Method of making magnetic devices including amorphous alloys
Abstract
Abstract The disclosed magnetic devices, including a magnetically coupled conducting path, incorporate amorphous, low magnetostriction alloys of the general formula (Co a Fe b T c ) i X j , the "metallic" constituents thereof being within the parenthetical expression. T, in the formulation, is selected from among Ni, Cr, Mn, V, Ti, Mo, W, Nb, Zr, Pd, Pt, Cu, Ag and Au, X being at least one "glass former" selected from among P, Si, B, C, As, Ge, Al, Ga, In, Sb, Bi and Sn. The "metallic" constituents comprise from 70-90 atomic percent of the alloy with cobalt being present in an amount of at least 70 atomic percent of the "metallic" constituents. The described material is prepared by rapid cooling from the liquid, directly to the shape needed for fabrication of the device (e.g., tape to be wound to form an inductor core). When the amorphous material is fabricated to its finished geometry, raised to a temperature somewhat below its crystallization temperature and quenched in a high heat of vaporization liquid (e.g., water), the permeability is greatly improved. An exemplary alloy was shown to possess properties, in some respects, equivalent to those of Supermalloy, an alloy of much more complex manufacture.
Inventors
- 👤 Ho Sou Chen
- 👤 Ernst Michael Gyorgy
- 👤 Harry John Leamy
- 👤 Richard Curry Sherwood
Bibliographic Details
Claims Analysis
Total Claims: 3References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1980-10-31 | 1981-05-02 | 1981-11-01 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1984-10-31 | 1985-05-02 | 1985-11-01 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1988-10-31 | 1989-05-02 | 1989-11-01 | $7700.00 | Window Closed / Lapsed |