Abstract

Abstract Liquid products from retorting oil shale are upgraded to a total liquid suited to pipeline transport and containing increased amounts of the premium products gasoline through distillate fuel by hydrotreating to convert sulfur, oxygen, nitrogen and metal constituents and cascading the hydrotreater effluent through a hydrocracking reactor containing a catalyst which is characterized by a crystalline zeolite having a silica/alumina ratio greater than 12 and a constraint index of 1 to 12, for example zeolite ZSM-5.

Inventors

  • 👤 Robert L. Gorring
  • 👤 Robert L. Smith

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-31 12:24
CPC Classifications
C; C10; C10G; C10G47/00; C10G47/02; C10G47/10; C10G47/12; C10G47/16; C10G1/00; C10G1/002; C10G65/00; C10G65/02; C10G65/12; F; F02; F02B; F02B3/00; F02B3/06

Claims Analysis

Total Claims: 9
Claim 1
Independent Claim 180 words
In a process for upgrading full range shale oil derived by retorting oil shale which process is conducted by contacting said full range shale oil in the presence of hydrogen with a composite dewaxing catalyst comprising a metal and a crystalline zeolite consisting essentially of one having a silica/alumina ratio greater than 12 and a constraint index of about 1 to 12, the improvement which comprises: contacting said full range shale oil in admixture with hydrogen with a hydrotreating catalyst at hydrotreating conditions to convert organic compounds of sulfur, nitrogen, oxygen and metal and passing substantially the entire effluent of such hydrotreating in cascade fashion into contact with said dewaxing catalyst at conversion conditions of temperature, pressure, space velocity and hydrogen concentration of a severity to hydrodewax the shale oil while simultaneously converting at least 50% of the shale oil boiling above about 750° F. to reaction products boiling below 750° F.; said severity including a temperature of 750° to 1000° F. and space velocity of 0.25 to 1 volumes of said shale oil per volume of catalyst per hour.
Claim 2
Dependent Claim 180 words
In a process for upgrading full range shale oil derived by retorting oil shale which process is conducted by contacting said full range shale oil in the presence of hydrogen with a composite dewaxing catalyst comprising a metal and a crystalline zeolite consisting essentially of one having a silica/alumina ratio greater than 12 and a constraint index of about 1 to 12, the improvement which comprises: contacting said full range shale oil in admixture with hydrogen with a hydrotreating catalyst at hydrotreating conditions to convert organic compounds of sulfur, nitrogen, oxygen and metal and passing substantially the entire effluent of such hydrotreating in cascade fashion into contact with said dewaxing catalyst at conversion conditions of temperature, pressure, space velocity and hydrogen concentration of a severity to hydrodewax the shale oil while simultaneously converting at least 50% of the shale oil boiling above about 750° F. to reaction products boiling below 750° F.; said severity including a temperature of 750° to 1000° F. and space velocity of 0.25 to 1 volumes of said shale oil per volume of catalyst per hour.
Claim 3
Dependent Claim 15 words
A process according to claim 1 wherein the metal of said dewaxing catalyst is nickel.
Claim 4
Dependent Claim 15 words
A process according to claim 1 wherein the metal of said dewaxing catalyst is palladium.
Claim 5
Dependent Claim 17 words
A process according to claim 1 wherein said severity includes a pressure of 500 to 1500 psig.
Claim 6
Dependent Claim 25 words
A process according to claim 1 wherein said hydrogen is supplied at a rate of 5 to 6 moles per mole of said shale oil.
Claim 7
Dependent Claim 32 words
A process according to claim 1 wherein said severity is at a level to convert at least 70% of the shale oil boiling above 750° F. to products boiling below 750° F.
Claim 8
Dependent Claim 11 words
A process according to claim 6 wherein said metal is palladium.
Claim 9
Dependent Claim 17 words
A process according to claim 1 wherein said composite consists essentially of said metal and said zeolite.

References Cited (Backward Citations)

US3764520A Cited
US3272734A Cited
US3506568A Cited
US3755138A Cited
US3980550A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1982-05-07 1982-11-06 1983-05-08 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1986-05-07 1986-11-06 1987-05-08 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1990-05-07 1990-11-06 1991-05-08 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag