Patent US4169005A successfully refreshed from Google Patents.
← Back to Patent Explorer
US4169005A Expired / Lapsed US ⏱️ 0.0 years remaining

Method for surfacing a wood panel with a plastic film

Assignee: US PLYWOOD Corp A CORP OF
•
Filing: 1977-09-01
•
Granted: 1979-09-25
•
Expires: 1997-09-01
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract In a process for surfacing a hardwood veneer with a plastic film, one surface of the hardwood veneer is first sanded to provide a smooth surface for prefinishing, followed by the application of a stain or toner to achieve the desired color and appearance of the panel. A first coat of adhesive is applied to the smooth surface of the panel and allowed to dry, followed by the application of a second coat of adhesive which is also subsequently dry. Next, the panel is heated to reactivate both coats of adhesive, and a clear plastic film is applied to the smooth surface of the hardwood veneer and laminated thereto. Next, an ultra-violet curable topcoat is applied to the plastic sheet and allowed to cure, thereby resulting in a surface that has excellent scratch, mar and burnish resistance.

Inventors

  • 👤 Ozzie Fogle
  • 👤 James Cooley

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-03 19:00
CPC Classifications
B; B29; B29C; B29C63/00; B29C63/02; B32; B32B; B32B37/00; B32B37/12; B29C63/48; B29C63/481; B29C66/00; B29C66/01; B29C66/05; B29C66/10; B29C66/11; B29C66/112; B29C66/1122; B29C66/40; B29C66/41; B29C66/45; B32B21/00; B32B21/04; B32B21/08; B32B21/14; B32B37/1207; B29C65/00; B29C65/48; B29C65/4805; B29C65/481; B29C65/482; B29C66/70; B29C66/71; B29K; B29K2711/00; B29K2711/14; B29K2995/00; B29K2995/0018; B29K2995/002; B29L; B29L2007/00; B29L2007/002; B32B2310/00; B32B2310/08; B32B2310/0806; B32B2310/0831

Claims Analysis

Total Claims: 17
Claim 1
Independent Claim 144 words
A method for surfacing a wood panel with a plastic film comprising the steps of: (A) sanding one surface of the wood panel to provide a smooth surface for prefinishing; (B) applying a stain or toner to said smooth surface of the panel to achieve the desired color and appearance; (C) applying a first coat of adhesive to the smooth surface of said panel; (D) drying said first coat of adhesive; (E) applying a second coat of adhesive to the smooth surface of said panel; (F) drying said second coat of adhesive; (G) heating said panel to reactivate said first and second coats of adhesives; (H) applying a clear plastic sheet to said smooth surface; (I) laminating said plastic sheet to the smooth surface of said panel; (J) applying an ultra-violet curable topcoat to the plastic sheet; and (K) curing said ultra-violet top coat.
Claim 2
Independent Claim 144 words
A method for surfacing a wood panel with a plastic film comprising the steps of: (A) sanding one surface of the wood panel to provide a smooth surface for prefinishing; (B) applying a stain or toner to said smooth surface of the panel to achieve the desired color and appearance; (C) applying a first coat of adhesive to the smooth surface of said panel; (D) drying said first coat of adhesive; (E) applying a second coat of adhesive to the smooth surface of said panel; (F) drying said second coat of adhesive; (G) heating said panel to reactivate said first and second coats of adhesives; (H) applying a clear plastic sheet to said smooth surface; (I) laminating said plastic sheet to the smooth surface of said panel; (J) applying an ultra-violet curable topcoat to the plastic sheet; and (K) curing said ultra-violet top coat.
Claim 3
Dependent Claim 25 words
A method for surfacing a wood panel with a plastic film as in claim 1 wherein said process is carried out in a continuous manner.
Claim 4
Dependent Claim 44 words
A method for surfacing a wood panel with a plastic film as in claim 1 wherein said wood panel is first formed by laminating a hardwood veneer substrate to a core material and thereafter the hardwood veneer substrate of the wood panel is sanded.
Claim 5
Dependent Claim 35 words
A method for surfacing a wood panel with a plastic film as in claim 1 wherein said stain or toner coat is applied to the smooth surface of the panel by a direct rollcoat application.
Claim 6
Dependent Claim 50 words
A method for surfacing a wood panel with a plastic film as in claim 1 wherein said stain or toner coat is a vinyl, acrylic, nitrocellulose, or alkyd base toned with either pigments or dyes, and with the percent solids of the materials in the range of 0.5 to 10%.
Claim 7
Dependent Claim 28 words
A method for surfacing a wood panel with a plastic film as in claim 1 wherein said first coat of adhesive is applied by a direct rollcoat process.
Claim 8
Dependent Claim 45 words
A method for surfacing a wood panel with a plastic film as in claim 1 wherein said first coat of adhesive and said second coat of adhesive are each applied at a depth of approximately 11/2 wet mils, having a 25 to 35% solids material.
Claim 9
Dependent Claim 50 words
A method for surfacing a wood panel with a plastic film as in claim 1 wherein the adhesive as used in said first and second coats has added thereto from 0.5-5% by weight of UV absorber such as 2,4-dihydroxybenzophenone, 2,2'-dihydroxy-4,4-dimethoxy-benzophenone, 2,2',4,4'-tetrahydroxybenzophenone, 2-hydroxy-4-methoxy-benzophenone-5-sulfonic acid, sodium 2,2'-dihydroxy-4,4-dimethoxy-5-sulfobenzophenone, ethyl-2-cyano-3,3-diphenyl acrylate, and 2-ethylhexyl-2-cyano-3,3-diphenyl acrylate.
Claim 10
Dependent Claim 35 words
A method for surfacing a wood panel with a plastic film as in claim 1 wherein said first coat of adhesive is dried at a temperature in the range of 250° F. to 350° F.
Claim 11
Dependent Claim 35 words
A method for surfacing a wood panel with a plastic film as in claim 1 wherein said second coat of adhesive is dried at a temperature in the range of 250° F. to 350° F.
Claim 12
Dependent Claim 38 words
A method for surfacing a wood panel with a plastic film as in claim 1 wherein said first and second coats of adhesive are dried in an oven at a conveying speed of approximately 100 feet per minute.
Claim 13
Dependent Claim 38 words
A method for surfacing a wood panel with a plastic film as in claim 1 wherein said plastic sheet is made of a clear poly-vinyl chloride film having a thickness in the range of 2 to 6 mils.
Claim 14
Dependent Claim 36 words
A method for surfacing a wood panel with a plastic film as in claim 1 wherein said plastic sheet is laminated to said wood panel by a rubber roll at a temperature of approximately 250° F.
Claim 15
Dependent Claim 29 words
A method for surfacing a wood panel with a plastic film as in claim 1 wherein the ultraviolet curable topcoat is applied at a thickness of approximately 2 mils.
Claim 16
Dependent Claim 35 words
A method for surfacing a wood panel with a plastic film as in claim 1 wherein said ultra violet curable top coat is a 100% solids polyacrylate resin with 10-20% silica pigments and 1-3% photoinitiator.
Claim 17
Dependent Claim 32 words
A method for surfacing a wood panel with a plastic film as in claim 1 wherein said ultraviolet curable topcoat is cured by passing the laminate under a series of ultraviolet lamps.

References Cited (Backward Citations)

US2632710A Cited
US3017287A Cited
US3287197A Cited
US3502533A Cited
US3644161A Cited
US3713935A Cited
US3867153A Cited
US4113894A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1982-09-24 1983-03-26 1983-09-25 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1986-09-24 1987-03-26 1987-09-25 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1990-09-24 1991-03-26 1991-09-25 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag