Liquid crystal cell with a glass solder seal

Assignee: Siemens AG
•
Filing: 1978-03-10
•
Granted: 1979-06-19
•
Expires: 1998-03-10
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A liquid crystal cell having a chamber for receiving a layer of liquid crystal material which chamber is defined by a pair of plate members joined together adjacent their edges by a substantially continuous glass solder seal characterized by the glass solder seal being provided in the form of one or more glass fibers which are interposed between the plates and fused to form the glass solder seal. To facilitate positioning the one or more glass solder fibers, positioning means are provided on one surface of one of the plates and may be protruberances which are formed either by crystallizing glass solder, or by laser bombardment of the one surface. To facilitate the obtaining of the desired spacing between the plates, each of the glass fibers may have a core which may be either hard glass or a metal such as gold which core is surrounded by a lower melting glass so that during fusion of the fiber, the core remains substantially unmelted. In another embodiment, the glass fibers contain a material, such as being impregnated with CuO, which will absorb infrared radiation so that during the method of forming the cell, the step of heating to fuse the fibers includes subjecting the fibers to infrared radiation after preheating the assembled plates and fibers.

Inventors

  • 👤 Werner Mueller
  • 👤 Christoph Rotter
  • 👤 Wolfgang Welsch

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-25 14:43
CPC Classifications
G; G02; G02F; G02F1/00; G02F1/01; G02F1/13; G02F1/133; G02F1/1333; G02F1/1339

Claims Analysis

Total Claims: 9
Claim 1
Independent Claim 205 words
A method for producing a liquid crystal cell having a chamber for receiving a layer of liquid crystal material, said chamber being defined by a pair of plate members joined together adjacent their edges by a substantially continuous means for hermetically sealing the plate members together in spaced relationship with the facing surfaces of the plate members being plane parallel and each of said facing surfaces having at least one portion provided with an electrically conducting coating, said means for sealing including a glass solder frame, said method comprising the steps of providing a pair of plate members, providing a glass solder frame on one of said pair of plate members by positioning at least one fiber consisting of a glass solder material free of any organic bonding agent in a predetermined position on a surface and adjacent the edges of said one plate member, placing the other of said pair of plate members with its surface engaging the glass solder frame of the glass solder fiber to form an assembly, and then subsequently heating the assembly to fuse the glass solder fiber to form a hermetic glass solder seal between the two plates to join the plates together to form the chamber defined thereby.
Claim 2
Independent Claim 205 words
A method for producing a liquid crystal cell having a chamber for receiving a layer of liquid crystal material, said chamber being defined by a pair of plate members joined together adjacent their edges by a substantially continuous means for hermetically sealing the plate members together in spaced relationship with the facing surfaces of the plate members being plane parallel and each of said facing surfaces having at least one portion provided with an electrically conducting coating, said means for sealing including a glass solder frame, said method comprising the steps of providing a pair of plate members, providing a glass solder frame on one of said pair of plate members by positioning at least one fiber consisting of a glass solder material free of any organic bonding agent in a predetermined position on a surface and adjacent the edges of said one plate member, placing the other of said pair of plate members with its surface engaging the glass solder frame of the glass solder fiber to form an assembly, and then subsequently heating the assembly to fuse the glass solder fiber to form a hermetic glass solder seal between the two plates to join the plates together to form the chamber defined thereby.
Claim 3
Dependent Claim 38 words
A method according to claim 1, wherein the step of positioning the glass fibers in said frame includes forming positioning means on the surface of said one plate member to fix the position of the glass fiber thereon.
Claim 4
Dependent Claim 29 words
A method according to claim 2, wherein the step of forming position means comprises subjecting the surface of said one plate member to laser bombardment to create protruberances thereon.
Claim 5
Dependent Claim 40 words
A method according to claim 2, wherein the step of forming positioning means comprises providing crystalizing glass solder at discrete places on said surface of said one plate member, heating the crystalizing glass solder to produce glass crystal protruberances thereon.
Claim 6
Dependent Claim 47 words
A method according to claim 1, wherein each of said glass fibers comprises a hard glass core surrounded by meltable glass so that during the step of heating, said core acts as means for providing a predetermined spacing between the surfaces of the pair of plate members.
Claim 7
Dependent Claim 47 words
A method according to claim 1, wherein each of said glass fibers comprises a metal core surrounded by a meltable glass so that during the step of heating, said metal core provides means for providing a predetermined spacing between the surfaces of the pair of plate members.
Claim 8
Dependent Claim 52 words
A process according to claim 1, wherein each of the glass fibers absorbs infrared radiation, and wherein the step of heating includes preheating the assembly to a given temperature and then subjecting the assembly to infrared radiation to cause fusion of each of the glass fibers to form the glass solder seal.
Claim 9
Dependent Claim 22 words
A process according to claim 7, wherein each of the glass fibers is impregnated with an infrared absorbent component such as CuO.

References Cited (Backward Citations)

US4050786A Cited
US3995941A Cited
US3862830A Cited
US3960534A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1982-06-18 1982-12-18 1983-06-19 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1986-06-18 1986-12-18 1987-06-19 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1990-06-18 1990-12-18 1991-06-19 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag