← Back to Patent Explorer
US4150981A Expired / Lapsed US ⏱️ 0.0 years remaining

Glassy alloys containing cobalt, nickel and iron having near-zero magnetostriction and high saturation induction

Assignee: Honeywell International Inc
•
Filing: 1977-08-15
•
Granted: 1979-04-24
•
Expires: 1997-08-15
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Glassy alloys containing cobalt, nickel and iron and evidencing near-zero magnetostriction and high saturation induction are disclosed. The glassy alloys consist essentially of about 13 to 73 atom percent cobalt, about 5 to 50 atom percent nickel, about 2 to 17 atom percent iron, with the proviso that the total of cobalt, nickel and iron is about 80 atom percent, and the balance essentially boron plus incidental impurities. The magnetostriction of the glassy alloys ranges from about +3x10-6 to -3x10-6 and the saturation induction is at least about 8 kGauss.

Inventors

  • 👤 Robert C. O'Handley

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-27 23:27
CPC Classifications
C; C22; C22C; C22C45/00; C22C45/04; H; H01; H01F; H01F1/00; H01F1/01; H01F1/03; H01F1/12; H01F1/14; H01F1/147; H01F1/153; H10; H10N; H10N35/00; H10N35/80; H10N35/85

Claims Analysis

Total Claims: 7
Claim 1
Independent Claim 80 words
A magnetic alloy that is substantially glassy, consisting essentially of about 13 to 73 atom percent cobalt, about 5 to 50 atom percent nickel, about 2 to 17 atom percent iron, with the proviso that the total of cobalt, nickel and iron is about 80 atom percent, and the balance essentially boron plus incidental impurities, said alloy having a value of magnetostriction ranging from about +3×10 -6 to -3×10 -6 and a saturation induction of at least about 8 kGauss.
Claim 2
Dependent Claim 80 words
A magnetic alloy that is substantially glassy, consisting essentially of about 13 to 73 atom percent cobalt, about 5 to 50 atom percent nickel, about 2 to 17 atom percent iron, with the proviso that the total of cobalt, nickel and iron is about 80 atom percent, and the balance essentially boron plus incidental impurities, said alloy having a value of magnetostriction ranging from about +3×10 -6 to -3×10 -6 and a saturation induction of at least about 8 kGauss.
Claim 3
Dependent Claim 17 words
The magnetic alloy of claim 1 in which nickel ranges from about 10 to 40 atom percent.
Claim 4
Dependent Claim 21 words
The magnetic alloy of claim 1 which is bounded by the polygon a-b-c-d-e-f-a shown in FIG. 1 of the attached drawings.
Claim 5
Dependent Claim 27 words
The magnetic alloy of claim 3 in which the composition lies within about ±2 atom percent of the line g-h-i of FIG. 1 of the attached drawings.
Claim 6
Dependent Claim 23 words
The magnetic alloy of claim 4 in which the composition lies substantially on the line g-h-i of FIG. 1 of the attached drawings.
Claim 7
Dependent Claim 48 words
The magnetic alloy of claim 1 selected from the group consisting of Co 56 Ni 16 Fe 8 B 20 , Co 44 Ni 24 Fe 12 B 20 , Co 34 Ni 34 Fe 12 B 20 and Co 28 Ni 36 Fe 16 B 20 .

References Cited (Backward Citations)

US3856513A Cited
US4052201A Cited
US4067732A Cited
US4036638A Cited
US4038073A Cited
US4056411A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1982-04-23 1982-10-23 1983-04-24 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1986-04-23 1986-10-23 1987-04-24 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1990-04-23 1990-10-23 1991-04-24 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag