Abstract
Abstract A mold for compression molding a plastic sheet from a viscous fluid provides more resistance to flow on the side of the sheet designed to be the underside than on the side of the sheet designed to be seen. This resistance to flow can be imparted by roughening the underside of the mold more than the top surface of the mold. The purpose for roughening one surface of the mold more than the other is so that the plastic mass will flow faster on the smoother side of the mold and carry bubbles to the rough side of the mold via a rolling action. By this method employing textured molds, the surface of automotive panels can be made having reduced surface imperfections.
Inventors
- 👤 Sigurdur I. Arnason
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-06 09:18
CPC Classifications
B; B29; B29C; B29C45/00; B29C45/17; B29C45/26; B29C45/37; B29C45/372; B29C33/00; B29C33/42; B29C33/424; B29C43/00; B29C43/02; B29C43/021; B29C65/00; B29C65/02; B29C65/34; B29C65/3472; B29C65/3476; B29K; B29K2105/00; B29K2105/0094; B29K2105/06; B29K2105/12; B29K2995/00; B29K2995/0037; B29K2995/0072; B29K2995/0073; B29L; B29L2031/00; B29L2031/30; B29L2031/3055
Claims Analysis
Total Claims: 2
Claim 1
Independent Claim
213 words
In a method for molding a thermosetting liquid having an initial viscosity of from 1,000 to 7×10 7 centipoises at room temperature filled with chopped glass fibers, into a cured sheet of material, which sheet in its final form has one visible surface and one surface which is less visible by: (a) placing the glass fiber filled thermosetting liquid between two heated dies; and (b) bringing the heated dies toward each other to cause the glass fiber filled thermosetting liquid to flow and fill the cavity formed by the dies and then set, wherein the improvement comprises: PG,15 a rougher surface on the die forming the less visible surface of the sheet than the surface of the die forming the more visible surface, wherein the rougher surface is rough enough to retard the flow of the compound more than the flow is retarded on the corresponding die surface forming the more visible surface, the rougher surface being rough enough to improve the paintability of the sheet produced but not so rough so as to impart a rough finish to the sheet after painting, the rougher surface being formed by the initial casting of the die surface or subsequent removal of material from the die surface by abrasion, etching, electric arc or plasma treatment.
Claim 2
Dependent Claim
213 words
In a method for molding a thermosetting liquid having an initial viscosity of from 1,000 to 7×10 7 centipoises at room temperature filled with chopped glass fibers, into a cured sheet of material, which sheet in its final form has one visible surface and one surface which is less visible by: (a) placing the glass fiber filled thermosetting liquid between two heated dies; and (b) bringing the heated dies toward each other to cause the glass fiber filled thermosetting liquid to flow and fill the cavity formed by the dies and then set, wherein the improvement comprises: PG,15 a rougher surface on the die forming the less visible surface of the sheet than the surface of the die forming the more visible surface, wherein the rougher surface is rough enough to retard the flow of the compound more than the flow is retarded on the corresponding die surface forming the more visible surface, the rougher surface being rough enough to improve the paintability of the sheet produced but not so rough so as to impart a rough finish to the sheet after painting, the rougher surface being formed by the initial casting of the die surface or subsequent removal of material from the die surface by abrasion, etching, electric arc or plasma treatment.
References Cited (Backward Citations)
DE1132319B
Cited
US3701748A
Cited
US3772241A
Cited
US3466259A
Cited
US3548030A
Cited
US3577478A
Cited
US3674893A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1983-02-04 | 1983-08-06 | 1984-02-05 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1987-02-04 | 1987-08-06 | 1988-02-05 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1991-02-04 | 1991-08-06 | 1992-02-05 | $7700.00 | Window Closed / Lapsed |