Abstract
Abstract A pipe section is mounted in a horizontal position and upper and lower halves of a spigot ring mold are clamped to the spigot end. The lower mold half is provided with a port for receiving a nozzle of a hardenable liquid resin supply hose and the upper mold half is provided with vents. Resin is forced into the mold under pressure until some comes out of the vents. After the resin is hardened, the mold is removed.
Inventors
- 👤 Franklin E. Davidson
- 👤 Lee E. Pearson
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-07 15:50
CPC Classifications
B; B29; B29C; B29C45/00; B29C45/14; B29C45/14598; Y; Y10; Y10S; Y10S425/00; Y10S425/044; Y10S425/812
Claims Analysis
Total Claims: 8
Claim 1
Independent Claim
276 words
A method of molding a resin spigot ring on an end portion of a section of glass fiber reinforced thermosetting resin pipe to provide a pair of spaced connected exterior raised ring portions defining an annular groove for later reception of an elastomeric annular gasket, the method comprising supporting the pipe section horizontally with the end portion free, applying a pair of elastomeric mold sealing rings to the pipe end portion in spaced relationship to each other and to the respective end face of the pipe, applying upper and lower mold halves to the pipe end portion in predetermined relationship to the respective end face of the pipe section to form a composite mold having a first pair of spaced internal annular grooves respectively adjacent opposite end faces thereof, a second pair of spaced internal annular grooves between the first pair, and an annular portion between the grooves of the second pair having an internal diameter smaller than the diameter of either of the grooves of the second pair but larger than the outside diameter of the pipe while locating the mold sealing rings respectively in the first pair of internal annular grooves of the mold, clamping the mold halves together, injecting hardenable liquid resin through an injection port in the lower mold half until resin overflows through vents in the upper mold half to fill the second pair of internal annular grooves of the mold and the space therebetween adjacent the pipe with the resin, letting the resin in the mold harden, unclamping and removing the upper and lower mold halves from the pipe section, and removing the mold sealing rings from the pipe section.
Claim 2
Independent Claim
276 words
A method of molding a resin spigot ring on an end portion of a section of glass fiber reinforced thermosetting resin pipe to provide a pair of spaced connected exterior raised ring portions defining an annular groove for later reception of an elastomeric annular gasket, the method comprising supporting the pipe section horizontally with the end portion free, applying a pair of elastomeric mold sealing rings to the pipe end portion in spaced relationship to each other and to the respective end face of the pipe, applying upper and lower mold halves to the pipe end portion in predetermined relationship to the respective end face of the pipe section to form a composite mold having a first pair of spaced internal annular grooves respectively adjacent opposite end faces thereof, a second pair of spaced internal annular grooves between the first pair, and an annular portion between the grooves of the second pair having an internal diameter smaller than the diameter of either of the grooves of the second pair but larger than the outside diameter of the pipe while locating the mold sealing rings respectively in the first pair of internal annular grooves of the mold, clamping the mold halves together, injecting hardenable liquid resin through an injection port in the lower mold half until resin overflows through vents in the upper mold half to fill the second pair of internal annular grooves of the mold and the space therebetween adjacent the pipe with the resin, letting the resin in the mold harden, unclamping and removing the upper and lower mold halves from the pipe section, and removing the mold sealing rings from the pipe section.
Claim 3
Dependent Claim
15 words
A pipe section having a spigot ring molded thereon by the method of claim 1.
Claim 4
Dependent Claim
250 words
For molding a resin spigot ring on an end portion of a section of glass fiber reinforced thermosetting resin pipe having a pair of spaced mold sealing rings thereon, to provide a pair of spaced connected exterior raised ring portions defining an annular groove for later reception of an elastomeric annular gasket after the mold sealing rings have been removed from the pipe section, a composite mold comprising upper and lower generally semicylindrical mold halves adapted to be clamped together around the pipe section over the mold sealing rings for the spigot ring molding operation and unclamped and removed from the pipe section after the spigot ring molding operation, the composite mold having a first pair of spaced internal annular grooves respectively adjacent opposite end faces thereof for respectively receiving the mold sealing rings, a second pair of spaced internal annular grooves between the first pair, and an annular portion between the grooves of the second pair having an internal diameter smaller than the diameter of either of the grooves of the second pair but larger than the outside diameter of the pipe, the second pair of internal annular grooves of the mold and the space therebetween adjacent the pipe being adapted to receive hardenable liquid resin, the lower mold half having a resin injection port communicating with the bottom of one of the second pair of internal annular grooves, and the upper mold half having vents at the top communicating respectively with the second pair of internal annular grooves.
Claim 5
Dependent Claim
250 words
For molding a resin spigot ring on an end portion of a section of glass fiber reinforced thermosetting resin pipe having a pair of spaced mold sealing rings thereon, to provide a pair of spaced connected exterior raised ring portions defining an annular groove for later reception of an elastomeric annular gasket after the mold sealing rings have been removed from the pipe section, a composite mold comprising upper and lower generally semicylindrical mold halves adapted to be clamped together around the pipe section over the mold sealing rings for the spigot ring molding operation and unclamped and removed from the pipe section after the spigot ring molding operation, the composite mold having a first pair of spaced internal annular grooves respectively adjacent opposite end faces thereof for respectively receiving the mold sealing rings, a second pair of spaced internal annular grooves between the first pair, and an annular portion between the grooves of the second pair having an internal diameter smaller than the diameter of either of the grooves of the second pair but larger than the outside diameter of the pipe, the second pair of internal annular grooves of the mold and the space therebetween adjacent the pipe being adapted to receive hardenable liquid resin, the lower mold half having a resin injection port communicating with the bottom of one of the second pair of internal annular grooves, and the upper mold half having vents at the top communicating respectively with the second pair of internal annular grooves.
Claim 6
Dependent Claim
23 words
A mold as claimed in claim 3 wherein the upper mold half has nipples at the vents for attachment of clear plastic tubing.
Claim 7
Dependent Claim
32 words
A mold as claimed in claim 3 wherein each of the mold halves has stop means engageable with an end face of a pipe section to locate the mold half longitudinally thereof.
Claim 8
Dependent Claim
26 words
A mold as claimed in claim 5 wherein the stop means is a plurality of stop plates bolted to an end face of the mold half.
References Cited (Backward Citations)
US483593A
Cited
GB190810751A
Cited
US1151615A
Cited
US2580668A
Cited
US2706498A
Cited
US2766484A
Cited
US3026575A
Cited
US2966317A
Cited
US3087201A
Cited
DE1198989B
Cited
US3777000A
Cited
US3863701A
Cited
US3741707A
Cited
US3888295A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1982-01-15 | 1982-07-17 | 1983-01-16 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1986-01-15 | 1986-07-17 | 1987-01-16 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1990-01-15 | 1990-07-17 | 1991-01-16 | $7700.00 | Window Closed / Lapsed |