flotation of step (g).
Claim 21
Dependent Claim 52 words
The method of claim 17 wherein the gravity separation is a heavy media separation employing an aqueous suspension of magnetite or ferrosilicon having a specific gravity of from about 1.8 to about 2.5 as the heavy medium, and the flotation to remove alkaline earth metal carbonate mineral impurity is a "carbonate" flotation.
Claim 22
Dependent Claim 40 words
The method of claim 16 further comprising the steps of subjecting the flotation feed from step (f) to a "double float" flotation to form an intermediate flotation concentrate and subjecting the intermediate flotation concentrate to the flotation of step (g).
Claim 23
Dependent Claim 52 words
The method of claim 19 wherein the gravity separation is a heavy media separation employing the aqueous suspension of magnetite or ferrosilicon having a specific gravity of from about 1.8 to about 2.5 as the heavy medium, and the flotation to remove alkaline earth metal carbonate mineral impurity is a "carbonate" flotation.
Claim 24
Dependent Claim 47 words
The method of claim 16 wherein the gravity separation is a heavy media separation employing an aqueous suspension of magnetite or ferrosilicon having a specific gravity of from about 1.8 to about 2.5 as the heavy medium, and the flotation of step (g) is a "carbonate" flotation.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1983-02-18 1983-08-20 1984-02-19 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1987-02-18 1987-08-20 1988-02-19 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1991-02-18 1991-08-20 1992-02-19 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag