Wafer sawing technique
Assignee: General Electric Co
•
Filing: 1977-11-03
•
Granted: 1979-02-06
•
Expires: 1997-11-03
Abstract
Abstract A method for dividing a semiconductor wafer into pellets includes attaching the wafer to a vinyl membrane with a coupling material which adheres more tenaciously to the membrane than to the pellets and sawing completely through the wafer and at least partially through the coupling material to separate the wafer into discrete pellets. In accordance with a preferred method, the membrane is at least slightly cut by the saw to insure complete division of the wafer. The pellets are readily removed from the coated membrane without any residues remaining thereon from the coupling material. A resinous vinyl coupling material is preferred.
Inventors
- 👤 Francis C. Gantley
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-25 12:36
CPC Classifications
H; H10; H10P; H10P72/00; H10P72/70; H10P72/74; H10P72/7402; B; B28; B28D; B28D1/00; B28D1/003; B28D5/00; B28D5/0058; B28D5/02; B28D5/022; H10P52/00; H10P72/7416; Y; Y10; Y10T; Y10T156/00; Y10T156/10; Y10T156/1052; Y10T156/1082; Y10T29/00; Y10T29/49; Y10T29/49789; Y10T29/4981; Y10T29/49812; Y10T83/00; Y10T83/04; Y10T83/0405
Claims Analysis
Total Claims: 21
Claim 1
Independent Claim
62 words
A method for dividing a semiconductor wafer into pellets comprising: providing a flexible membrane; coating a surface of said wafer with a layer of coupling material which adheres more tenaciously to said membrane than to said wafer; bonding said wafer to said membrane; and dividing said wafer into pellets by sawing completely through said wafer and at least partially through said layer.
Claim 2
Independent Claim
62 words
A method for dividing a semiconductor wafer into pellets comprising: providing a flexible membrane; coating a surface of said wafer with a layer of coupling material which adheres more tenaciously to said membrane than to said wafer; bonding said wafer to said membrane; and dividing said wafer into pellets by sawing completely through said wafer and at least partially through said layer.
Claim 3
Dependent Claim
25 words
The method of claim 1 further comprising removing said pellets from said membrane to a storage medium while maintaining the relative orientation of said pellets.
Claim 4
Dependent Claim
26 words
The method of claim 1 wherein said coating step comprises applying said coupling material in a thin layer and at least partially curing said coupling material.
Claim 5
Dependent Claim
40 words
The method of claim 3 wherein said applying and curing comprises applying said coupling material in liquid form and spinning said wafer to distribute said coupling material in a thin layer and to at least partially cure said coupling material.
Claim 6
Dependent Claim
14 words
The method of claim 1 wherein said coupling material is a resinous vinyl material.
Claim 7
Dependent Claim
12 words
The method of claim 1 wherein said membrane is a vinyl membrane.
Claim 8
Dependent Claim
13 words
The method of claim 6 wherein said membrane is at least slightly stretchable.
Claim 9
Dependent Claim
14 words
The method of claim 7 wherein said coupling material is a vinyl coupling material.
Claim 10
Dependent Claim
29 words
The method of claim 8 wherein said coating step comprises applying said coupling material to said wafer in a thin layer and at least partially curing said coupling material.
Claim 11
Dependent Claim
40 words
The method of claim 9 wherein said applying and curing comprises applying said coupling material in liquid form and spinning said wafer to distribute said coupling material in a thin layer and to at least partially cure said coupling material.
Claim 12
Dependent Claim
37 words
The method of claim 10 wherein bonding said wafer to said membrane comprises placing said coated wafer and said membrane in face-to-face relationship and heating the interface therebetween so as to bond said wafer to said membrane.
Claim 13
Dependent Claim
18 words
The method of claim 11 wherein said heating comprises heating the surface of said membrane opposite said wafer.
Claim 14
Dependent Claim
15 words
The method of claim 12 wherein said heating comprises heating through a thin porous layer.
Claim 15
Dependent Claim
14 words
The method of claim 13 wherein said thin porous layer comprises a paper layer.
Claim 16
Dependent Claim
17 words
The method of claim 13 wherein said sawing comprises sawing completely through said layer of coupling material.
Claim 17
Dependent Claim
16 words
The method of claim 15 wherein said sawing comprises sawing at least partially through said membrane.
Claim 18
Dependent Claim
13 words
The method of claim 16 further comprising removing said pellets from said membrane.
Claim 19
Dependent Claim
19 words
The method of claim 17 wherein said removing comprises removing by lifting said pellets with a vacuum pick-up means.
Claim 20
Dependent Claim
13 words
The method of claim 18 further comprising placing said pellets in storage means.
Claim 21
Dependent Claim
25 words
The method of claim 19 wherein said placing includes maintaining the same relative orientation of said pellets in said storage means as on said wafer.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1982-02-05 | 1982-08-07 | 1983-02-06 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1986-02-05 | 1986-08-07 | 1987-02-06 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1990-02-05 | 1990-08-07 | 1991-02-06 | $7700.00 | Window Closed / Lapsed |