US4154866A Expired / Lapsed US ⏱️ 0.0 years remaining

Method of producing from wood tar a liquid smoke product for use in food processing, and product of said method

Assignee: Stange Co
•
Filing: 1976-08-24
•
Granted: 1979-05-15
•
Expires: 1996-08-24
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A liquid smoke product which contains no detectable amount of 3,4-benzopyrene (also known as benzo(a)pyrene) consists essentially of propylene glycol together with those components of the heavy, essentially water insoluble material that settle out of an aqueous condensation of wood smoke (hereinafter called "wood tar") which codistill at or below the boiling point of propylene glycol and most of which are soluble in propylene glycol. A method of making the above product by mixing about three parts by weight of wood tar with one part by weight propylene glycol to form a feed material, heating said feed material to about 280° F. to 290° F., reducing the pressure to about 100 mm. of mercury to cause codistillation of the desired components with the propylene glycol and thereby form a liquid fraction and a vapor fraction, entirely separating the vapor fraction from the liquid fraction, and condensing the vapor fraction which is then treated with a small percentage of activated carbon to assure that the amount of 3,4-benzopyrene is below 0.5 parts per billion, by weight.

Inventors

  • 👤 Balys Dainius
  • 👤 Charles Dame
  • 👤 James O'Hara

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-07 01:17
CPC Classifications
A; A23; A23L; A23L27/00; A23L27/20; A23L27/27

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 184 words
A method of treating wood tar to make a liquid smoke product which contains no detectable amount of 3,4-benzopyrene, said method comprising: (a) forming a feed material by mixing from a maximum of about twenty parts by weight to about three parts by weight of wood tar with one part by weight of propylene glycol; (b) heating said feed material to about 220° F. followed by heating said feed material to about 280° F., said feed material being agitated while being heated; (c) subjecting said feed material to a pressure less than about 2/3 atmosphere whereby said feed material is separated into a vapor fraction consisting of said propylene glycol and the components of said wood tar which codistill at or below the boiling point of the propylene glycol, and a liquid fraction; (d) separating the vapor fraction from the liquid fraction; (e) condensing said vapor fraction; (f) intimately contacting said condensed vapor fraction with pulverized activated carbon to assure that no detectable amount of 3,4-benzopyrene is present in said vapor fraction; and (g) filtering said activated carbon powder from said condensed vapor fraction.
Claim 2
Independent Claim 184 words
A method of treating wood tar to make a liquid smoke product which contains no detectable amount of 3,4-benzopyrene, said method comprising: (a) forming a feed material by mixing from a maximum of about twenty parts by weight to about three parts by weight of wood tar with one part by weight of propylene glycol; (b) heating said feed material to about 220° F. followed by heating said feed material to about 280° F., said feed material being agitated while being heated; (c) subjecting said feed material to a pressure less than about 2/3 atmosphere whereby said feed material is separated into a vapor fraction consisting of said propylene glycol and the components of said wood tar which codistill at or below the boiling point of the propylene glycol, and a liquid fraction; (d) separating the vapor fraction from the liquid fraction; (e) condensing said vapor fraction; (f) intimately contacting said condensed vapor fraction with pulverized activated carbon to assure that no detectable amount of 3,4-benzopyrene is present in said vapor fraction; and (g) filtering said activated carbon powder from said condensed vapor fraction.
Claim 3
Dependent Claim 41 words
The method of claim 1 in which the pulverized activated carbon has a particle size of 65-75% minus 325 mesh (U.S. Sieve Series, opening of 44 microns), and a total surface area (N 2 B.E.T. Method) of 1000-1100 m 2 /g.
Claim 4
Dependent Claim 29 words
The method of claim 1 in which the pulverized activated carbon has been pre-washed with acid to eliminate iron contaminants capable of reacting with components of the liquid smoke.
Claim 5
Dependent Claim 17 words
The method of claim 1 wherein said adsorbent is removed from said condensed vapor fraction by filtration.
Claim 6
Dependent Claim 12 words
The liquid smoke product produced according to the method of claim 1.

References Cited (Backward Citations)

US1753358A Cited
US2095857A Cited
US2400466A Cited
US3106473A Cited
US3445248A Cited
US3480446A Cited
US3663237A Cited
US3806609A Cited
US3873741A Cited
DE2507385A1 Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1982-05-14 1982-11-13 1983-05-15 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1986-05-14 1986-11-13 1987-05-15 $3760.00 Window Closed / Lapsed