High severity reforming

Assignee: Cosden Technology Inc
•
Filing: 1977-11-03
•
Granted: 1979-11-13
•
Expires: 1997-11-03
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Disclosed is a process for the production of highly aromatic reformates in high yield from a naphtha feed fraction by high-severity catalytic reforming using a reforming catalyst which includes a hydrocracking promotor metal. The process comprises reforming the stock under conditions of high severity in a plurality of sequentially arranged reaction zones in which the concentration of the hydrocracking promotor metal of the reforming catalyst is adjusted to provide a minimal hydrocracking activity relative to the other reforming reactions to the catalyst in the first reaction zones, and an enhanced hydrocracking activity to the catalyst in the last reaction zones. The reformates produced according to this process are particularly useful in the blending of high aromatic content gasoline and/or in the production of high purity aromatic hydrocarbons.

Inventors

  • 👤 Warden W. Mayes

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 20:37
CPC Classifications
C; C10; C10G; C10G59/00; C10G59/02; Y; Y02; Y02P; Y02P20/00; Y02P20/50; Y02P20/582

Claims Analysis

Total Claims: 33
Claim 1
Independent Claim 110 words
A process for the production of highly aromatic reformates, suitable for use as blending stocks in the blending of high aromatic content gasoline or the preparation of high purity aromatics, from a naphtha feed fraction by high severity catalytic reforming, using a reforming catalyst which includes a hydrocracking promotor metal, comprising reforming said naphtha feed under reforming conditions of high severity in a plurality of sequentially arranged reaction zones in which the concentration of the promotor metal of the reforming catalyst is adjusted to provide an enhanced hydrocracking activity to the catalyst in the last reaction zones, and a minimal hydrocracking activity to the catalyst in the first reaction zones.
Claim 2
Dependent Claim 110 words
A process for the production of highly aromatic reformates, suitable for use as blending stocks in the blending of high aromatic content gasoline or the preparation of high purity aromatics, from a naphtha feed fraction by high severity catalytic reforming, using a reforming catalyst which includes a hydrocracking promotor metal, comprising reforming said naphtha feed under reforming conditions of high severity in a plurality of sequentially arranged reaction zones in which the concentration of the promotor metal of the reforming catalyst is adjusted to provide an enhanced hydrocracking activity to the catalyst in the last reaction zones, and a minimal hydrocracking activity to the catalyst in the first reaction zones.
Claim 3
Dependent Claim 32 words
The process of claim 1, wherein said promotor metal is selected from the group consisting of scandium, yttrium, titanium, zirconium, hafnium, thorium, germanium, manganese, iridium, combinations thereof and compounds containing said metals.
Claim 4
Dependent Claim 11 words
The process of claim 2, wherein said promotor metal is iridium.
Claim 5
Dependent Claim 16 words
The process of claim 1, wherein said stock is reformed in at least three reaction zones.
Claim 6
Dependent Claim 14 words
The process of claim 4 wherein said stock is reformed in four reaction zones.
Claim 7
Dependent Claim 28 words
The process of claim 1, when the concentration of the metal promotor of said catalyst is progressively increased from the first to the last of said reaction zones.
Claim 8
Dependent Claim 26 words
The process of claim 6, wherein the concentration of the metal promotor of said catalyst is increased progressively from about 0.02 to about 0.20 weight percent.
Claim 9
Dependent Claim 32 words
The process of claim 1, wherein the concentration of the metal promotor of said catalyst is maintained at a greater concentration in the last reaction zone than in the preceding reaction zones.
Claim 10
Dependent Claim 35 words
The process of claim 8, wherein the concentration of the metal promotor of said catalyst comprises about 0.20 weight percent in the last reaction zone and about 0.02 weight percent in the remaining reaction zones.
Claim 11
Dependent Claim 21 words
The process of claim 1, wherein said naphtha feedstock is a C 6 to 400° F. ASTM distillation endpoint naphtha fraction.
Claim 12
Dependent Claim 31 words
The process of claim 1, wherein said naphtha feedstock is a C 6 to C 8 naphtha fraction having an ASTM distillation endpoint of about 300° F. to about 360° F.
Claim 13
Dependent Claim 35 words
The process of claim 1, wherein said reforming conditions are of sufficient severity to produce a reformate having a minimum concentration of non-aromatic material, and/or a research clear octane value of about at least 100.
Claim 14
Dependent Claim 63 words
The process of claim 12, wherein said reforming conditions comprise a temperature of from about 800° F. to about 1100° F., a pressure of from about 50 psig to about 1000 psig, a liquid hourly space velocity of from about 0.1 to about 20.0 and a recycle hydrogen rate of from about 1.0 to 20 moles of hydrogen per mole of hydrocarbon feed.
Claim 15
Dependent Claim 40 words
The process of claim 13, wherein the temperature is maintained within the range of from about 950° to about 975° F. in the last reaction zones, and from about 850° F. to about 900° F. in the first reaction zones.
Claim 16
Dependent Claim 136 words
A process for the production of high-purity aromatic hydrocarbons selected from the group consisting of C 7 , C 8 , or C 7 and C 8 aromatic hydrocarbons in a high yield from a naphtha feed fraction by high-severity catalytic reforming, utilizing a reforming catalyst which includes a hydrocracking promotor metal, and fractional distillation, comprising the steps of: a. reforming said naphtha feed under reforming conditions of high severity in a plurality of sequentially arranged reaction zones in which the concentration of the promotor metal of the reforming catalyst is adjusted to provide an enhanced hydrocracking activity to the catalyst in the last reaction zones, and a minimal hydrocracking activity to the catalyst in the first reaction zones; and b. fractionally distilling the resultant reformate to directly recover said aromatic hydrocarbons in highly pure form.
Claim 17
Dependent Claim 136 words
A process for the production of high-purity aromatic hydrocarbons selected from the group consisting of C 7 , C 8 , or C 7 and C 8 aromatic hydrocarbons in a high yield from a naphtha feed fraction by high-severity catalytic reforming, utilizing a reforming catalyst which includes a hydrocracking promotor metal, and fractional distillation, comprising the steps of: a. reforming said naphtha feed under reforming conditions of high severity in a plurality of sequentially arranged reaction zones in which the concentration of the promotor metal of the reforming catalyst is adjusted to provide an enhanced hydrocracking activity to the catalyst in the last reaction zones, and a minimal hydrocracking activity to the catalyst in the first reaction zones; and b. fractionally distilling the resultant reformate to directly recover said aromatic hydrocarbons in highly pure form.
Claim 18
Dependent Claim 25 words
The process of claim 15, wherein said naphtha feed fraction is a C to C naphtha fraction having an ASTM distillation endpoint of 400° F.
Claim 19
Dependent Claim 29 words
The process of claim 15, wherein said naphtha feed fraction is a C to C naphtha fraction having an ASTM distillation endpoint of about 300° F. to 360° F.
Claim 20
Dependent Claim 20 words
The process of claim 15, wherein said aromatic hydrocarbons are selected from the group consisting of toluene, and mixed xylenes.
Claim 21
Dependent Claim 18 words
The process of claim 15, wherein said naphtha feed fraction is reformed in at least three reaction zones.
Claim 22
Dependent Claim 16 words
The process of claim 19, wherein said naphtha feed fraction is reformed in four reaction zones.
Claim 23
Dependent Claim 28 words
The process of claim 15, wherein the concentration of the promotor metal of said catalyst is progressively increased from the first to the last of said reaction zones.
Claim 24
Dependent Claim 26 words
The process of claim 21, wherein the concentration of the promotor metal of said catalyst is progressively increased from about 0.02 to about 0.20 weight percent.
Claim 25
Dependent Claim 22 words
The process of claim 15, wherein the concentration of the promotor metal of said catalyst is increased in the last reaction zone.
Claim 26
Dependent Claim 35 words
The process of claim 23, wherein the concentration of the promotor metal of said catalyst comprises about 0.20 weight percent in the last reaction zone and about 0.02 weight percent in the remaining reaction zones.
Claim 27
Dependent Claim 35 words
The process of claim 15, wherein said reforming conditions are of sufficient severity to produce a reformate having a minimum concentration of non-aromatic material, and/or a research clear octane value of at least about 100.
Claim 28
Dependent Claim 63 words
The process of claim 25, wherein said reforming conditions comprise a temperature of from about 800° F. to about 1100° F., a pressure of from about 50 psig to about 1000 psig, a liquid hourly space velocity of from about 0.1 to about 20.0 and a recycle hydrogen rate of from about 1.0 to 20 moles of hydrogen per mole of naphtha feed.
Claim 29
Dependent Claim 40 words
The process of claim 26, wherein said temperature is maintained within the range of from about 950 to about 975° F. in the last reaction zones, and from about 850° F., to about 900° F. in the first reaction zones.
Claim 30
Dependent Claim 32 words
The process of claim 15, wherein said promotor metal is selected from the group consisting of scandium, yttrium, titanium, zirconium, hafnium, thorium, germanium, manganese, iridium, combinations thereof and compounds containing said metals.
Claim 31
Dependent Claim 11 words
The process of claim 27, wherein said promotor metal comprises iridium.
Claim 32
Dependent Claim 121 words
A process for the production of highly aromatic reformates, suitable for use as blending stocks in the blending of high aromatic content gasoline or the preparation of high purity aromatics, from a naphtha feed fraction by high severity catalytic reforming, using a reforming catalyst which includes a hydrocracking promotor metal, comprising reforming said naphtha feed under reforming conditions of high severity in a plurality of sequentially arranged reaction zones in which the concentration of the promotor metal of the reforming catalyst is progressively increased from the first to the last of said reaction zones to provide an enhanced hydrocracking activity to the catalyst in the last reaction zones, and a minimal hydrocracking activity to the catalyst in the first reaction zones.
Claim 33
Dependent Claim 121 words
A process for the production of highly aromatic reformates, suitable for use as blending stocks in the blending of high aromatic content gasoline or the preparation of high purity aromatics, from a naphtha feed fraction by high severity catalytic reforming, using a reforming catalyst which includes a hydrocracking promotor metal, comprising reforming said naphtha feed under reforming conditions of high severity in a plurality of sequentially arranged reaction zones in which the concentration of the promotor metal of the reforming catalyst is progressively increased from the first to the last of said reaction zones to provide an enhanced hydrocracking activity to the catalyst in the last reaction zones, and a minimal hydrocracking activity to the catalyst in the first reaction zones.

References Cited (Backward Citations)

US2848377A Cited
US2908629A Cited
US3499945A Cited
US3635815A Cited
US3871996A Cited
US3647679A Cited
US4000058A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1982-11-12 1983-05-14 1983-11-13 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1986-11-12 1987-05-14 1987-11-13 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1990-11-12 1991-05-14 1991-11-13 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag