Patent US4184845A successfully refreshed from Google Patents.
US4184845A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Process for reduction of lignin color
Assignee: Westvaco Corp
•
Filing: 1975-04-18
•
Granted: 1980-01-22
•
Expires: 1995-04-18
Abstract
Abstract Disclosed herein is a two-step process for reducing the color of sulfonated alkali lignins and lignosulfonates by at least 80% which comprises, blocking at least 90% of the free-phenolic hydroxyl groups in the lignin and then subjecting the blocked lignins to oxidative action by air, molecular oxygen or hydrogen peroxide. The thus treated lignins are useful as dispersants for disperse dyes and vat dyes.
Inventors
- 👤 Stephen Y. Lin
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-26 08:47
CPC Classifications
C; C08; C08H; C08H6/00; C09; C09B; C09B67/00; C09B67/0071; C09B67/0084; C09B67/0085; C09B67/0086; D; D06; D06P; D06P1/00; D06P1/44; D06P1/46; D06P1/48; D06P1/50
Claims Analysis
Total Claims: 8
Claim 1
Independent Claim
87 words
A two-step process for producing light colored lignin which comprises; (a) reacting a sulfonated alkali lignin or lignosulfonate with from 1 to 20 moles of a member selected from the group consisting of alkylene oxides, halogen-containing alkyl alcohol, alkyl sulfonate and alkylene carbonate at a temperature from 0° C. to 200° C. until at least 90% of the phenolic hydroxyl groups are blocked and thereafter, (b) treating said blocked lignin with an oxidant until the original color of said lignin is made lighter by at least 80%.
Claim 2
Dependent Claim
87 words
A two-step process for producing light colored lignin which comprises; (a) reacting a sulfonated alkali lignin or lignosulfonate with from 1 to 20 moles of a member selected from the group consisting of alkylene oxides, halogen-containing alkyl alcohol, alkyl sulfonate and alkylene carbonate at a temperature from 0° C. to 200° C. until at least 90% of the phenolic hydroxyl groups are blocked and thereafter, (b) treating said blocked lignin with an oxidant until the original color of said lignin is made lighter by at least 80%.
Claim 3
Dependent Claim
25 words
The process of claim 1 wherein said lignin is a member of the group consisting of sulfonated kraft lignin, sulfonated soda lignin and sulfite lignin.
Claim 4
Dependent Claim
23 words
The process of claim 1 wherein said blocking agent is a member of the group consisting of propylene oxide, dimethyl sulfate and chloroethanol.
Claim 5
Dependent Claim
20 words
The process of claim 1 wherein said oxidant is a member of the group consisting of air and molecular oxygen.
Claim 6
Dependent Claim
34 words
The process of claim 4 wherein said treating is carried out at a temperature from 50° C. to 150° C. at gas pressure of 50 to 200 p.s.i. for 5 minutes to 2 hours.
Claim 7
Dependent Claim
36 words
The process of claim 1 wherein said oxidant is hydrogen peroxide in amounts of 1 to 6 moles per 1,000 grams of blocked lignin and oxidizing is carried out at a pH from 7 to 11.
Claim 8
Dependent Claim
31 words
A dyestuff composition comprising a disperse or vat dye cake and from 1% to 75% by weight of said dye cake is the product produced by the process of claim 1.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1983-01-21 | 1983-07-23 | 1984-01-22 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1987-01-21 | 1987-07-23 | 1988-01-22 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1991-01-21 | 1991-07-23 | 1992-01-22 | $7700.00 | Window Closed / Lapsed |