Claims Analysis
Total Claims: 14
Claim 1
Independent Claim
126 words
In a method of fortifying alkali metal chloride brine comprising the steps of contacting the brine with alkali metal chloride salt having heavy metal impurities therein whereby to fortify the brine, adding sodium carbonate and barium carbonate to the fortified brine whereby to precipitate calcium and sulfate ions therefrom, and separating the precipitate from the fortified alkaline brine whereby to obtain a fortified, purified, alkaline, brine the improvement comprising adding F++ ion to the brine prior to its fortification, adding acid to the alkaline brine after fortification whereby to lower the pH of the brine to from about 1.5 to 4.5, and thereafter adding OH - ion to the acidified brine to increase the pH thereof to about 7.0 whereby to flocculate heavy metal impurities thereform.
Claim 2
Dependent Claim
126 words
In a method of fortifying alkali metal chloride brine comprising the steps of contacting the brine with alkali metal chloride salt having heavy metal impurities therein whereby to fortify the brine, adding sodium carbonate and barium carbonate to the fortified brine whereby to precipitate calcium and sulfate ions therefrom, and separating the precipitate from the fortified alkaline brine whereby to obtain a fortified, purified, alkaline, brine the improvement comprising adding F++ ion to the brine prior to its fortification, adding acid to the alkaline brine after fortification whereby to lower the pH of the brine to from about 1.5 to 4.5, and thereafter adding OH - ion to the acidified brine to increase the pH thereof to about 7.0 whereby to flocculate heavy metal impurities thereform.
Claim 3
Dependent Claim
20 words
The method of claim 1 wherein said salt contains in excess of 1 part per million of heavy metal impurities.
Claim 4
Dependent Claim
21 words
The method of claim 2 wherein said fortified, purified brine contains less than 1 part per million of heavy metal impurities.
Claim 5
Dependent Claim
23 words
The method of claim 1 comprising adding from about 1 to about 10 grams of Fe ++ per gram of heavy metal impurity.
Claim 6
Dependent Claim
51 words
The method of claim 4 comprising adding Fe ++ to the brine prior to fortification, adding acid to the brine after fortification whereby to lower its pH to from about 1.5 to 4.5, and thereafter adding OH - ion to increase the pH thereof to from about 6 to about 8.
Claim 7
Dependent Claim
160 words
In a method of electrolyzing alkali metal chloride brine comprising the steps of feeding fortified brine to an electrolytic cell, passing an electrical current through the cell, withdrawing depleted brine, adding hydrochloric acid to the depleted brine whereby to dechlorinate the depleted brine, contacting the dechlorinated depleted brine with alkali metal chloride salt having heavy metal impurities therein whereby to refortify the brine, adding sodium carbonate and barium carbonate to the refortified brine whereby to precipitate calcium and sulfate ions therefrom, and separating the precipitate from the refortified brine whereby to obtain a refortified alkaline, purified brine, the improvement comprising adding Fe ++ ion to the dechlorinated depleted brine prior to its refortification, adding acid to the alkaline brine after refortification whereby to lower the pH of the brine to from about 1.5 to 4.5, and thereafter adding OH - ion to the acidified brine to increase the pH thereof to about 7.0 whereby to flocculate heavy metal impurities therefrom.
Claim 8
Dependent Claim
160 words
In a method of electrolyzing alkali metal chloride brine comprising the steps of feeding fortified brine to an electrolytic cell, passing an electrical current through the cell, withdrawing depleted brine, adding hydrochloric acid to the depleted brine whereby to dechlorinate the depleted brine, contacting the dechlorinated depleted brine with alkali metal chloride salt having heavy metal impurities therein whereby to refortify the brine, adding sodium carbonate and barium carbonate to the refortified brine whereby to precipitate calcium and sulfate ions therefrom, and separating the precipitate from the refortified brine whereby to obtain a refortified alkaline, purified brine, the improvement comprising adding Fe ++ ion to the dechlorinated depleted brine prior to its refortification, adding acid to the alkaline brine after refortification whereby to lower the pH of the brine to from about 1.5 to 4.5, and thereafter adding OH - ion to the acidified brine to increase the pH thereof to about 7.0 whereby to flocculate heavy metal impurities therefrom.
Claim 9
Dependent Claim
23 words
The method of claim 6 comprising adding from about 1 to about 10 grams of Fe ++ per gram of heavy metal impurity.
Claim 10
Dependent Claim
49 words
The method of claim 7 comprising adding Fe ++ to the depleted brine, adding acid to the brine after refortification whereby to lower its pH to from about 1.5 to 4.5, and thereafter adding OH - ion to increase the pH thereof to from about 6 to about 8.
Claim 11
Dependent Claim
20 words
The method of claim 6 wherein said salt contains in excess of 1 part per million of heavy metal impurities.
Claim 12
Dependent Claim
21 words
The method of claim 9 wherein said refortified, repurified brine contains less than 1 part per million of heavy metal impurities.
Claim 13
Dependent Claim
17 words
The method of claim 6 wherein the electrolytic cell is a flowing mercury amalgam cathode electrolytic cell.
Claim 14
Dependent Claim
14 words
The method of claim 6 wherein the electrolytic cell is a permionic membrane cell.