Abstract

Abstract Disclosed is a method of electrolyzing alkali metal chloride brine. The method comprises feeding fortified brine to an electrolytic cell, passing an electrical current through the cell, and withdrawing depleted brine from the cell. Hydrochloric acid is added to the depleted brine to dechlorinate it; and the depleted, dechlorinated brine is then contacted with solid salt to refortify the brine. The solid brine is a source of heavy metal impurities. Sodium carbonate and barium carbonate are added to the refortified brine in order to precipitate calcium and sulfate ions therefrom. The precipitate is then separated from the refortified brine in order to obtain a refortified, purified brine. According to the disclosed method, ferrous ion and sufficient hydroxyl ion are added to the dechlorinated, depleted brine prior to its refortification in order to maintain the pH thereof above about 7 during fortification. After refortification, the pH is adjusted to pH 7 by the addition of hydrochloric acid and heavy metal impurities, such as vanadium, are flocculated therefrom. According to an alternate method, the pH can be adjusted to pH 2 by the addition of HCl and then to pH 7 by the addition of NaOH.

Inventors

  • 👤 William W. Carlin

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-25 02:15
CPC Classifications
C; C25; C25B; C25B1/00; C25B1/01; C25B1/34; C01; C01D; C01D3/00; C01D3/14; C01D3/16; C25B15/00; C25B15/08; C25B15/085

Claims Analysis

Total Claims: 14
Claim 1
Independent Claim 126 words
In a method of fortifying alkali metal chloride brine comprising the steps of contacting the brine with alkali metal chloride salt having heavy metal impurities therein whereby to fortify the brine, adding sodium carbonate and barium carbonate to the fortified brine whereby to precipitate calcium and sulfate ions therefrom, and separating the precipitate from the fortified alkaline brine whereby to obtain a fortified, purified, alkaline, brine the improvement comprising adding F++ ion to the brine prior to its fortification, adding acid to the alkaline brine after fortification whereby to lower the pH of the brine to from about 1.5 to 4.5, and thereafter adding OH - ion to the acidified brine to increase the pH thereof to about 7.0 whereby to flocculate heavy metal impurities thereform.
Claim 2
Dependent Claim 126 words
In a method of fortifying alkali metal chloride brine comprising the steps of contacting the brine with alkali metal chloride salt having heavy metal impurities therein whereby to fortify the brine, adding sodium carbonate and barium carbonate to the fortified brine whereby to precipitate calcium and sulfate ions therefrom, and separating the precipitate from the fortified alkaline brine whereby to obtain a fortified, purified, alkaline, brine the improvement comprising adding F++ ion to the brine prior to its fortification, adding acid to the alkaline brine after fortification whereby to lower the pH of the brine to from about 1.5 to 4.5, and thereafter adding OH - ion to the acidified brine to increase the pH thereof to about 7.0 whereby to flocculate heavy metal impurities thereform.
Claim 3
Dependent Claim 20 words
The method of claim 1 wherein said salt contains in excess of 1 part per million of heavy metal impurities.
Claim 4
Dependent Claim 21 words
The method of claim 2 wherein said fortified, purified brine contains less than 1 part per million of heavy metal impurities.
Claim 5
Dependent Claim 23 words
The method of claim 1 comprising adding from about 1 to about 10 grams of Fe ++ per gram of heavy metal impurity.
Claim 6
Dependent Claim 51 words
The method of claim 4 comprising adding Fe ++ to the brine prior to fortification, adding acid to the brine after fortification whereby to lower its pH to from about 1.5 to 4.5, and thereafter adding OH - ion to increase the pH thereof to from about 6 to about 8.
Claim 7
Dependent Claim 160 words
In a method of electrolyzing alkali metal chloride brine comprising the steps of feeding fortified brine to an electrolytic cell, passing an electrical current through the cell, withdrawing depleted brine, adding hydrochloric acid to the depleted brine whereby to dechlorinate the depleted brine, contacting the dechlorinated depleted brine with alkali metal chloride salt having heavy metal impurities therein whereby to refortify the brine, adding sodium carbonate and barium carbonate to the refortified brine whereby to precipitate calcium and sulfate ions therefrom, and separating the precipitate from the refortified brine whereby to obtain a refortified alkaline, purified brine, the improvement comprising adding Fe ++ ion to the dechlorinated depleted brine prior to its refortification, adding acid to the alkaline brine after refortification whereby to lower the pH of the brine to from about 1.5 to 4.5, and thereafter adding OH - ion to the acidified brine to increase the pH thereof to about 7.0 whereby to flocculate heavy metal impurities therefrom.
Claim 8
Dependent Claim 160 words
In a method of electrolyzing alkali metal chloride brine comprising the steps of feeding fortified brine to an electrolytic cell, passing an electrical current through the cell, withdrawing depleted brine, adding hydrochloric acid to the depleted brine whereby to dechlorinate the depleted brine, contacting the dechlorinated depleted brine with alkali metal chloride salt having heavy metal impurities therein whereby to refortify the brine, adding sodium carbonate and barium carbonate to the refortified brine whereby to precipitate calcium and sulfate ions therefrom, and separating the precipitate from the refortified brine whereby to obtain a refortified alkaline, purified brine, the improvement comprising adding Fe ++ ion to the dechlorinated depleted brine prior to its refortification, adding acid to the alkaline brine after refortification whereby to lower the pH of the brine to from about 1.5 to 4.5, and thereafter adding OH - ion to the acidified brine to increase the pH thereof to about 7.0 whereby to flocculate heavy metal impurities therefrom.
Claim 9
Dependent Claim 23 words
The method of claim 6 comprising adding from about 1 to about 10 grams of Fe ++ per gram of heavy metal impurity.
Claim 10
Dependent Claim 49 words
The method of claim 7 comprising adding Fe ++ to the depleted brine, adding acid to the brine after refortification whereby to lower its pH to from about 1.5 to 4.5, and thereafter adding OH - ion to increase the pH thereof to from about 6 to about 8.
Claim 11
Dependent Claim 20 words
The method of claim 6 wherein said salt contains in excess of 1 part per million of heavy metal impurities.
Claim 12
Dependent Claim 21 words
The method of claim 9 wherein said refortified, repurified brine contains less than 1 part per million of heavy metal impurities.
Claim 13
Dependent Claim 17 words
The method of claim 6 wherein the electrolytic cell is a flowing mercury amalgam cathode electrolytic cell.
Claim 14
Dependent Claim 14 words
The method of claim 6 wherein the electrolytic cell is a permionic membrane cell.

References Cited (Backward Citations)

US2114576A Cited
US2790707A Cited
US2982608A Cited
US3067133A Cited
US3752759A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1982-05-21 1982-11-20 1983-05-22 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1986-05-21 1986-11-20 1987-05-22 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1990-05-21 1990-11-20 1991-05-22 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag