US4130771A Expired / Lapsed US ⏱️ 0.0 years remaining

Method of adjusting the frequency of a crystal resonator and reducing ageing effects

Assignee: K & L MICROWAVE Inc A DE CORP
•
Filing: 1977-06-09
•
Granted: 1978-12-19
•
Expires: 1997-06-09
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method is provided for adjusting the resonant frequency of an aluminum plated quartz resonator so as to reduce the effect of aging. The method comprises initially forming the aluminum plated resonator so that its frequency is above the nominal frequency, and then reducing the frequency to the nominal value by anodically forming an oxide film with a thickness in excess of 50A on the aluminum plating.

Inventors

  • 👤 Virgil E. Bottom

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-26 13:22
CPC Classifications
H; H03; H03H; H03H3/00; H03H3/007; H03H3/02; H03H3/04

Claims Analysis

Total Claims: 16
Claim 1
Independent Claim 190 words
Method of producing a piezoelectric crystal unit that is resistant to aging and can maintain a predetermined nominal resonant frequency f r comprising: providing a piezoelectric crystal unit having at least one aluminum electrode arranged so that said unit has a resonant frequency greater than f r and so that the aluminum electrode has at least one exposed surface; making said at least one aluminum electrode of said unit the anode and a separate aluminum body the cathode, respectively, in an electric circuit comprising a D.C. power supply and a liquid electrolyte which surrounds said unit and aluminum body and which contains oxygen-bearing anions and does not dissolve aluminum oxide; and adjusting the voltage output by said power supply to said circuit in accordance with the difference between the resonant frequency of said unit and said predetermined nominal resonant frequency so as to cause an oxide layer to be formed on said at least one electrode by anodic oxidation to a thickness of at least about 50A to cause said resonant frequency to be stabilized and changed to substantially said nominal frequency and to make said unit resistant to aging.
Claim 2
Dependent Claim 190 words
Method of producing a piezoelectric crystal unit that is resistant to aging and can maintain a predetermined nominal resonant frequency f r comprising: providing a piezoelectric crystal unit having at least one aluminum electrode arranged so that said unit has a resonant frequency greater than f r and so that the aluminum electrode has at least one exposed surface; making said at least one aluminum electrode of said unit the anode and a separate aluminum body the cathode, respectively, in an electric circuit comprising a D.C. power supply and a liquid electrolyte which surrounds said unit and aluminum body and which contains oxygen-bearing anions and does not dissolve aluminum oxide; and adjusting the voltage output by said power supply to said circuit in accordance with the difference between the resonant frequency of said unit and said predetermined nominal resonant frequency so as to cause an oxide layer to be formed on said at least one electrode by anodic oxidation to a thickness of at least about 50A to cause said resonant frequency to be stabilized and changed to substantially said nominal frequency and to make said unit resistant to aging.
Claim 3
Dependent Claim 27 words
Method of claim 1 where said oxide layer on said at least one electrode has a thickness in the range of from about 50A to about 300A.
Claim 4
Dependent Claim 47 words
Method of claim 1 wherein said resonator is made with an initial resonant frequency less than f r , and said electrodes are etched to increase the resonant frequency above f r before said oxide layer is formed on said at least one electrode by anodic oxidation.
Claim 5
Dependent Claim 32 words
The method according to claim 1 wherein said unit has at least two aluminum electrodes and an oxide layer is formed on each of said at least two electrodes by anodic oxidation.
Claim 6
Dependent Claim 172 words
Method of adjusting the bandwidth of a piezoelectric crystal unit by a selected amount and also making the unit resistant to aging where said unit includes a crystal with at least one aluminum electrode having at least one exposed surface, comprising the steps of: immersing said unit and an aluminum cathode in an electrolyte which contains oxygen-bearing anions and which does not dissolve aluminum oxide; and providing a voltage between said at least one electrode and said cathode with a polarity such as to cause anodic oxidation of the exposed surface of said at least one electrode, and adjusting said voltage in accordance with the amount by which said bandwidth is to be adjusted so that said anodic oxidation will cause an oxide layer to be formed on said exposed surface to a thickness sufficient to shift the bandwidth by said selected amount to stabilize the frequency of said unit and to make said unit resistant to aging, said voltage being sufficient to form an anodized oxide layer of at least 50A.
Claim 7
Dependent Claim 172 words
Method of adjusting the bandwidth of a piezoelectric crystal unit by a selected amount and also making the unit resistant to aging where said unit includes a crystal with at least one aluminum electrode having at least one exposed surface, comprising the steps of: immersing said unit and an aluminum cathode in an electrolyte which contains oxygen-bearing anions and which does not dissolve aluminum oxide; and providing a voltage between said at least one electrode and said cathode with a polarity such as to cause anodic oxidation of the exposed surface of said at least one electrode, and adjusting said voltage in accordance with the amount by which said bandwidth is to be adjusted so that said anodic oxidation will cause an oxide layer to be formed on said exposed surface to a thickness sufficient to shift the bandwidth by said selected amount to stabilize the frequency of said unit and to make said unit resistant to aging, said voltage being sufficient to form an anodized oxide layer of at least 50A.
Claim 8
Dependent Claim 199 words
A piezoelectric crystal unit that is resistant to aging and can maintain a predetermined nominal frequency having at least one aluminum electrode, said unit being made in accordance with a process comprising: providing a piezoelectric crystal unit having at least one aluminum electrode arranged so that said unit has a resonant frequency greater than f r and so that the aluminum electrode has at least one exposed surface; making said at least one aluminum electrode of said unit the anode and a separate aluminum body the cathode, respectively, in an electric circuit comprising a DC power supply and a liquid electrolyte which surrounds said unit and aluminum body and which contains oxygen-bearing anions and does not dissolve aluminum oxide; and adjusting the voltage output by said power supply to said circuit in accordance with the difference between the resonant frequency of said unit and said predetermined nominal resonant frequency so as to cause an oxide layer to be formed on said at least one aluminum by anodic oxidation to a thickness of at least about 50A to cause said resonant frequency to be stabilized and changed to substantially said nominal frequency and to make said unit resistant to aging.
Claim 9
Dependent Claim 199 words
A piezoelectric crystal unit that is resistant to aging and can maintain a predetermined nominal frequency having at least one aluminum electrode, said unit being made in accordance with a process comprising: providing a piezoelectric crystal unit having at least one aluminum electrode arranged so that said unit has a resonant frequency greater than f r and so that the aluminum electrode has at least one exposed surface; making said at least one aluminum electrode of said unit the anode and a separate aluminum body the cathode, respectively, in an electric circuit comprising a DC power supply and a liquid electrolyte which surrounds said unit and aluminum body and which contains oxygen-bearing anions and does not dissolve aluminum oxide; and adjusting the voltage output by said power supply to said circuit in accordance with the difference between the resonant frequency of said unit and said predetermined nominal resonant frequency so as to cause an oxide layer to be formed on said at least one aluminum by anodic oxidation to a thickness of at least about 50A to cause said resonant frequency to be stabilized and changed to substantially said nominal frequency and to make said unit resistant to aging.
Claim 10
Dependent Claim 18 words
A piezoelectric crystal unit according to claim 6 wherein said oxide layer has a thickness below about 300A.
Claim 11
Dependent Claim 35 words
A piezoelectric crystal unit in accordance with claim 6, wherein said unit includes at least two aluminum electrodes and an oxide layer is formed on each of said at least two electrodes by anodic oxidation.
Claim 12
Dependent Claim 213 words
Method of producing a piezoelectric crystal unit that is resistant to aging and can maintain a predetermined nominal resonant frequency f r comprising: providing a piezoelectric crystal unit having at least one aluminum electrode arranged so that said unit has a resonant frequency greater than f r and so that said at least one aluminum electrode has at least one exposed surface; adapting said unit for anodic oxidation of its said at least one electrode by (a) connecting the said at least one electrode of said unit to the positive output terminal of a DC power supply, (b) connecting an aluminum cathode to the negative output terminal of the same power supply and (c) suspending the unit and aluminum cathode in an electrolyte which contains oxygen-bearing anions and does not dissolve aluminum oxide; and adjusting the output voltage of said power supply to a predetermined level so that current passes from said supply through said electrolyte, said at least one aluminum electrode and said cathode and causes an oxide layer to be formed on the exposed surface of said at least one electrode by anodic oxidation to a thickness of at least 50A required to change the resonant frequency of said unit to substantially f r and make the unit resistant to aging.
Claim 13
Dependent Claim 213 words
Method of producing a piezoelectric crystal unit that is resistant to aging and can maintain a predetermined nominal resonant frequency f r comprising: providing a piezoelectric crystal unit having at least one aluminum electrode arranged so that said unit has a resonant frequency greater than f r and so that said at least one aluminum electrode has at least one exposed surface; adapting said unit for anodic oxidation of its said at least one electrode by (a) connecting the said at least one electrode of said unit to the positive output terminal of a DC power supply, (b) connecting an aluminum cathode to the negative output terminal of the same power supply and (c) suspending the unit and aluminum cathode in an electrolyte which contains oxygen-bearing anions and does not dissolve aluminum oxide; and adjusting the output voltage of said power supply to a predetermined level so that current passes from said supply through said electrolyte, said at least one aluminum electrode and said cathode and causes an oxide layer to be formed on the exposed surface of said at least one electrode by anodic oxidation to a thickness of at least 50A required to change the resonant frequency of said unit to substantially f r and make the unit resistant to aging.
Claim 14
Dependent Claim 92 words
Method of producing a crystal resonator unit that is resistant to aging and can maintain a predetermined nominal resonant frequency f r comprising the steps of: providing a crystal resonator having at least one metal electrode arranged so that said resonator has a resonant frequency greater than f r , and forming an oxide layer on said electrode of a thickness of at least 50A so as to make the crystal resonator resistant to aging and to permanently stabilize and adjust the resonant frequency of said resonator to substantially f r .
Claim 15
Dependent Claim 92 words
Method of producing a crystal resonator unit that is resistant to aging and can maintain a predetermined nominal resonant frequency f r comprising the steps of: providing a crystal resonator having at least one metal electrode arranged so that said resonator has a resonant frequency greater than f r , and forming an oxide layer on said electrode of a thickness of at least 50A so as to make the crystal resonator resistant to aging and to permanently stabilize and adjust the resonant frequency of said resonator to substantially f r .
Claim 16
Dependent Claim 18 words
The method of claim 10 wherein two separate aluminum electrodes are used as the electrodes for said unit.

References Cited (Backward Citations)

US2101893A Cited
US3401276A Cited
GB1185819A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1981-12-18 1982-06-19 1982-12-19 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1985-12-18 1986-06-19 1986-12-19 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1989-12-18 1990-06-19 1990-12-19 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag