Abstract

Abstract Battery comprising a container housing a plurality of sealed cells employing an oxyhalide-, halide- and/or liquid sulfur dioxide-containing nonaqueous electrolyte, and a porous shock absorbing material impregnated with an immobilizing agent which will react with and neutralize any oxyhalide, halide, liquid sulfur dioxide or their reaction products that escape from the cells.

Inventors

  • 👤 Lewis F. Urry

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-31 07:41
CPC Classifications
H; H01; H01M; H01M6/00; H01M6/14; H01M50/00; H01M50/20; H01M50/204; H01M50/207; H01M50/213; H01M50/289; H01M50/293; H01M10/00; H01M10/42; H01M10/4228; Y; Y02; Y02E; Y02E60/00; Y02E60/10

Claims Analysis

Total Claims: 14
Claim 1
Independent Claim 177 words
A battery comprising an outer container having an opening at the top and a closed base member; disposed within said container at least two nonaqueous cells employing an electrolyte solution containing at least a liquid selected from the group consisting of an oxyhalide, a halide, liquid sulfur dioxide and mixtures thereof, said cells electrically connected in predetermined electrical relation so as to provide two electrode terminals for a cell assembly disposed at the open end of the container; a terminal board having two external terminals exposed on its surface and being secured to the open end of the container, each of said external terminals being electronically connected to one of the two electrode terminals of the cell assembly; and a resilient material disposed within the container between the cells and at least a portion of an inner wall of the container, said resilient material containing an immobilizing chemical agent that will substantially react with and neutralize any of the oxyhalide, halide, liquid sulfur dioxide, mixtures thereof or their reaction products that escape from any of the cells.
Claim 2
Dependent Claim 177 words
A battery comprising an outer container having an opening at the top and a closed base member; disposed within said container at least two nonaqueous cells employing an electrolyte solution containing at least a liquid selected from the group consisting of an oxyhalide, a halide, liquid sulfur dioxide and mixtures thereof, said cells electrically connected in predetermined electrical relation so as to provide two electrode terminals for a cell assembly disposed at the open end of the container; a terminal board having two external terminals exposed on its surface and being secured to the open end of the container, each of said external terminals being electronically connected to one of the two electrode terminals of the cell assembly; and a resilient material disposed within the container between the cells and at least a portion of an inner wall of the container, said resilient material containing an immobilizing chemical agent that will substantially react with and neutralize any of the oxyhalide, halide, liquid sulfur dioxide, mixtures thereof or their reaction products that escape from any of the cells.
Claim 3
Dependent Claim 29 words
The battery of claim 1 wherein the resilient material is selected from the group consisting of plastic foam, pressed fibers, felted fibers, woven fabric, corrugated board, and particulate materials.
Claim 4
Dependent Claim 60 words
The battery of claim 1 wherein two cells are positioned in the container and wherein a first portion of the resilient material is positioned between one of the inner walls of the container and one of the cells and a second portion of the resilient material is positioned between the opposite inner wall of the container and the other cell.
Claim 5
Dependent Claim 33 words
The battery of claim 1 wherein two cells are positioned in the container and wherein the resilient material is positioned between one of the inner walls of the container and the two cells.
Claim 6
Dependent Claim 59 words
The battery of claim 1 wherein two cells are positioned in the container and wherein a first portion of the resilient material is positioned between one of the walls of the container and the two cells and wherein a second portion of the resilient material is positioned between the opposite inner wall of the container and the two cells.
Claim 7
Dependent Claim 56 words
The battery of claim 1 wherein the cells employ an electrolyte containing sulfuryl chloride, thionyl chloride or mixtures thereof and wherein the resilient material is impregnated with an immobilizing agent selected from the group consisting of sodium acid carbonate, sodium carbonate, potassium carbonate, trisodium phosphate, magnesium oxide, magnesium carbonate, magnesium hydroxide, calcium hydroxide, and calcium carbonate.
Claim 8
Dependent Claim 13 words
The battery of claim 6 wherein the immobilizing agent is sodium acid carbonate.
Claim 9
Dependent Claim 60 words
The battery of claim 6 wherein two cells are positioned in the container and wherein a first portion of the resilient material is positioned between one of the inner walls of the container and one of the cells and a second portion of the resilient material is positioned between the opposite inner wall of the container and the other cell.
Claim 10
Dependent Claim 33 words
The battery of claim 6 wherein two cells are position in the container and wherein the resilient material is positioned between one of the inner walls of the container and the two cells.
Claim 11
Dependent Claim 59 words
The battery of claim 6 wherein two cells are positioned in the container and wherein a first portion of the resilient material is positioned between one of the walls of the container and the two cells and wherein a second portion of the resilient material is positioned between the opposite inner wall of the container and the two cells.
Claim 12
Dependent Claim 20 words
The battery of claim 6 wherein the resilient material is polyurethane foam and the immobilizing agent is sodium acid carbonate.
Claim 13
Dependent Claim 19 words
The battery of claim 1 wherein a particulate material is added to substantially fill any voids within the container.
Claim 14
Dependent Claim 19 words
The battery of claim 1 wherein a foamable material is added to substantially fill any voids within the container.

References Cited (Backward Citations)

US2542934A Cited
US3082285A Cited
US3542602A Cited
US3663721A Cited
US3736190A Cited
US3880673A Cited
US4087595A Cited
US3929507A Cited
US3993501A Cited
US4032696A Cited
US4048389A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1983-01-14 1983-07-16 1984-01-15 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1987-01-14 1987-07-16 1988-01-15 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1991-01-14 1991-07-16 1992-01-15 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag