Plasticized sulfur with improved stability

Assignee: Sunoco Inc R&M
•
Filing: 1978-04-03
•
Granted: 1979-05-22
•
Expires: 1998-04-03
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Sulfur is plasticized by the addition of 1,4,4a,5,8,8a-hexahydro-1,4,5,8-exo,endo-dimethanonaphthalene which is an adduct of norbornadiene and cyclopentadiene.

Inventors

  • 👤 Richard D. Cassar

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-01 14:57
CPC Classifications
C; C08; C08K; C08K5/00; C08K5/36; C01; C01B; C01B17/00; C01B17/02; C01B17/0243; C04; C04B; C04B28/00; C04B28/36

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 48 words
A process for plasticizing sulfur to obtain a flexible product which comprises adding with thorough mixing 1,4,4a,5,8,8a-hexahydro-1,4,5,8-exo-endo-dimethanonaphthalene to molten sulfur held at a temperature of at least about 150° C., said 1,4,4a,5,8,8a-exo-endo-dimethanonaphthalene being added in an amount of from about 5% to about 50% by weight of sulfur.
Claim 2
Dependent Claim 48 words
A process for plasticizing sulfur to obtain a flexible product which comprises adding with thorough mixing 1,4,4a,5,8,8a-hexahydro-1,4,5,8-exo-endo-dimethanonaphthalene to molten sulfur held at a temperature of at least about 150° C., said 1,4,4a,5,8,8a-exo-endo-dimethanonaphthalene being added in an amount of from about 5% to about 50% by weight of sulfur.
Claim 3
Dependent Claim 23 words
The process of claim 1 where the 1,4,4a,5,8,8a-hexahydro-1,4,5,8-exo,endo-dimethanonaphthalene is added in an amount from about 15% to about 50% by weight of sulfur.
Claim 4
Dependent Claim 38 words
A plasticized sulfur composition obtained by adding with thorough mixing 1,4,4a,5,8,8a-exo-endo-dimethanonaphthalene to molten sulfur at a temperature of at least about 150° C., in an amount of from about 5% to about 50% by weight of said sulfur.
Claim 5
Dependent Claim 38 words
A plasticized sulfur composition obtained by adding with thorough mixing 1,4,4a,5,8,8a-exo-endo-dimethanonaphthalene to molten sulfur at a temperature of at least about 150° C., in an amount of from about 5% to about 50% by weight of said sulfur.
Claim 6
Dependent Claim 23 words
The sulfur composition of claim 3 where the added 1,4,4a,5,8,8a-hexahydro-1,4,5,8-exo,endo-dimethanonaphthalene is in the amount of from about 15% to about 50% of sulfur.

References Cited (Backward Citations)

US3211709A Cited
US3498915A Cited
US3998897A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1982-05-21 1982-11-20 1983-05-22 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1986-05-21 1986-11-20 1987-05-22 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1990-05-21 1990-11-20 1991-05-22 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag