Patent US4152147A successfully refreshed from Google Patents.
← Back to Patent Explorer
US4152147A Expired / Lapsed US ⏱️ 0.0 years remaining

Beryllium-containing iron-boron glassy magnetic alloys

Assignee: Honeywell International Inc
•
Filing: 1978-04-10
•
Granted: 1979-05-01
•
Expires: 1998-04-10
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract {PG,1 Introduction of beryllium into iron-boron base glassy alloys improves the thermal stability while substantially retaining the saturation moment of the base alloy. The alloys of the invention consist essentially of about 10 to 18 atom percent boron, about 2 to 10 atom percent beryllium and about 72 to 80 atom percent iron plus incidental impurities.

Inventors

  • 👤 Ryusuke Hasegawa
  • 👤 Ranjan Ray
  • 👤 Lee E. Tanner

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-29 18:57
CPC Classifications
C; C22; C22C; C22C45/00; C22C45/02

Claims Analysis

Total Claims: 7
Claim 1
Independent Claim 35 words
A beryllium-substituted, iron-boron, primarily glassy magnetic alloy consisting essentially of about 10 to 18 atom percent boron, about 2 to 10 atom percent beryllium and about 72 to 80 atom percent iron plus incidental impurities.
Claim 2
Dependent Claim 35 words
A beryllium-substituted, iron-boron, primarily glassy magnetic alloy consisting essentially of about 10 to 18 atom percent boron, about 2 to 10 atom percent beryllium and about 72 to 80 atom percent iron plus incidental impurities.
Claim 3
Dependent Claim 18 words
The alloy of claim 1 in which the beryllium content ranges from about 2 to 6 atom percent.
Claim 4
Dependent Claim 15 words
The alloy of claim 2 in which the beryllium content is about 2 atom percent.
Claim 5
Dependent Claim 30 words
The alloy of claim 1 consisting essentially of about 18 atom percent boron, 2 to 10 atom percent beryllium and about 80 to 72 atom percent iron plus incidental impurities.
Claim 6
Dependent Claim 30 words
The alloy of claim 1 consisting essentially of about 2 to 10 atom percent beryllium, about 18 to 10 atom percent boron and about 80 percent iron plus incidental impurities.
Claim 7
Dependent Claim 9 words
The alloy of claim 1 which is substantially glassy.

References Cited (Backward Citations)

US3871836A Cited
US3856513A Cited
US3989517A Cited
US4036638A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1982-04-30 1982-10-30 1983-05-01 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1986-04-30 1986-10-30 1987-05-01 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1990-04-30 1990-10-30 1991-05-01 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.